Search NASA⌕ Search

Engineering topics

Bruemmer, Stephen M

Publications and source records attributed to Bruemmer, Stephen M.

Metal Oxidation Kinetics and the Transition from Thin to Thick Films

We report an investigation of growth kinetics and transition from thin to thick films during metal oxidation. In the thin film limit (< 20 nm), Cabrera and Mott’s theory is usually adopted by explicitly considering ionic drift through the oxide in response to electric fields, where the growth kinetics follow an inverse logarithmic law . It is generally accepted that Wagner’s theory, involving self-diffusion, is valid only in the limit of thick film regime (>1μm) and leads to parabolic growth kinetics , where l is the oxide film thickness. Theory presented here unifies the two models and provides a complete description of oxidation including the transition from thin to thick film. The range of validity of Cabrera and Mott’s theory and Wagner’s theory can be well defined in terms of the Debye-Hückel screening length. The transition from drift-dominated ionic transport for thin film to diffusion-dominated transport for thick film is found to strictly follow the direct logarithmic law that is frequently observed in many experiments.

Oxidation, Cabrera and Mott, Wagner, transition, l↗

Microstructure of the Native Oxide Layer on Ni and Cr-doped Ni Nanoparticles

Metallic or alloy nanoparticles exposed to air at room temperature will be instantaneously oxidized and covered by an oxide layer. However, for most cases, the true structural nature of the oxide layer formed at this stage is hard to determine. In this paper, we report the structure, morphology, and electronic structure (the density of state of both valence and conduction bands measured by a combination of XPS and EELS) of pure Ni and Cr-doped Ni nanoparticles synthesized using a cluster deposition process. Structural characterization carried out at the atomic level using aberration corrected high resolution transmission electron microscopy (HRTEM) in combination with electron and x-ray diffractions reveals that both pure Ni and Cr-doped Ni particles exposed to air at room temperature similarly possesses a core-shell structure of metal core covered by an oxide layer of typically 1.6 nm in thickness. There exists a critical size of ~ 6 nm, below which the particle is fully oxidized. The oxide particle corresponds to the rock-salt structured NiO and is faceted on the (001) planes. XPS of O-1s shows a strong peak that is attributed to (OH)-, which in combination with the atomic level HRTEM imaging indicates that the very top layer of the oxide is hydrolyzed as Ni(OH)2. Chemical composition analysis using EDS, EELS, and XPS indicates that the Cr dopant at the level of ~ 5at% forms solid solution with the Ni lattice. The Cr shows no segregation on the surface or preferential oxidation during the initial oxidation.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

A Generalized Mathematical Framework for Thermal Oxidation Kinetics

We present a generalized mathematical model for thermal oxidation and the growth kinetics of oxide films. The model expands long-standing classical models by taking into account the reaction occurring at the interface as well as transport processes in greater detail. The standard Deal-Grove model (the linear-parabolic rate law) relies on the assumption of quasi-static diffusion that results in a linear concentration profile of, for example, oxidant species in the oxide layer. By relaxing this assumption and resolving the entire problem, three regimes can be clearly identified corresponding to different stages of oxidation. Namely, the oxidation starts with the reaction-controlled regime (described by a linear rate law), is followed by a transitional regime (described by a logarithmic or power law depending on the stoichiometry coefficient m), and ends with the well-known diffusion-controlled regime (described by a parabolic rate law). Deal-Grove's theory is shown to be the lower order approximation of the proposed model. Various oxidation rate laws are unified into a single model to describe the entire oxidation process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Aging Management using Proactive Management of Materials Degradation

The U.S. Nuclear Regulatory Commission (NRC) has undertaken a program to lay the technical foundations for defining proactive actions to manage degradation of materials in light water reactors (LWRs). The current focus is existing plants; however, if applied to new construction, there is potential to better monitor and manage plants throughout their life cycle. This paper discusses the NRC’s Proactive Management of Materials Degradation (PMMD) program and its application to nuclear power plant structures, systems, and components (SSC).

