Origin of rate limitations in solid-state polymer batteries from constrained segmental dynamics within the cathode

Currently, one of the key challenges preventing the wide commercialization of polymer-based solid-state batteries is achieving high-rate capabilities. This work unravels chain structure and segmental dynamics in a polymer-based composite cathode consisting of LiFePO 4 (LFP), carbon, and poly(ethylene oxide) (PEO) with lithium bis(trifluoromethanesulfonyl)imide. Small-angle neutron scattering (SANS) data reveal that PEO chains are adsorbed on the surface of LFP particles during slurry processing to make the composite electrode. The strong interaction between LFP and PEO chains leads to greatly reduced segmental dynamics of PEO, as discovered by quasi-elastic neutron scattering (QENS). The reduced segmental dynamics results in 70% decreased Li + mobility of the polymer electrolyte in the composite cathode. The combined SANS and QENS study indicates that one of the key bottlenecks that limits the rate performance of PEO-based polymer batteries originates from molecular interactions within the cathode.

25 ENERGY STORAGE↗

Understanding the Solution Dynamics and Binding of a PVDF Binder with Silicon, Graphite, and NMC Materials and the Influence on Cycling Performance

The impact of the binding, solution structure, and solution dynamics of poly(vinylidene fluoride) (PVDF) with silicon on its performance as compared to traditional graphite and Li 1.05 Ni 0.33 Mn 0.33 Co 0.33 O 2 (NMC) electrode materials was explored. Through refractive index (RI) measurements, the concentration of the binder adsorbed on the surface of electrode materials during electrode processing was determined to be less than half of the potentially available material resulting in excessive free binder in solution. Using ultrasmall-angle neutron scattering (USANS) and small-angle neutron scattering (SANS), it was found that PVDF forms a conformal coating over the entirety of the silicon particle. This is in direct contrast to graphite–PVDF and NMC–PVDF slurries, where PVDF only covers part of the graphite surface, and the PVDF chains make a network-like graphite–PVDF structure. Conversely, a thick layer of PVDF covers NMC particles, but the coating is porous, allowing for ion and electronic transport. The homogeneous coating of silicon breaks up percolation pathways, resulting in poor cycling performance of silicon materials as widely reported. These results indicate that the Si–PVDF interactions could be modified from a binder to a dispersant.

25 ENERGY STORAGE↗

Competitive adsorption within electrode slurries and impact on cell fabrication and performance

We ask why do battery researchers use 10-20 wt% binder in research cells when commercial chemistries use much less? This report seeks to explore this question by understanding the ordering and structure of polyimide binder with a silicon/pitch-carbon black electrode system. Correlating the effect of binder concentration on electrode architecture and electrochemical properties is vital to enhancing silicon anode cycle and calendar life. Using ultra-small angle neutron scattering (USANS) and binder adsorption isotherms an optimal region of polyimide (PI) binder coverage was found. Further, there is a preferential adsorption of PI to carbon black that has to be completed before PI binds to the silicon. Optimizing the concentration of binder leads to a 50% increase in capacity due to the optimization of binder-silicon-carbon interactions.

25 ENERGY STORAGE↗

Structure and dynamics of small polyimide oligomers with silicon as a function of aging

The effect of UV curing and shearing on the structure and behavior of a polyimide (PI) binder as it disperses silicon particles in a battery electrode slurry was investigated. PI dispersant effectiveness increases with UV curing time, which controls the overall binder molecular weight. Here, the shear force during electrode casting causes higher molecular weight PI to agglomerate, resulting in battery anodes with poorly dispersed Si particles that do not cycle well. It is hypothesized that when PI binder is added above a critical amount, it conformally coats the silicon particles and greatly impedes Li ion transport. There is an “interzonal region” for binder loading where it disperses silicon well and provides a coverage that facilitates Li transport through the anode material and into the silicon particles. These results have implications in ensuring reproducible electrode manufacturing and increasing cell performance by optimizing the PI structure and coordination with the silicon precursor.

36 MATERIALS SCIENCE↗

Direct Measure of Electrode Spatial Heterogeneity: Influence of Processing Conditions on Anode Architecture and Performance

The spatial (in)homogeneity of aqueous processed silicon electrodes using standard poly(acrylic acid)-based binders and slurry preparation conditions is demonstrated in this work. X-ray nanotomography shows segregation of materials into submicron-thick layers depending on the mixing method and starting binder molecular weights. Using a dispersant, or in situ production of dispersant from the cleavage of the binder into smaller molecular weight species, increases the resulting lateral homogeneity while drastically decreasing the vertical homogeneity as a result of sedimentation and separation due to gravitational forces. This data explains some of the variability in the literature with respect to silicon electrode performance and demonstrates two potential ways to improve slurry-based electrode fabrications.

36 MATERIALS SCIENCE↗