Damage Tolerance Assessment of Laser Clad Repairs of Coarse Grain Ti-6Al-4V

Background: Laser cladding offers a promising approach to repairing aviation components, with the ability to restore the geometric shape and the static and fatigue strength. Objective: The damage tolerance of a coarse grain Ti-6Al-4 V material is assessed via three sets of samples: (i) baseline, (ii) laser clad repaired, and (iii) laser cladding followed by heat treatment. Method: The specimens were subjected to fatigue loading using a marker band technique, in which cracks initiated from pre-defined laser slots and the small crack growth rates were measured by quantitative fractography. Additional characterization was performed on these samples, including hardness measurements, microstructure analysis, and multimodal residual stress analyses. Results: The region of the specimen undergoing laser cladding exhibited higher hardness values and a compressive residual stress, based on the slitting method. The samples subjected to heat treatment after cladding displayed negligible differences in grain size and minimal residual stress relaxation. Conclusions: The results demonstrated significant variability, with data demonstrating that cracks in the laser clad region (exhibiting the largest compressive residual stress) grew faster than cracks in the substrate region of the sample or in the baseline cases. Finally, these counterintuitive results are rationalized with additional analyses from synchrotron-based energy dispersive X-ray diffraction and high energy X-ray diffraction, demonstrating significant spatial variability in the residual elastic strains in the millimeter-sized prior β grains within the material.

36 MATERIALS SCIENCE↗

Small fatigue crack growth behavior of Ti-6Al-4V produced via selective laser melting: In situ characterization of a 3D crack tip interactions with defects

Small fatigue crack growth (SFCG) behavior is examined for additively manufactured Ti-6Al-4V specimens with optimal and trial build conditions (representing an increased degree of defects) through a combination of in situ tomography and in situ energy dispersive X-ray diffraction. The results showed slower crack growth rates for the SFCG samples compared to the long cracks (which was not expected). Finally, in the case of the trial conditions, the increased levels of porosity deterred crack growth by blunting the crack, as evident by the in situ tomography characterization.

36 MATERIALS SCIENCE↗

Residual Strain Analysis in Linear Friction Welds of Similar and Dissimilar Titanium Alloys Using Energy Dispersive X-ray Diffraction

Residual strains in linear friction welds (LFW) of similar, Ti-6Al-4V (Ti64) welded to Ti-6Al-4V, and dissimilar, Ti-6Al-4V welded to Ti-5Al-5V-5Mo-3Cr (Ti5553), titanium alloys have been characterized using energy-dispersive X-ray diffraction. For each type of LFW, one sample was chosen in the as-welded (AW) condition and another sample was selected after a post-weld heat treatment (HT). Residual strains have been separately studied in the alpha and beta phases of the material, and five components (three axial and two shear) have been reported in each case. In-plane axial components of the residual strains show a smooth and symmetric behavior about the weld center for the Ti64-Ti64 LFW samples in the AW condition, whereas these components in the Ti64-Ti5553 LFW sample show a symmetric trend with jump discontinuities. Such jump discontinuities, observed in both the AW and HT conditions of the Ti64-Ti5553 samples, suggest different strain-free lattice parameters in the weld region and the parent material, whereas the results from the Ti64-Ti64 LFW samples in both AW and HT conditions suggest nearly uniform strain-free lattice parameters throughout the weld region. Finally, the observed trends in the in-plane axial residual strain components have been rationalized by the corresponding microstructural changes and variations across the weld region via backscatter electron (BSE) images.