Search NASA⌕ Search

Engineering topics

Bloom, Ira

Publications and source records attributed to Bloom, Ira.

At least 55 records · Page 3

Stabilized Electrode/Electrolyte Interphase by a Saturated Ionic Liquid Electrolyte for High-Voltage NMC532/Si-Graphite Cells

Nonaqueous electrolyte has become one of the technical barriers in enabling Li-ion battery comprising of a high voltage cathode and high capacity anode. Here, we demonstrate a saturated piperidinum bis(fluorosulfonyl)imide ionic liquid (IL) with a LiFSI salt not only supports the redox reaction on the cathode at high voltages, but also shows exceptional kinetic stability on the lithiated anode as evidenced by its improved cycling performance in a NMC532/Si-graphite full cells cycled between 4.6 and 3.0 V. On the basis of the spectroscopic/microscopic analysis and molecular dynamics (MD) simulations, the superior performance of the cells is attributed to the formation of solid-electrolyte-interphase on both electrode as well as unique solvation structure where a deadlocked coordination network is established at the saturated state, which prevents transition metal dissolution into the electrolyte via a solvation process.

25 ENERGY STORAGE↗

Graphite Lithiation under Fast Charging Conditions: Atomistic Modeling Insights

The charging of lithium ion batteries in a fast and safe manner is critical for promoting the mass adoption of electric vehicles. Li intercalation in graphite electrodes is known to be one of the bottlenecks during the fast charging process. The mechanism of Li diffusion in highly polarized graphite anode at high current rates remains, however, not well understood. In this work, Density Functional Theory (DFT) calculations are used to gain insights into the Li diffusion process in graphite when it is far from equilibrium under fast charging conditions. The effect of uncompensated charges on Li mobility is determined in the highly polarized regions of the anode close to the interfaces. The extra charge was found to increase the interlayer spacing in the diffusion layer and adjacent channels, increasing the diffusivity and promoting the formation of Li clusters. A concerted diffusion mechanism at the edge of high-concentration Li domains is proposed to enhance the diffusion of Li.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Transition-Metal Dissolution from NMC-Family Oxides: A Case Study

In this work we investigated the static reactions of highly delithiated Li(Ni 1/3 Mn 1/3 Co 1/3 )O 2 , Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 , Li(Ni 0.6 Mn 0.2 Co 0.2 )O 2 , and Li(Ni 0.8 Mn 0.1 Co 0.1 )O 2 positive electrodes with 2,3-butanedione and with tetrabutyl ammonium bifluoride as model leaching agents. In the bifluoride trials, it was found that [Ni] in the leachate was proportional to X Co ( X Ni ) 3 , where X M is the ideal stoichiometry in the bulk oxide, and inversely proportional to ( X Mn ) 2 ; [Mn] to X Co ( X Ni ); and [Co] to X Co . The relationships between metal concentrations and stoichiometry may indicate that nickel, as a next-nearest neighbor on the positive electrode surface, can make dissolution more favorable in some instances.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrode scale and electrolyte transport effects on extreme fast charging of lithium-ion cells

A combination of cell testing and electrochemical modeling is used to investigate extreme fast charging (XFC) performance for cells with a low loading of 1.5 mAh.cm -2 and moderate loading of 2.5 mAh.cm -2 . Cells with a low loading of 1.5 mAh.cm -2 withstand XFC performance remarkably well even up to 9C CC charging with high charge acceptance and very little lithium plating. For a moderate loading of 2.5 mAh.cm -2 , the 6C CC charge capacity is poor with significant amounts of lithium plating. Insufficient electrolyte transport properties are shown to be a major limitation for XFC performance of moderate and high loading cells. Charging at elevated temperature is shown to be an effective strategy for moderate loading cells enabling good 10-minute charge acceptance and mitigating lithium plating. Finally, the electrochemical model is used to investigate strategies for enabling 4-6C CC charging for cells with a loading of 3-4 mAh.cm -2 . A combination of elevated temperature, reduced tortuosity, and electrolytes with improved transport are likely needed to enable XFC for high energy density cells.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /Graphite cells–effect of binder