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Insights into Stress Corrosion Cracking Mechanisms from High-Resolution Measurements of Crack-Tip Structures and Compositions

The fundamental basis for mechanistic understanding and modeling of SCC remains in question for many systems. Specific mechanisms controlling SCC can vary with changes in alloy characteristics, applied/residual stress or environmental conditions. The local crack electrochemistry, crack-tip mechanics and material metallurgy are the main factors controlling crack growth. These localized properties are difficult or impossible to measure in active cracks. Nevertheless, it is essential to quantitatively interrogate these crack-tip conditions if mechanistic understanding is to be obtained. A major recent advance has been the ability to investigate SCC cracks and crack tips using high-resolution ATEM techniques. ATEM enables the characterization of SCC cracks including trapped tip solution chemistries, corrosion product/film compositions and structures, and elemental composition gradients and defect microstructures along the crack walls and at the crack tip. A wide variety of methods for imaging and analyses at resolutions down to the atomic level can be used to examine the crack and corrosion film characteristics. Surface films and reaction layers have been examined by cross-sectional TEM techniques, but little work had been conducted on environmentally induced internal cracks until that of Lewis and co-workers [1-3] and the current authors [4-17]. This capability combined with modern ATEM techniques has enabled exciting new insights into corrosion processes occurring at buried interfaces and is being used to identify mechanisms controlling IGSCC in boiling water reactor (BWR) and pressurized water reactor (PWR) components. The objective of this paper is to summarize certain results focused on IGSCC of Fe- base and Ni-base stainless alloys in high-temperature water environments. Representative crack-tip examples will be shown to illustrate specific aspects that are characteristic of SCC in the material/environment combinations. Differences and similarities in crack-tip structures- chemistries will be highlighted comparing Fe-base 316/304SS to Ni-base alloy 600/182 and for tests in oxidizing versus hydrogenated water environments.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

CRACK GROWTH RESPONSE OF ALLOY 152 AND 52 WELD METALS IN SIMULATED PWR PRIMARY WATER

The crack growth response of alloy 152 and 52 weld metals has been measured in simulated PWR primary water at both high (325-350 C) and low (50 C) temperatures. Tests were performed on samples machined from alloy 152 or 52 mockup welds. Propagation rates under cycle + hold and constant K conditions at high temperatures show stable, but extremely low SCC growth rates. The most significant intergranular cracking occurred during cycling at 50 C, particularly for the alloy 152 weld metal at high stress intensity.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

CRACK GROWTH RESPONSE OF ALLOY 690 IN SIMULATED PWR PRIMARY WATER

The stress corrosion crack growth response of three extruded alloy 690 CRDM tube heats was investigated in several thermomechanical conditions. Extremely low propagation rates (< 1 x 10{sup -9} mm/s) were observed under constant stress intensity factor (K) loading at 325-350 C in the as-received, thermally treated (TT) materials despite using a variety of transitioning techniques. Post-test observation of the crack-growth surfaces revealed only isolated intergranular (IG) cracking. One-dimensional cold rolling to 17% reduction and testing in the S-L orientation did not promote enhanced stress corrosion rates. However, somewhat higher propagation rates were observed in a 30% cold-rolled alloy 690TT specimen tested in the T-L orientation. Cracking of the cold-rolled material was promoted on grain boundaries oriented parallel to the rolling plane with the % IG increasing with the amount of cold rolling.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

