Search NASA⌕ Search

Engineering topics

Bliem, Roland

Publications and source records attributed to Bliem, Roland.

Tuning Point Defects by Elastic Strain Modulates Nanoparticle Exsolution on Perovskite Oxides

Exsolution generates stable and catalytically active metal nanoparticles via phase precipitation out of a host oxide. An ability to control the size and dispersion of the exsolution particles is desirable for design of nanostructured (electro)catalysts. In this work, we demonstrate that tuning point defects by lattice strain affects both the thermodynamics and the kinetics of iron (Fe 0 ) exsolution on La 0.6 Sr 0.4 FeO 3 (LSF) thin film model. By combining in situ surface characterization and ab initio defect modeling, we show oxygen vacancy and Schottky defects to be the primary point defects formed upon Fe0 exsolution. Lattice strain tunes the formation energy, and thus the abundance of these defects, and alters the amount and size of the resulting exsolution particles. In addition, we find that the density of exsolved nanoparticles matches the concentration of oxygen vacancy pairs, thus pointing to the surface oxygen vacancy pairs as preferential nucleation sites for exsolution. The tensile-strained LSF with a facile formation of these critical point defects results in a higher Fe 0 metal concentration, a larger density of nanoparticles, and a reduced particle size at its surfaces. These results provide important mechanistic insights and highlight the role of point-defect engineering in designing nanostructured catalysts in energy and fuel conversion technologies.

36 MATERIALS SCIENCE↗

Thermally Driven Interfacial Degradation between Li 7 La 3 Zr 2 O 12 Electrolyte and LiNi 0.6 Mn 0.2 Co 0.2 O 2 Cathode

Solid-state batteries offer higher energy density and enhanced safety compared to the present lithium-ion batteries using liquid electrolytes. A challenge to implement them is the high resistances, especially at the solid electrolyte interface with the cathode. Sintering at elevated temperature is needed in order to get good contact between the ceramic solid electrolyte and oxide cathodes and thus to reduce contact resistances. Many solid electrolyte and cathode materials react to form secondary phases. It is necessary to find out which phases arise as a result of interface sintering and evaluate their effect on electrochemical properties. Herein, we assessed the interfacial reactions between LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and Li 7 La 3 Zr 2 O 12 (LLZO) as a function of temperature in air. We prepared model systems by depositing thin-film NMC622 cathode layers on LLZO pellets. The thin-film cathode approach enabled us to use interface-sensitive techniques such as X-ray absorption spectroscopy in the near-edge as well as the extended regimes and identify the onset of detrimental reactions. We found that the Ni and Co chemical environments change already at moderate temperatures, on-setting from 500 °C and becoming especially prominent at 700 °C. By analyzing spectroscopy results along with X-ray diffraction, we identified Li 2 CO 3 , La 2 Zr 2 O 7 , and La(Ni,Co)O 3 as the secondary phases that formed at 700 °C. The interfacial resistance for Li transfer, measured by electrochemical impedance spectroscopy, increases significantly upon the onset and evolution of the detected interface chemistry. Our findings suggest that limiting the bonding temperature and avoiding CO 2 in the sintering environment can help to remedy the interfacial degradation.

36 MATERIALS SCIENCE↗