Cells based on NMC/graphite, containing styrene-butadiene rubber/carboxymethylcellulose binder in the anodes and pVdF latex/carboxymethykellulose in the cathodes, were systematically overcharged to 100, 120, 140, 160, 180, 250% and 270% state-of-charge. The impact of the binder was characterized by elemental analysis, SEM, and HPLC. These results were compared to similar cells just using the poly (vinylidene difluoride) binder. Not only did the binder impact the rate of transition metal transport from the cathode to the anode, it also had a marked effect on the microstructure and composition of the materials on the anode surface.

25 ENERGY STORAGE↗

Effect of binder on the overcharge response in LiFePO 4 -containing cells

Two types of small pouch cells based on LiFePO 4 /graphite, one containing a N-methyl pyrrolidinone (NMP)-soluble binder, poly(vinylidene difluoride), and the other an aqueous-soluble binder, styrene-butadiene rubber/carboxymethylcellulose were systematically charged to 100, 120, 140, 160, 180, and 250% state of charge (SOC). The cells were then discharged to 3.0 V at room temperature before being disassembled for postmortem analysis. Microstructural changes in the anode associated with increasing SOC were more pronounced in the aqueous processed cells in comparison to the NMP-processed cells. Dendrite formation was observed on the aqueous-processed anode at 120% SOC, while the NMP-processed anode surface does not show dendrites until 250% SOC. Overall, the aqueous-processed anode surfaces displayed more evidence of microstructural degradation as a function of increasing SOC. In the NMP-processed cells, four organic compounds on the anode surface were found to show a dependence on SOC, while only two displayed a similar dependency in the aqueous-processed cells. The nature of the binder changed the number and composition of the species found at the anode.

25 ENERGY STORAGE↗

Effect of formation protocol: Cells containing Si-Graphite composite electrodes

The effect of formation protocol was observed in tests using small pouch cells containing silicon-graphite/Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 chemistry. The time for the formation protocol was either 13.2 or 186 h for the tested cells. It is demonstrated that the “fast” formation protocol produces cells with similar performance characteristics to that of the “slow” protocol. Moreover, the solid-electrolyte interface layers from both formation protocols are stable and function analogously, albeit with different chemistry. The fast formation protocol may thus allow a more economical route to cell fabrication.

25 ENERGY STORAGE↗

Liquid ammonia chemical lithiation: an approach for high energy and high voltage Si-graphite | Li 1+ x Ni 0.5 Mn 1.5 O 4 Li-ion batteries

Chemical lithiation using lithium metal dissolved in liquid ammonia is introduced for the first time as a viable, potentially scalable method to over-lithiate cathode materials, in this case, the 5V spinel Li 1+ x Ni 0.5 Mn 1.5 O 4 . In this formula the value of x represents the amount of extra lithium inserted into the spinel. Such over-lithiated cathodes can subsequently be used to pre-lithiate high-energy anodes in a lithium-ion battery configuration during the first charge step. Lithiated 5V spinel Li 1+ x Ni 0.5 Mn 1.5 O 4 cathode materials prepared by this technique show higher first delithiation capacities, confirming the chemically inserted lithium is electrochemically active. Full cells with a Si-graphite anode and the Li 1+ x Ni 0.5 Mn 1.5 O 4 (x=0.62) cathode show a 23 % higher reversible capacity in the first cycle than LiNi 0.5 Mn 1.5 O 4 baseline cells, and improved capacity retention. The extra, chemically inserted lithium therefore sacrificially compensates for the loss of lithium at the anode allowing higher utilization of the cathode capacity in following cycles.