CHARACTERIZATION OF DEFECTS IN ALLOY 152, 52 AND 52M WELDS

Defect distributions have been documented by optical metallography, scanning electron microscopy and electron backscatter diffraction in alloy 152 and 52 mockups welds, alloy 52 and 52M overlay mockups and an alloy 52M inlay. Primary defects were small cracks at grain boundaries except for more extensive cracking in the dilution zone of an alloy 52 overlay on 304SS. Detailed characterizations of the dilution zone cracks were performed by analytical transmission electron microscopy identifying grain boundary titanium-nitride precipitation associated with the intergranular separations. I. INTRODUCTION Weldments continue to be a primary location of stress-corrosion cracking (SCC) in light-water reactor systems. While problems related to heat-affected-zone (HAZ) sensitization and intergranular (IG) SCC of austenitic stainless alloys in boiling-water reactors (BWRs) have been significantly reduced, SCC has now been observed in HAZs of non-sensitized materials and in dissimilar metal welds where Ni-base alloy weld metals are used. IGSCC in weld metals has been observed in both BWRs and pressurized water reactors (PWRs) with recent examples for PWR pressure vessel penetrations producing the most concern. This has led to the replacement of alloy 600/182/82 welds with higher Cr, more corrosion-resistant replacement materials (alloy 690/152/52/52M). Complicating this issue has been a known susceptibility to cracking during welding [1-7] of these weld metals. There is a critical need for an improved understanding of the weld metal metallurgy and defect formation in Ni-base alloy welds to effectively assess long-term performance. A series of macroscopic to microscopic examinations were performed on available mockup welds made with alloy 52 or alloy 152 plus selected overlay and inlay mockups. The intent was to expand our understanding of weld metal structures in simulated LWR service components with a focus on as-welded defects. Microstructural features, defect distributions, defect characteristics and weld residual strains were examined by optical metallography, scanning electron microscopy, electron backscatter diffraction and transmission electron microscopy. Industry-supplied mock-up welds were characterized including alloy 52 and 152 weldments, alloy 52M overlay and inlay welds, and an alloy 52 overlay. II. WELDMENTS II.A. Alloy 52 and 152 Weld Mockups The alloy 52 and 152 weld mockups were fabricated by MHI for the Kewaunee reactor and were obtained from the EPRI NDE Center. The mockups were U-groove welds joining two plates of 304SS as shown in Figure 1. Alloy 152 butter (heat 307380) was placed on the U-groove surface for both mockups by shielded metal arc welding (SMAW). For the alloy 152 weld mockup, the alloy 152 fill (heat 307380) was also applied using SMAW while for the alloy 52 weld mockup, the alloy 52 fill (heat NX2686JK) was applied using gas tungsten arc welding (GTAW). Welding parameters for the fill materials were substantially different with the alloy 152 SMAW having a deposition speed of 4-25 cm/min with a current of 95-145 A and the alloy 52 GTAW having a deposition speed of 4-10 cm/min with a current of 150-300 A. One prominent feature in these mockup welds is the presence of a crack starting at the 304SS butt joint at the bottom of the U-groove and extending up into the weld. It appears that the 304SS plate on either side of the butt joint acted as an anchor for the weld resulting in a stress rise across the slit that drove crack formation and extension up into the fill weld. As will be shown in the next section, the extent of the cracking around this stress riser was much greater in the MHI 52 weld mockup.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

A Destructive Validation of NDE Responses of Service-Induced PWSCC Found in North Anna 2 Control Rod Drive Nozzle 31

Studies conducted at the Pacific Northwest National Laboratory (PNNL) in Richland, Washington focused on assessing the effectiveness of nondestructive examination (NDE) techniques for inspecting control rod drive mechanism (CRDM) nozzles and J-groove weldments. The primary objective of this work is to provide information to the United States Nuclear Regulatory Commission (NRC) on the effectiveness of NDE methods as related to the in-service inspection of CRDM nozzles and J-groove weldments, and to enhance the knowledge base of primary water stress corrosion cracking (PWSCC) through destructive characterization of the CRDM assemblies.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

LWR Aging Management Using a Proactive Approach to Control Materials Degradation

Material issues can be the limiting factor for the operation of nuclear power plants. There is growing interest in new and improved philosophies and methodolgies for plant life management, which include the migration from reliance on periodic inservice inspection to include condition-based maintenance. A further step in the development of plant management is the move from proactive responses based on ISI to become proactive, through the investigation of the potential for implementation of a proactive management of materials degradation program and its potential impact on the managements of LWRs

Materials Degradation↗

Failure Prevention For Nuclear Power Plants Through Proactive Management of Materials Degradation (PMMD)

Failure prevention is central to the operation of nuclear power plants. To meet this goal there is growing interest in new and improved philosophies and methodologies for plant life management (PLiM), which include the migration from reliance on periodic inservice inspection to include condition-based maintenance. A further step in the development of plant management is the move from reactive responses based on ISI to become proactive, through the investigation of the potential for implementation of a proactive management of materials degradation (PMMD) program and its potential impact on the management of LWRs.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Nano-cavities observed in a 316SS PWR Flux Thimble Tube Irradiated to 33 and 70 dpa

The radiation-induced microstructure of a cold-worked 316SS flux thimble tube from an operating pressurized water reactor (PWR) was examined. Two irradiated conditions, 33 dpa at 290ºC and 70 dpa at 315ºC were examined by transmission electron microscopy. The original dislocation network had completely disappeared and was replaced by fine dispersions of Frank loops and small nano-cavities at high densities. The latter appear to be bubbles containing high levels of helium and hydrogen. An enhanced distribution of these nano-cavities was found at grain boundaries and may play a role in the increased susceptibility of the irradiated 316SS to intergranular failure of specimens from this tube during post-irradiation slow strain rate testing in PWR water conditions.

Edwards, Danny J↗