Electronic Processes in CdIn{sub 2}Te{sub 4} Crystals

The results of investigations of electrical, optical, and photoelectric properties of CdIn{sub 2}Te{sup 4} crystals, which were grown by the Bridgman method are presented. It is shown that electrical conductivity is determined mainly by electrons with the effective mass m{sub n} = 0.44m{sub 0} and the mobility 120–140 cm{sup 2}/(V s), which weakly depends on temperature. CdIn{sub 2}Te{sub 4} behaves as a partially compensated semiconductor with the donor-center ionization energy E{sub d} = 0.38 eV and the compensation level K = N{sub a}/N{sub d} = 0.36. The absorption-coefficient spectra at the energy hν < E{sub g} = 1.27 eV are subject to the Urbach rule with a typical energy of 18–25 meV. The photoconductivity depends on the sample thickness. The diffusion length, the charge-carrier lifetime, and the surface-recombination rate are determined from the photoconductivity spectra.

36 MATERIALS SCIENCE↗

Impurity levels in Hg{sub 3}In{sub 2}Te{sub 6} crystals

The parameters of impurity levels in Hg{sub 3}In{sub 2}Te{sub 6} samples are studied using the temperature dependences of the electron concentration n(T) and the Fermi-level energy E{sub F}(T). The dependences n(T) and E{sub F}(T) are obtained from data on the Hall coefficient R(T) and the thermopower α(T). Differential analysis of the dependences n(T) shows that, under variations in the degree of compensation by heat treatment of the samples, a wider spectrum of impurity levels in the band gap of Hg{sub 3}In{sub 2}Te{sub 6} can be analyzed.

36 MATERIALS SCIENCE↗

Behavior of the Fe impurity in Hg{sup 3}In{sup 2}Te{sup 6} crystals

Optical and photoelectric measurements reveal that doping with iron leads to the formation of a deep level at E{sup c}–0.69 eV in Hg{sup 3}In{sup 2}Te{sup 6} crystals. When light is absorbed by Fe{sup 2+} impurity centers, both electronic transitions of the impurity-level–conduction-band type and optical transitions between ground and excited states of the aforementioned centers (intracenter transitions) are observed. Investigations of transport phenomena point to the acceptor properties of Fe{sup 2+} centers.

36 MATERIALS SCIENCE↗

Electrical and optical properties of Mn-doped Hg{sub 3}In{sub 2}Te{sub 6} crystals

The effect of Mn impurities on the properties of Hg{sub 3}In{sub 2}Te{sub 6} crystals is studied by electrical and optical measurements. It is shown that, despite the high dopant concentration (1 Multiplication-Sign 10{sup 19} cm{sup -3}), the electron concentration remains the same as that in an undoped crystal ({approx}10{sup 13} cm{sup -3} at 300 K). At the same time, narrowing of the band gap from 0.74 to 0.7 eV is observed. From an analysis of the absorption spectra, it is found that the absorption edge is formed by optical transitions involving density-of-states (DoS) tails and that two acceptor- and donor-type impurity bands are formed in the band gap. The two bands are described by a Gaussian distribution of the DoS, with an energy gap between the peaks of E{sub 0} = E{sub d}{sup 0} - E{sub a}{sup 0} = 0.4 eV. The total donor and acceptor concentration N{sub d} + N{sub a} and the degree of compensation K = N{sub a}/N{sub d} {yields} 1 are determined. Such compensation is responsible for pinning of the Fermi level near the middle of the band gap and for quasi-intrinsic conductivity at temperatures T {>=} 300 K.

36 MATERIALS SCIENCE↗