25 ENERGY STORAGE↗

Extreme Fast Charge Challenges for Lithium-Ion Battery: Variability and Positive Electrode Issues

Enabling a 10 min fast charge for electric vehicles is a possible route to reduce range anxiety and increase the utility of electric vehicles. While lithium plating during fast charging is a known challenge, the full suite of limitations which occur in full cells during a 10 min fast charge are unknown. In the present work the central constraints of extreme fast charging are explored through extensive experiments and analysis in single layer graphite/NMC532 pouch cells. Methods of developing fast-charging protocols considering the impedance and transport limitations are presented and the relative benefits of altering the charging rate, profile, relaxation, etc., are investigated. Analysis during and at the end of cycling identified both known and unexpected aging pathways. The most distinct outcomes from the work are a significant increase in cell-to-cell variability as the number of fast charge cycles increase [up to 11% (1σ)] and the identification of distinct aging of the NMC532 positive electrode including cracking of the secondary particles and a trend toward under-lithiation of the positive electrode. Here, while significant aging of the positive electrode was observed, only a few conditions had discernible Li plating and no distinct reversible Li signature was seen during periodic reference performance tests.

25 ENERGY STORAGE↗

Effect of overcharge on lithium-ion cells: Silicon/graphite anodes

Small pouch cells containing Si/graphite electrodes were systematically charged to 100, 120, 140, 160, 180 and 250% state of charge. Description of the Si/graphite electrode after the overcharge showed some features similar to those found in a pure graphite electrode. Since the amount of silicon in the electrode was ~15 wt%, this was not unexpected. The effect of silicon was observed in the composition of the SEI layer and the trends in two components of the SEI layer.

25 ENERGY STORAGE↗

Modeling memoryless degradation under variable stress

Accelerated degradation tests can be used as the basis for predicting the performance or state of health of products and materials at use conditions over time. Measurements acquired at accelerated levels of stress are used to develop models that relate to the degradation of one or more performance measures. Frequently, products/materials of interest are subjected to variable stress levels during their lifetimes. However, testing is usually performed only at a few fixed stress levels. In such cases, cumulative degradation models are developed and assessed by using data acquired under those fixed stress conditions. The degradation rate at any stress condition within the range of the model can be estimated by the derivative of the cumulative model at that stress condition. It follows that, to predict cumulative degradation over variable use conditions, one might integrate the fluctuating degradation rate over time. Existing approaches for doing this consider degradation rates that depend only on the current stress level. Here, we propose to allow the degradation rate to also depend on the current state of health as indicated by the associated performance measure(s). The resulting modeling approach is capable of portraying a broader range of degradation behavior than existing approaches. The assertion of memoryless degradation by using this or any other approach should be assessed experimentally with data acquired under variable stress in order to increase confidence that the integrated rate model is accurate. In this article, we demonstrate the additional capability of the proposed approach by developing empirical memoryless rate-based degradation models to predict resistance increase and capacity decrease in lithium-ion cells that are being evaluated for use in electric vehicles. Here, we then assess the plausibility of these models.

42 ENGINEERING↗

Decomposition of Phosphorus-Containing Additives at a Charged NMC Surface through Potentiostatic Holds

In this work, multiple phosphorus-containing compounds were evaluated as electrolyte additives for their reactivity at the cathode surface using LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) // Li 4 Ti 5 O 12 (LTO) cells with both cycling and high voltage potentiostatic holds. Additives surveyed include phosphite and phosphate derivatives with either trifluoroethyl, ethyl, or trimethylsilyl groups. With the same substituents, phosphite additives showed lower Coulombic efficiency (CE) and higher oxidation current during the potentiostatic hold. Regardless of substitution group, all phosphates showed slightly higher CE than the additive-free electrolyte (baseline), although no additive significantly decreases oxidation reactions over the course of the potentiostatic hold. Post-mortem X-ray photoelectron spectroscopy analysis of the cathodes indicates that the additive with trimethylsilyl group leads to significantly higher incidence of oxygen and phosphorus on the cathode surface for both phosphites and phosphates. Atomistic simulations indicate the susceptibility of these additives to electrochemical and chemical oxidation, showing chemical oxidation to be much more likely with the phosphite additives. Lastly, the identity of the ligands on the phosphorus-containing additive can dramatically affect both the decomposition current as well as cathode surface after the potentiostatic hold.

