Mechanical Characterization of Electrolyzer Membranes and Components Under Compression

Proton-exchange membrane (PEM) water electrolysis is a promising technology for producing clean hydrogen by electrochemically splitting water when paired with renewable energy sources. A major roadblock to improving electrolyzer durability is the mechanical degradation of the cell components, which requires an understanding of their mechanical response under device-relevant conditions. However, there is a lack of studies on the mechanical characterization of the PEM and other components, as well as and their interactions. This study aims to address this gap by using a custom-designed testing apparatus to investigate the mechanics of electrolyzer components in uniaxial compression at 25 and 80 °C. Findings show stress-strain response of components have a varying degree of nonlinearity owing to their distinct deformation mechanisms and morphologies, from porous structures to polymers. These results are used to develop an expression for compressive stress-strain response of Nafion membranes and then analyze the deformation of components under applied pressure by using a 1-D spring network model of cell assembly. This work provides a new understanding of mechanical responses of the electrolyzer membrane and cell components, which can help assess material design and cell assembly strategies for improved electrolyzer durability.

08 HYDROGEN↗

Compressive Creep of Polymer Electrolyte Membranes: A Case Study for Electrolyzers

For proton-exchange membrane (PEM) water electrolyzers to be commercially feasible, PEMs must perform over long lifetimes in liquid environments under compression while maintaining mechanical stability. A hydrated environment, while inherent for operation and conductivity, undermines PEM stability. Mechanical stability of PEMs is commonly characterized in tension, which is not applicable to electrolyzers, wherein PEMs could undergo high pressures. In this study, a compression creep procedure is developed using a custom-designed setup to monitor creep response of hydrated PEMs. Furthermore, our results show that PEMs exhibit continuous creep response under compression over 24 h, with a dependence on the applied pressure and hydration state.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