Search NASA⌕ Search

Engineering topics

Apblett, Christopher A.

Publications and source records attributed to Apblett, Christopher A..

At least 19 records

Critical Evaluation of Potentiostatic Holds as Accelerated Predictors of Capacity Fade during Calendar Aging

Li-ion batteries will lose both capacity and power over time due to calendar aging caused by slow parasitic processes that consume Li + ions. Studying and mitigating these processes is traditionally an equally slow venture, which is especially taxing for the validation of new active materials and electrolyte additives. Here, we evaluate whether potentiostatic holds can be used to accelerate the diagnosis of Li + loss during calendar aging. The technique is based on the idea that, under the right conditions, the current measured as the cell voltage is held constant can be correlated with the instantaneous rate of side reactions. Thus, in principle, these measurements could capture the rate of capacity fade in real time . In practice, we show that this method is incapable of quantitatively forecasting calendar aging trends. Instead, our study demonstrates that potentiostatic holds can be applied for initial qualitative screening of systems that exhibit promising long-term stability, which can be useful to shrink the parameter space for calendar aging studies. By facilitating the identification of improved formulations, this approach can help accelerate innovation in the battery industry.

25 ENERGY STORAGE↗

Calendar aging of silicon-containing batteries

High-energy batteries for automotive applications require cells to endure well over a decade of constant use, making their long-term stability paramount. This is particularly challenging for emerging cell chemistries containing silicon, for which extended testing information is scarce. While much of the research on silicon anodes has focused on mitigating the consequences of volume changes during cycling, comparatively little is known about the time-dependent degradation of silicon-containing batteries. Here we discuss a series of studies on the reactivity of silicon that, collectively, paint a picture of how the chemistry of silicon exacerbates the calendar aging of lithium-ion cells. Assessing and mitigating this shortcoming should be the focus of future research to fully realize the advantages of this battery technology.

25 ENERGY STORAGE↗

Mechanical studies of the solid electrolyte interphase on anodes in lithium and lithium ion batteries

A stable solid electrolyte interphase (SEI) layer is key to high performing lithium ion batteries for metrics such as calendar and cycle life. The SEI must be mechanically robust to withstand large volumetric changes in anode materials such as lithium and silicon, so understanding the mechanical properties and behavior of the SEI is essential for the rational design of artificial SEI and anode form factors. The mechanical properties and mechanical failure of the SEI are challenging to study, because the SEI is thin at only ~ 10 – 200 nm thick and is air sensitive. Furthermore, the SEI changes as a function of electrode material, electrolyte and additives, temperature, potential, and formation protocols. A variety of in situ and ex situ techniques have been used to study the mechanics of the SEI on a variety of lithium ion battery anode candidates; however, there hasn't been a succinct review of the findings thus far. Because of the difficultly of isolating the true SEI and its mechanical properties, there have been a limited number of studies that can fully de-convolute the SEI from the anode it forms on. A review of past research will be helpful for culminating current knowledge and helping to inspire new innovations to better quantify and understand the mechanical behavior of the SEI. This review will summarize the different experimental and theoretical techniques used to study the mechanics of SEI on common lithium ion battery anodes and their strengths and weaknesses.

25 ENERGY STORAGE↗

Investigating the Chemical Reactivity of Lithium Silicate Model SEI Layers

Silicon anodes suffer from an unstable solid electrolyte interphase (SEI) layer that contributes to undesirable capacity fade with cycling. A key part to addressing this unstable SEI formation is to examine how certain components of the SEI react with the electrolyte over time. One SEI component that has not been thoroughly studied in the context of the chemical reactivity against the electrolyte is lithiated silicate. Four model silicate thin films with increasing lithium content were deposited by radio frequency (RF) magnetron sputtering to study how the lithiation of the native oxide on a silicon anode affects the chemical stability of the anode surface. SiO2, Li2Si2O5, Li2SiO3, and Li3SiOx films were exposed to 1.2 M LiPF6 in the 3:7 wt% ethylene carbonate/ethyl methyl carbonate (EC/EMC) electrolyte for periods of time that are representative of the amount of time it takes to undergo cell formations. Soaked samples were rinsed, dried, and characterized by a combination of attenuated total reflectance-infrared spectroscopy (ATR-IR), focused ion beam-secondary electron microscopy (FIB-SEM), and X-ray photoelectron spectroscopy (XPS) depth profiling. It was found that the rate of the decrease in film thickness of the silicates exposed to the electrolyte over time increases as a function of the lithium content in the thin film. This reaction involves HF etching and LiPF6 salt degradation leading to silicate loss and fluorination throughout the bulk. Understanding this chemical instability is critical to determining the overall mechanism of SEI degradation over time.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

Intrinsic Chemical Reactivity of Silicon Electrode Materials: Gas Evolution

In this work, we explore how the chemical reactivity toward an aprotic battery electrolyte changes as a function of lithium salt and silicon surface termination chemistry. The reactions are highly correlated, where one decomposition reaction leads to a subsequent decomposition reaction. We report the data show that the presence of silicon hydrides (SiH$_x$) promotes the formation of CO gas, while surface oxides SiO$_x$ drive the formation of CO 2 . The extent and rate of oxidation depend on the surface basicity of the SiO 2 surface species. The most acidic surfaces seem to hinder CO 2 generation but not the decomposition of the salt. Indeed, the presence of F-containing salts (LiPF 6 and LiTFSI) promotes the reactions between carbonate electrolyte and silicon surfaces. Surfaces with high Li content seem to be the most passivating to gassing reactions, pointing to a pathway to stabilize the interfaces during cell formation and assembly.

25 ENERGY STORAGE↗

Accelerating Learning with Set-Based Concurrent Engineering

The traditional design approach for product development is to develop a design based on customer requirements and technical knowledge, build the product according to the detail requirements provided, and then test the product to validate that it works as intended. The team typically starts by identifying a single design approach and spends their time validating a single design during testing. Design teams often encounter issues in the course of development with performance, manufacturability, interfaces and more. To compensate for test failures, teams often build in time into the schedule for additional design loopbacks. Further, when the loopbacks lead to change, the late changes are costly and risky, causing the team to focuses on "fixing the bare minimum" to meet cost and schedule expectations.

42 ENGINEERING↗

EERE Silicon Electrolyte Interface Stabilization (SIESta) FY19 Q2 Report

This quarter, we have focused on characterizing the electrochemical of native oxide and "pristine' silicon surfaces by electrochemical cycling for various conditions, starting with either a freshly etched Si surface, or varying amounts of oxide on the surface (either native grown or deposited). These changes can be used to determine if the pristine surface evolves differently than those that have been modified (Q1 milestone). We are also developing new diagnostics (microcalorimetry and stress measurement in-situ) to determine how the nature of the silicon surface affects the composition, function, and thickness of the SEI (Q2 milestone).

36 MATERIALS SCIENCE↗

Silicon Electrolyte Interface Stabilization (SEISTa)

This quarter, we have focused on characterizing the electrochemical response, both through cyclic voltammetry and through constant current charge/discharge characterization of the silicon samples coated with silicates containing varying amounts of Li in the SiOx layer. These studies were performed using a standard Gen-2 electrolyte without FEC. We also performed electrochemical impedance spectroscopy on samples exposed to the Gen-2 electrolyte continually, and collected EIS spectra as a function of time and temperature.

30 DIRECT ENERGY CONVERSION↗