Enhanced Hanford High-Fluoride Waste Glass Property Data Development: Phase 1

This study focused on investigating the effects of fluorine concentration on simulated high-level waste glass properties to eventually establish a fluorine limit (as a single-component or multiple-component constraint) for glass formulations for high-fluoride Hanford wastes. This is a first step to provide data to understand the impacts of changing flowsheets on the mission duration and extent. A test matrix of 20 high-fluoride glasses was generated, and the chemical compositions were measured. The following properties were measured and tested against current model predictions: crystal formation after centerline canister cooling, crystallinity as a function of temperature, density, viscosity, electrical conductivity, toxic leaching characteristics using the toxicity characteristic leach profile (TCLP), product consistency using the product consistency test (PCT), and SO 3 solubility. Overall, current models failed to adequately predict most of the properties, possibly due to differences in compositional space used to generate the models and the current test matrix. Additional work is needed to more accurately assess the impacts of high-fluoride wastes on Hanford processing, including additional data collection over a broader composition region and model development for the key models of interest such as PCT and TCLP.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Formulation and testing of a high-tin borosilicate nuclear waste glass for in-can melting

Here, borosilicate waste glasses were successfully developed to immobilize two high-level waste raffinate streams via an in-can melter process with an Inconel 601 canister at 1050 °C. Measured viscosity and crystallinity thermal profiles were within the targeted processing constraints for the in-can melter process. Measured chemical durability of the glass by ASTM C1285–21 (Method A), ranged from normalized loss of boron, NL(B) = 1.44 – 2.65 g•m -2 , and NL(B) decreased with increased waste loading, accompanied by increased SnO 2 crystallinity. Measured corrosion of the in-can melter canister by a glass melt showed that Inconel 601 performed well at 1100 °C for up to 500 hr. Resistance polarization measurements versus time revealed that Inconel 601 corrosion rates in (and by) glass melts decreased from an initial rate of 63 mm•y -1 down to 10.2 mm•y -1 after 137 h with increased duration, which was attributed to formation of an oxide passivation layer (mainly Cr 2 O 3 ) at the alloy-glass interface.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Crystallization Constraints for WTP LAW Operations: Assessment of CCC Impacts on VHT and PCT

Much work has been done to expand the glass composition region available for operation of the Hanford Waste Treatment and Immobilization Plant. This includes the development of updated glass property-composition models as well as constraints. This report supports this effort by suggesting constraints for avoiding excessive, and likely detrimental, crystallization during slow cooling of the low-activity glass waste forms in their containers. The constraints target crystals in the Na-Al-silicate and Na-Ca-silicate families. These types of crystals were found to be potentially detrimental to glass durability as they remove Al and Si from the glass matrix, resulting in poor performance of the residual glass during testing such as the Product Consistency Test and the Vapor Hydration Test. Using previously acquired results and results from testing during this effort, the constraints described in the report were determined, and are suggested as options to reduce the risk of forming crystals of the types and concentrations that are likely detrimental to glass durability.