25 ENERGY STORAGE↗

A comparison of methodologies for the non-invasive characterisation of commercial Li-ion cells

Lithium-ion cells currently power almost all electronic devices and power tools; they are a key enabling technology for electric vehicles and are increasingly considered to be the technology of choice for grid storage. In line with this increased applicability, there is furthemore an increase in the development of new commercial lithium-ion cell technologies that incorporate innovative functional components (electrode material compositions and electrolyte formulations) and designs, leading to a diverse range of performance characteristics. The uniqueness of each technology in-turn gives rise to unique evolutions of cell performance as the cell degrades because of usage. Non-destructively measuring and subsequently tracking the evolution of lithium-ion cell characteristics is valuable for both industrial engineers and academic researchers. To proceed in this regard, stakeholders have often devised their own procedures for characterising lithium-ion cells, typically without considering unification, comparability or compatibility. This makes the comparison of technologies difficult. This comprehensive review for the first time has analysed and discusses the various international standards and regulations for the characterisation and electrical testing of lithium-ion cells, specifically for high-power automotive and grid applications. (C) 2019 The Authors. Published by Elsevier Ltd.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /Graphite lithium ion cells with poly(vinylidene fluoride) binder. I - Microstructural changes in the anode

Cells based on NMC/graphite, containing poly(vinylidene difluoride) (PVDF) binders in the positive and negative electrodes, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state-of-charge (SOC). At 250% SOC the cell vented. Scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) of the anodes showed several state-of-overcharge-dependent trends. Starting at 120% SOC, dendrites appeared and increased in concentration as the SOC increased. Dendrite morphology appeared to be dependent on whether the active material was on the “dull” or “shiny” side of the copper collector. Significantly more delamination of the active material from the collector was seen on the “shiny” side of the collector particularly at 180 and 250% SOC. Transition metals were detected at 120% SOC and increased in concentration as the SOC increased. Finally, there was considerable spatial heterogeneity in the microstructures across each laminate with several regions displaying complex layered structures.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 cathodes: NMP-soluble binder. II — Chemical changes in the anode

For this study, cells based on nickel manganese cobalt oxide (NMC)/graphite electrodes, which contained polyvinylidene difluoride (PVDF) binders in the electrodes, were systematically charged to 100, 120, 140, 160, 180, and 250% state of charge (SOC). Characterization of the anodes by inductively-coupled-plasma mass spectrometry (ICP-MS), X-ray photoelectron spectroscopy (XPS), and high-performance liquid chromatography coupled with electrospray ionization mass spectrometry (HPLC-ESI-MS) showed several extent-of-overcharge-dependent trends. The concentrations (by wt) of nickel, manganese, and cobalt in the negative electrode increased with SOC, but the metals remained in the same ratio as that of the positive. Electrolyte reaction products, such as LiF:LiPO 3 , increased with overcharge, as expected. Three organic products were found by HPLC-ESI-MS. From an analysis of the mass spectra, two of these compounds seem to be organophosphates, which were formed by the reaction of polymerized electrolyte decomposition products and PF 3 or O=PF 3 . Their concentration tended to reach a constant ratio. The third was seen at 250% SOC only.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /graphite lithium ion cells with poly(vinylidene fluoride) binder. III — Chemical changes in the cathode

Here, 1.5 Ah pouch cells based on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 cathodes and graphite anodes, both containing poly (vinylidene fluoride) (PVDF) binders, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state of charge (SOC), at which point they vented. The cells were subsequently discharged to 0% SOC and disassembled under an inert atmosphere for characterization. A combination of X-ray photoelectron spectroscopy (XPS), scanning-electron microscopy (SEM), energy-dispersive spectroscopy (EDS), 6 Li SSNMR, and X-ray diffraction (XRD) analysis of the NMC532 cathodes indicates the formation of a thin C- and O-rich cathode electrolyte interphase layer, progressive Li loss above 140% SOC, and retention of the bulk crystal structure at all states of charge.

25 ENERGY STORAGE↗