A six degrees of freedom femtosecond laser system for fabrication of small-scale mechanical property specimens

Here, we present the details of a novel ultra-short pulsed laser machining workstation that has been employed for high-throughput laser machining of small-scale mechanical property specimens. This system employs a six degrees of freedom hexapod positioning stage capable of macroscopic movements at high positional accuracy. We developed a methodology that uses quantitative image analysis to measure key parameters required to minimize the hexapod positioning and rotational error. Application of this system to laser machining of small-scale 316L stainless steel tensile specimens and ultra-high molecular weight polyethylene compressive specimens using eucentric tilt and rotation about the specimen axis will be shown, where serial laser milling at a specimen tilt angle of 10° was used to effectively eliminate any taper in the sample cross section that is typically found in laser machining.

47 OTHER INSTRUMENTATION↗

A Methodology for determining optimal milling parameters for low-taper microtensile sample production

Femtosecond lasers are beginning to see an increase in interest for industrial and high throughput microsample milling applications. Despite this, much of the literature regarding removal rate studies for ultrashort pulse laser milling continues to focus on single-pulse or similar experiments that have a very small time on target. The material volume removal rates of femtosecond milling can vary wildly depending on parameters like laser scan speed, hatch spacing, z-axis step size, and pulses on the material. Currently, there is no established methodology for determining the optimal values of these parameters for micromilling applications. This methodology was developed in this study. The methodology consists of a pulse study, a repeat study, and a z-step study that will return the milling parameters that resulted in the largest volume removal rate for the laser used for this research. The methodology was created for the laser system used in this study, and was tested on 316 Stainless Steel, but was developed in such a way that it may be adapted to any material, and with some tweaking of variables might be used in other laser systems. The laser system used in this study utilizes a novel positioning stage that introduces 6 degrees of freedom to the translation of laser samples, being able to tilt and move in all three axes. Using both the developed methodology and the unique capabilities of the laser microtensile samples were produced with taper angles of <1° in 316 Stainless Steel.

Barker, Zachary Wayne↗