Here, the laser powder bed fusion (PBF-L) additive manufacturing (AM) community has dedicated significant efforts into process optimization and control for defect-free Ti-6Al-4V. As defects become less of an issue for PBF-L Ti-6Al-4V, the processing-structure-properties (PSP) relationships between AM microstructures can now be explored to optimize mechanical properties. Lower temperature aging treatments around 550 °C in wrought Ti-6A-4V have been historically understood to precipitation harden the α phase with an ordered, hexagonal close packed (HCP) α 2 phase. The α 2 phase existed as nanoscale Ti 3 Al precipitates coherent with the parent α phase. The goal of the present investigation was to implement a vacuum heat treatment of 545 °C for 100 hours on PBF-L Ti-6Al-4V. This vacuum heat treatment took place after an initial hot isostatic pressure (HIP) treatment that decomposed the as-built, martensitic microstructure. The vacuum aging successfully produced nanoscale precipitates of α 2 phase within α-laths, confirmed via atom probe tomography (APT). Microstructural-length scale and quasi-static mechanical properties were investigated by nanoindentation and uniaxial tensile tests of miniaturized test specimens. Given the sensitivity of Ti-6Al-4V mechanical properties to small changes in chemistry, all test specimens originated from the same build. The α 2 precipitation resulted in significantly harder α-laths (≈ 2 GPa) as measured via nanoindentation, as well as a relative yield and ultimate tensile strength increase of 60 MPa and 38 MPa, respectively. Analysis of Variance (ANOVA) of the datasets revealed no statistical differences in total elongation between the HIPed and HIPed + aged specimens, indicative of the aging treatment producing a net benefit of strength with no loss in ductility.

36 MATERIALS SCIENCE↗

Microstructural effects on the rotating bending fatigue behavior of Ti–6Al–4V produced via laser powder bed fusion with novel heat treatments

The rotating bending fatigue (RBF) behavior (fully reversed, R = -1) of additively manufactured (AM) Ti–6Al–4V alloy produced via laser powder bed fusion (PBF-L) was investigated with respect to different microstructures achieved through novel heat treatments. The investigation herein seeks to elucidate the effect of microstructure by controlling variables that can affect fatigue behavior in Ti–6Al–4V, such as chemistry, porosity, and surface roughness. In order to control these variables, different hot isostatic pressing (HIP) treatments at 800 °C, 920 °C, and 1050 °C with a 920 °C temper were applied to three sets of Ti–6Al–4V cylinders that originated from the same PBF-L build, such that there were 30 tests per condition. After HIP treatment, the specimens were machined and tested. The highest runout stress was achieved after sub-β transus HIP at 800 °C for 2 h at 200 MPa of pressure. A significant drop in fatigue strength was attributed to large prior-β grains and grain boundary α resulting from super-β transus HIP treated specimens. In conclusion, for the sub-β transus HIP specimens, differences in fatigue strength were attributed to α lath thickness, relative dislocation density, and dislocation boundary strengthening.

36 MATERIALS SCIENCE↗

Schmid factor crack propagation and tracking crystallographic texture markers of microstructural condition in direct energy deposition additive manufacturing of Ti-6Al-4V

