Search NASA⌕ Search

Engineering topics

Bettge, Martin

Publications and source records attributed to Bettge, Martin.

Cathode active materials for lithium-ion batteries

Compounds, powders, and cathode active materials that can be used in lithium ion batteries are described herein. Methods of making such compounds, powders, and cathode active materials are described.

Dai, Hongli↗

Physical Theory of Voltage Fade in Lithium- and Manganese-Rich Transition Metal Oxides

Lithium- and manganese-rich (LMR) transition metal oxide cathodes are of interest for lithium-ion battery applications due to their increased energy density and decreased cost. However, the advantages in energy density and cost are offset, in part, due to the phenomena of voltage fade. Specifically, the voltage profiles (voltage as a function of capacity) of LMR cathodes transform from a high energy configuration to a lower energy configuration as they are repeatedly charged (Li removed) and discharged (Li inserted). Here, we propose a physical model of voltage fade that accounts for the emergence of a low voltage Li phase due to the introduction of transition metal ion defects within a parent Li phase. The phenomenological model was re-cast in a general form and experimental LMR charge profiles were de-convoluted to extract the evolutionary behavior of various components of LMR capacitance profiles. Evolution of the voltage fade component was found to follow a universal growth curve with a maximal voltage fade capacity of ≈ 20% of the initial total capacity.

25 ENERGY STORAGE↗

Electrochemical Modeling and Performance of a Lithium- and Manganese-Rich Layered Transition-Metal Oxide Positive Electrode

The impedance of a lithium- and manganese-rich layered transition-metal oxide (MR-NMC) positive electrode, specifically Li 1.2 Ni 0.15 Mn 0.55 Co 0.1 O 2 , is compared to two other transition-metal layered oxide materials, specifically LiNi 0.8 Co 0.15 Al 0.05 O 2 (NCA) and Li 1.05 (Ni 1/3 Co 1/3 Mn 1/3 ) 0.95 O 2 (NMC). A more detailed electrochemical impedance spectroscopy (EIS) study is conducted on the LMR-NMC electrode, which includes a range of states-of-charge (SOCs) for both current directions (i.e. charge and discharge) and two relaxation times (i.e. hours and one hundred hours) before the EIS sweep. The LMR-NMC electrode EIS studies are supported by half-cell constant current and galvanostatic intermittent titration technique (GITT) studies. Two types of electrochemical models are utilized to examine the results. The first type is a lithium ion cell electrochemical model for intercalation active material electrodes that includes a complex active material/electrolyte interfacial structure. In conclusion, the other is a lithium ion half-cell electrochemical model that focuses on the unique composite structure of the bulk LMR-NMC materials.

25 ENERGY STORAGE↗

Unexpected Voltage Fade in LMR-NMC Oxides Cycled below the “Activation” Plateau

A common feature of lithium-excess layered oxides, nominally of composition xLi 2 MnO 3 •(1-x)LiMO 2 (M = transition metal) is a high-voltage plateau (~4.5 V vs. Li/Li + ) in their capacity-voltage profile during the first delithiation cycle. This plateau is believed to result from activation of the Li 2 MnO 3 component, which makes additional lithium available for electrochemical cycling. However, oxides cycled beyond this activation plateau are known to display voltage fade which is a continuous reduction in their equilibrium potential. In this article we show that these oxides display gradual voltage fade even on electrochemical cycling in voltage ranges well below the activation plateau. The average fade is ~0.08 mV-cycle-1 for Li 1.2 Ni 0.15 Mn 0.55 Co 0.1 O 2 vs. Li cells after 20 cycles in the 2–4.1 V range at 55°C; a ~54 mV voltage hysteresis, expressed as the difference in average cell voltage between charge and discharge cycles, is also observed. The voltage fade results from a gradual accumulation of local spinel environments in the crystal structure. Some of these spinel sites result from lithium deficiencies during oxide synthesis and are likely to be at the particle surfaces; other sites result from the migration of transition metal atoms in the partially-delithiated LiMO 2 component into the lithium planes during electrochemical cycling. The observed rate of voltage fade depends on a combination of factors that includes the phase equilibrium between the layered and spinel components and the kinetics of transition metal migration.

Li, Yan↗

From coin cells to 400 mAh pouch cells: Enhancing performance of high-capacity lithium-ion cells via modifications in electrode constitution and fabrication

In this article we describe efforts to improve performance and cycle life of cells containing Li1.2Ni0.15Mn0.55Co0.1O2-based positive and graphite-based negative electrodes. Initial work to identify high-performing materials, compositions, fabrication variables, and cycling conditions is conducted in coin cells. The resulting information is then used for the preparation of double-sided electrodes, assembly of pouch cells, and electrochemical testing. We report the cycling performance of cells with electrodes prepared under various conditions. Our data indicate that cells with positive electrodes containing 92 wt% Li1.2Ni0.15Mn0.55Co0.1O2, 4 wt% carbons (no graphite), and 4 wt% PVdF (92-4-4) show ~20% capacity fade after 1000 cycles in the 2.5-4.4V range, significantly better than our baseline cells that show the same fade after only 450 cycles. Our analyses indicate that the major contributors to cell energy fade are capacity loss and impedance rise. Therefore incorporating approaches that minimize capacity fade and impedance rise, such as electrode coatings and electrolyte additives, can significantly enhance calendar and cycle life of this promising cell chemistry.

Electrode fabrication↗

Nanostructured light-absorbing crystalline CuIn{sub (1–x)}Ga{sub x}Se{sub 2} thin films grown through high flux, low energy ion irradiation

A hybrid effusion/sputtering vacuum system was modified with an inductively coupled plasma (ICP) coil enabling ion assisted physical vapor deposition of CuIn{sub 1−x}Ga{sub x}Se{sub 2} thin films on GaAs single crystals and stainless steel foils. With <80 W rf power to the ICP coil at 620–740 °C, film morphologies were unchanged compared to those grown without the ICP. At low temperature (600–670 °C) and high rf power (80–400 W), a light absorbing nanostructured highly anisotropic platelet morphology was produced with surface planes dominated by (112){sub T} facets. At 80–400 W rf power and 640–740 °C, both interconnected void and small platelet morphologies were observed while at >270 W and above >715 °C nanostructured pillars with large inter-pillar voids were produced. The latter appeared black and exhibited a strong (112){sub T} texture with interpillar twist angles of ±8°. Application of a negative dc bias of 0–50 V to the film during growth was not found to alter the film morphology or stoichiometry. The results are interpreted as resulting from the plasma causing strong etching favoring formation of (112){sub T} planes and preferential nucleation of new grains, balanced against conventional thermal diffusion and normal growth mechanisms at higher temperatures. The absence of effects due to applied substrate bias suggests that physical sputtering or ion bombardment effects were minimal. The nanostructured platelet and pillar films were found to exhibit less than one percent reflectivity at angles up to 75° from the surface normal.

36 MATERIALS SCIENCE↗