Life testing of 10 cm × 10 cm fuel-electrode-supported solid oxide cells in reversible operation
Not provided.
Engineering topics
Publications and source records attributed to Barnett, Scott.
Not provided.
This project aims to develop and test novel Reversible Solid Oxide Cells (ReSOCs) specifically designed to yield low area specific resistance, as required to achieve high round trip efficiency in reversible operation at high current density. A key objective is to improve long-term reversible SOC durability; mechanistic degradation models will be used to predict long-term durability using input data from accelerated testing that combines electrochemical life testing with quantitative microstructural and chemical evaluation. The modeling tasks seek to design low-loss, low-cost ReSOC systems using input data from the experimental cell studies. A key challenge is to develop a thermal management strategy that maintains thermally self-sustaining operation while operating the stack at a potential lower than the thermo-neutral steam electrolysis voltage of ~1.3 V, to maintain high efficiency.
The project aims to develop mechanistic degradation models that realistically predict long-term Solid Oxide Electrolysis Cell (SOEC) durability, using input data from accelerated electrochemical life testing combined with quantitative microstructural and microchemical evaluation. A promising SOEC type will be further developed. The understanding achieved by combining experimental results and theory will be used to guide improvements in long-term SOEC durability, and validate that this technology can reach DOE H 2 production cost and durability targets. Planned outcomes include: (1) new experimental accelerated testing data on SOEC degradation at the oxygen electrode, fuel electrode, and electrolyte; (2) predictive theory of degradation developed based on the accelerated test data; (3) new electrode materials and processing methods that minimize degradation rate; (4) determination of the impact of SOEC electrolyte thickness and electrode composition/microstructure on performance and degradation; (5) determination of the operating conditions where degradation is minimized; and (6) validation of degradation models for extrapolating accelerated test data to predict long-term durability.
An interfacial energy can be a function of a bulk field such as temperature or electric field. Here we find that in a system with a gradient in temperature or electric potential, the resulting variation in interfacial energy can induce a particle to migrate by either surface or bulk diffusion. For a circular particle under a constant unidirectional gradient in the bulk field, the field dependence of the interfacial energy induces a circular particle to move as a circle at a constant velocity along the direction from higher to lower interfacial energy. A linear stability analysis of this steady state migration suggests that perturbations will damp out as time evolves, and thus under these conditions a migrating circular particle is morphologically stable. Other spatial distributions of interface energy can lead to the distortion of an initially circular shaped particle during migration. A phase field model is developed that captures these distortions and verifies the theoretical results mentioned above.
Not provided.
Gd-doped Ceria (GDC) barrier layers are widely used in solid oxide electrolysis cells to prevent reactions between the Y-stabilized Zirconia (YSZ) electrolyte and oxygen electrode. In some cases, electrolysis operation causes fracture near the GDC/YSZ interface. Here, we explain this effect using a numerical calculation, showing that a peak oxygen pressure is observed near the GDC/YSZ interface during electrolysis operation. Moreover, GDC/YSZ interdiffusion and possible zirconate phase formation occurring during electrode firing yield a low oxygen ion conductivity region that introduces a much higher peak oxygen partial pressure at the interdiffusion layer/YSZ interface, thereby exacerbating degradation. The results indicate that the peak pressure can be reduced and, thereby, damage can be mitigated by altering processing in order to minimize interdiffusion, decreasing the GDC layer thickness, and reducing oxygen electrode polarization resistance or altering electrolyte transport properties, e.g., changing the Gd doping level of GDC to increase the oxygen vacancy diffusivity.
During this project, a dense GDC barrier layer was deposited on YSZ substrate to prevent chemical reaction between LSCF and YSZ by a cost-effective EPD method. PPy was used as the agent to make YSZ conductive. Highly compact GDC green layer was obtained by the EPD process in an ethanol-based suspension. The deposition rate on PPy coated YSZ is slower than that on graphite because the charge transfer process is the rate-determining step. The main resistance is from the ion accumulation/depletion zone. The H + ions reduced at the cathode consist of free H + ions and absorbed H + ions corresponding to the unavoidable electrochemical reaction and deposition, respectively. A factor f was introduced to reflects EPD efficiency and describe the competitive relationship between deposition and electrochemical reaction during EPD process. f is in the range from 0 to 0.5 which is determined by the amount ration between free H + ions and absorbed H + ions at the suspension/deposit interface and the conductivity of the cathode. f decreases with the increase of current density or applied voltage and the conductivity of the cathode. GDC thin layers formed by DC-EPD in a thickness range of 5-8 µm were successfully densified at as low as 1300 °C and the adhesion between GDC and YSZ was good. The densification temperature can be further reduced to 1250 °C when AC-EPD was used to replace DC-EPD. The deposition rate increases with the increase of duty cycle and voltage ratio. The deposition rate increases with the increase of frequency from 10 Hz to 500 Hz, while decrease when the frequency increases from 500 Hz to 5000 Hz. Desorption of absorbed charge carrier is easy and irreversible. The deposition rate is independent on the conductivity of the cathode when the electrochemical reaction can be ignored with a high frequency. Inter-diffusion of cation ions between the electrolyte and barrier layer has been systematically characterized via 3-D atom probe, TEM, and other techniques. No measurable Sr transport occurs across the GDC layer with a thickness of 1.5 – 6 μm at a LSCF processing temperature of 1000 °C. However, Sr transport does occur across GDC layer with a thickness of 1.5 or 3 μm at a higher LSCF sintering temperature (1000 °C or 1200 °C). The primary pathway are open pores or grain boundaries in the GDC. The observed zirconate layer is discontinuous even for the most extreme conditions (1.5 μm GDC, 1200 °C LSCF sintering temperature). Increasing the thickness of GDC to 4.5 μm can effectively suppress any zirconate formation measurable by SEM-EDX. Cobalt is observed at grain boundaries within the GDC, suggesting some depletion of Co from the LSCF layer that may ultimately impact electrode performance.