Metallic additive manufacturing (AM) provides a customizable and tailorable manufacturing process for new engineering designs and technologies. The greatest challenge currently facing metallic AM is maintaining control of microstructural evolution during solidification and any solid state phase transformations during the build process. Ti-6Al-4V has been extensively surveyed in this regard, with the potential solid state and solidification microstructures explored at length. In this study, we evaluate the applicability of previously determined crystallo- graphic markers of microstructural condition observed in electron beam melting powder bed fusion (PBF-EB) builds of Ti-6Al-4V in a directed energy deposition (DED) build process. The aim of this effort is to elucidate whether or not these specific crystallographic textures are useful tools for indicating microstructural conditions in AM variants beyond PBF-EB. Parent β-Ti grain size was determined to be directly related to α-Ti textures in the DED build process, and the solid state microstructural condition could be inferred from the intensity of specific α-Ti orientations. Qualitative trends on the as-solidified β-Ti grain size were also determined to be related to the presence of a fiber texture, and proposed as a marker for as-solidified grain size in any cubic metal melted by AM. Analysis of the DED Ti-6Al-4V build also demonstrated a near complete fracture of the build volume, suspected to originate from accumulated thermal stresses in the solid state. Crack propagation was found to only appreciably occur in regions of slow cooling with large α +β colonies. Schmid factors for the basal and prismatic α-Ti systems explained the observed crack pathway, including slower bifurcation in colonies with lower Schmid factors of both slip systems. Colony morphologies and localized equiaxed β-Ti solidification were also found to originate from build pauses during production and uneven heating of the build edges during deposition. Tailoring of DED Ti-6Al-4V microstructures with the insight gained here is proposed, along with cautionary insight on preventing unplanned build pauses to maintain an informed and controlled thermal environment for microstructural control.

36 MATERIALS SCIENCE↗

The influence of temperature on the strain-hardening behavior of Fe-22/25/28Mn-3Al-3Si TRIP/TWIP steels

In this work, the influence of temperature and stacking fault energy (SFE) on the strain-hardening behavior and critical resolved shear stress for twinning was investigated for three Fe–22/25/28Mn–3Al–3Si wt.% transformation- and twinning-induced plasticity (TRIP/TWIP) steels. The SFEs were calculated by two different methods, density functional theory and statistical thermodynamic modeling. The dislocation structure, observed at low levels of plastic deformation, transitions from “planar” to “wavy” dislocation glide with an increase in temperature, Mn content, and/or SFE. The change in dislocation glide mechanisms from planar to wavy reduces the strain hardening rate, in part due to fewer planar obstacles and greater cross slip activity. Additionally, the alloys exhibit a large decrease in strength and ductility with increasing temperature from 25 to 200 °C, attributed to a substantial reduction in the thermally activated component of the flow stress, predominate suppression of TRIP and TWIP, and a significant increase in the critical resolved shear stress for mechanical twinning. Interestingly, the increase in SFE with temperature had a rather minor influence on the critical resolved shear stress for mechanical twinning, and other temperature dependent factors which likely play a more dominant role are discussed.

36 MATERIALS SCIENCE↗

Texture evolution as a function of scan strategy and build height in electron beam melted Ti-6Al-4V

Metal additive manufacturing (AM) enables customizable, on-demand parts, allowing for new designs and improved engineering performance. Yet, the ability to control AM metal alloy microstructures (i.e., grain morphology, crystallographic texture, and phase content) is lacking. Furthermore, this work performs corroborative neutron diffraction and large-scale electron backscatter diffraction (EBSD) measurements to assess crystallographic texture in electron beam melted (EBM) Ti-6Al-4V as a function of scan strategy and build height. Texture components for one raster and two spot melt scan strategies were evaluated using a triclinic specimen symmetry to capture all possible texture components, which were found to be considerably different than previously reported values from studies employing orthotropic specimen symmetry. This finding highlights the importance of a standard method and best practice for assessing textures produced by AM.

36 MATERIALS SCIENCE↗

Shoulder fillet effects in strength distributions of microelectromechanical system components

The failure forces and fracture strengths of polysilicon microelectromechanical system (MEMS) components in the form of stepped tensile bars with shoulder fillets were measured using a sequential failure chain methodology. Approximately 150 specimens for each of four fillet geometries with different stress concentration factors were tested. The resulting failure force and strength distributions of the four geometries were related by a common sidewall flaw population existing within different effective stressed lengths. The failure forces, strengths, and flaw population were well described by a weakest-link based analytical framework. Finite element analysis was used to verify body-force based expressions for the stress concentration factors and to provide insight into the variation of specimen effective length with fillet geometry. Monte Carlo simulations of flaw size and location, based on the strength measurements, were also used to provide insight into fillet shape and size effects. The successful description of the shoulder fillet specimen strengths provides further empirical support for application of the strength and flaw framework in MEMS fabrication and design optimization.

36 MATERIALS SCIENCE↗