Search NASA⌕ Search

Engineering topics

Aabdin, Z

Publications and source records attributed to Aabdin, Z.

Sb[subscript 2]Te[subscript 3] and Bi[subscript 2]Te[subscript 3] Thin Films Grown by Room-Temperature MBE

Sb{sub 2}Te3 and Bi{sub 2}Te3 thin films were grown on SiO{sub 2} and BaF{sub 2} substrates at room temperature using molecular beam epitaxy. Metallic layers with thicknesses of 0.2 nm were alternately deposited at room temperature, and the films were subsequently annealed at 250 C for 2 h. x-Ray diffraction and energy-filtered transmission electron microscopy (TEM) combined with high-accuracy energy-dispersive x-ray spectrometry revealed stoichiometric films, grain sizes of less than 500 nm, and a texture. High-quality in-plane thermoelectric properties were obtained for Sb{sub 2}Te3 films at room temperature, i.e., low charge carrier density (2.6 x 10{sup 19} cm{sup -3}, large thermopower (130 {micro}V K{sup -1}), large charge carrier mobility (402 cm{sup 2} V{sup -1} s{sup -1}), and resulting large power factor (29 {micro}W cm{sup -1} K{sup -2}). Bi{sub 2}Te3 films also showed low charge carrier density (2.7 x 10{sup 19} cm{sup -3}), moderate thermopower (-153 {micro}V K{sup -1}), but very low charge carrier mobility (80 cm{sup 2} V{sup -1} s{sup -1}), yielding low power factor (8 {micro}W cm{sup -1} K{sup -2}). The low mobilities were attributed to Bi-rich grain boundary phases identified by analytical energy-filtered TEM.

36 MATERIALS SCIENCE↗

Room-temperature MBE deposition, thermoelectric properties, and advanced structural characterization of binary Bi[subscript 2]Te[subscript 3] and Sb[subscript 2]Te[subscript 3] thin films

Sb{sub 2}Te{sub 3} and Bi{sub 2}Te{sub 3} thin films were grown at room temperature on SiO{sub 2} and BaF{sub 2} substrates using molecular beam epitaxy. A layer-by-layer growth was achieved such that metallic layers of the elements with 0.2 nm thickness were deposited. The layer structure in the as-deposited films was confirmed by X-ray diffraction and was seen more clearly in Sb{sub 2}Te{sub 3} thin films. Subsequent annealing was done at 250 C for 2 h and produced the Sb{sub 2}Te{sub 3} and Bi{sub 2}Te{sub 3} crystal structure as confirmed by high-energy X-ray diffraction. This preparation process is referred to as nano-alloying and it was demonstrated to yield single-phase thin films of these compounds. In the thin films a significant texture could be identified with the crystal c axis being almost parallel to the growth direction for Sb{sub 2}Te{sub 3} and tilted by about 30{sup o} for Bi{sub 2}Te{sub 3} thin films. In-plane transport properties were measured for the annealed films at room temperature. Both films yielded a charge carrier density of about 2.6 x 10{sup 19} cm{sup -3}. The Sb{sub 2}Te{sub 3} films were p-type, had a thermopower of +130 {micro}V K{sup -1}, and surprisingly high mobilities of 402 cm{sup 2} V{sup -1} s{sup -1}. The Bi{sub 2}Te{sub 3} films were n-type, showed a thermopower of -153 {micro}V K{sup -1}, and yielded significantly smaller mobilities of 80 cm2 V{sup -1} s{sup -1}. The chemical composition and microstructure of the films were investigated by transmission electron microscopy (TEM) on cross sections of the thin films. The grain sizes were about 500 nm for the Sb{sub 2}Te{sub 3} and 250 nm for the Bi{sub 2}Te{sub 3} films. In the Bi{sub 2}Te{sub 3} thin film, energy-filtered TEM allowed to image a Bi-rich grain boundary phase, several nanometers thick. This secondary phase explains the poor mobilities of the Bi{sub 2}Te{sub 3} thin film. With these results the high potential of the nano-alloying deposition technique for growing films with a more complex layer architecture is demonstrated.

36 MATERIALS SCIENCE↗