Reduction-stable mixed ionic and electronic conductors such as Sr(Ti,Fe)O 3-δ (STF) are promising materials for application in anodes of solid oxide fuel cells. The defect chemistry of STF and its properties as solid oxide fuel cell (SOFC) cathode have been studied thoroughly, while mechanistic investigations of its electrochemical properties as SOFC anode material are still scarce. In this study, thin film model electrodes of STF with 30% and 70% Fe content were investigated in H 2 +H 2 O atmosphere by electrochemical impedance spectroscopy. Lithographically patterned thin film Pt current collectors were applied on top or beneath the STF thin films to compensate for the low electronic conductivity under reducing conditions. Oxygen exchange resistances, electronic and ionic conductivities and chemical capacitances were quantified and discussed in a defect chemical model. Increasing Fe content increases the electro-catalytic activity of the STF surface as well as the electronic and ionic conductivity. Current collectors on top also increase the electrochemical activity due to a highly active Pt-atmosphere-STF triple phase boundary. Furthermore, the electrochemical activity depends decisively on the H 2 :H 2 O mixing ratio and the polarization. Lastly, Fe 0 nanoparticles may evolve on the surface in hydrogen rich atmospheres and increase the hydrogen adsorption rate.
This project addresses fundamental materials challenges in solid oxide electrochemical cells, devices that have a broad range of important energy applications. Although nano-scale mixed ionically and electronically conducting (MIEC) materials provide an important opportunity to improve performance and reduce device operating temperature, durability issues threaten to limit their utility and have remained largely unexplored. Our work has focused on both (1) understanding the fundamental processes related to oxygen transport and surface-vapor reactions in nano-scale MIEC materials, and (2) determining and understanding the key factors that control their long-term stability. Furthermore, materials stability has been explored under the “extreme” conditions encountered in many solid oxide cell applications, i.e, very high or very low effective oxygen pressures, and high current density.
Solid oxide fuel cells (SOFCs) are high efficiency energy conversion devices. Present materials set, using yttria stabilized zirconia (YSZ) electrolyte, limit the cell operating temperatures to 800 C or higher. It has become increasingly evident however that lowering the operating temperature would provide a more expeditious route to commercialization. The advantages of intermediate temperature (600 to 800 C) operation are related to both economic and materials issues. Lower operating temperature allows the use of low cost materials for the balance of plant and limits degradation arising from materials interactions. When the SOFC operating temperature is in the range of 600 to 700 C, it is also possible to partially reform hydrocarbon fuels within the stack providing additional system cost savings by reducing the air preheat heat-exchanger and blower size. The promise of Sr and Mg doped lanthanum gallate (LSGM) electrolyte materials, based on their high ionic conductivity and oxygen transference number at the intermediate temperature is well recognized. The focus of the present project was two-fold: (a) Identify a cell fabrication technique to achieve the benefits of lanthanum gallate material, and (b) Investigate alternative cathode materials that demonstrate low cathode polarization losses at the intermediate temperature. A porous matrix supported, thin film cell configuration was fabricated. The electrode material precursor was infiltrated into the porous matrix and the counter electrode was screen printed. Both anode and cathode infiltration produced high performance cells. Comparison of the two approaches showed that an infiltrated cathode cells may have advantages in high fuel utilization operations. Two new cathode materials were evaluated. Northwestern University investigated LSGM-ceria composite cathode while Caltech evaluated Ba-Sr-Co-Fe (BSCF) based pervoskite cathode. Both cathode materials showed lower polarization losses at temperatures as low as 600 C than conventional manganite or cobaltite cathodes.