Controlling dendrite propagation in solid-state batteries with engineered stress
Metal-dendrite penetration is a mode of electrolyte failure that threatens the viability of metal-anode-based solid-state batteries. Whether dendrites are driven by mechanical failure or electrochemical degradation of solid electrolytes remains an open question. If internal mechanical forces drive failure, superimposing a compressive load that counters internal stress may mitigate dendrite penetration. Here, we investigate this hypothesis by dynamically applying mechanical loads to growing dendrites in Li 6.6 La 3 Zr 1.6 Ta 0.4 O 12 solid electrolytes. Operando microscopy reveals marked deflection in the dendrite growth trajectory at the onset of compressive loading. For sufficient loading, this deflection averts cell failure. Using fracture mechanics, we quantify the impact of stack pressure and in-plane stresses on dendrite trajectory, chart the residual stresses required to prevent short-circuit failure, and propose design approaches to achieve such stresses. For the materials studied here, we show that dendrite propagation is dictated by electrolyte fracture, with electronic leakage playing a negligible role.
SISGR: Chemomechanics of Far-From-Equilibrium Interfaces (COFFEI)
Portable, reliable, and deployable devices for energy storage and conversion require fundamental changes in design of solid-state composites comprising ceramics and metals. These materials comprise the electrodes and electrolytes of next-generation solid-oxide fuel cells and all solid-state batteries, forming solid-state functional composites. The advent of solid-state batteries – which replace liquid electrolytes with solid electrolytes capable of lithium ion transport for reliable energy storage in portable batteries – and the increased demand space for all solid-state fuel cells capable of oxygen reduction at intermediate temperatures remain important challenges for improved material stability and decreased system cost. However, little is understood about three fundamental facets of materials that enable such solid-state energy applications. First, how do such materials deform, fracture, or delaminate under operando conditions? Second, how does such mechanical deformation limit or facilitate electronic and ionic transport within and across such material interfaces? Third, how we can predictably design interface-rich composites to engineer both structural and electrochemical stability? This COFFEI Group comprised expertise from Materials Science & Engineering and Nuclear Science & Engineering to integrate unique in situ experiments, simulations, and fabricated interfaces that address these fundamental questions in solid-state interfaces of nanoscale composites that will guide solid-state electrochemistry, transport kinetics, and mechanical deformation for nonstoichiometric materials that enable such applications. In particular, we built on COFFEI’s understanding of chemomechanical coupling among defect concentrations, ionic transport, electron transport, and stored elastic energy that is particularly acute in the far-from-equilibrium conditions typical of energy device applications. By tailoring our focus to solid-state interfaces, we addressed these important issues by (a) developing and applying advanced in situ and ex situ characterization tools to characterize model materials and interfaces synthesized with molecular-level control, under both laboratory-controlled and extreme environments representative of energy device operation; and (b) employing computational modeling and simulation frameworks to predict transport mechanisms, reactivity and stability of these model materials and interfaces under significant chemical strains typical of energy device operation. Recent progress provided insights to additional materials systems and electrochemomechanical fatigue and fracture that were not fully envisioned when the program was initiated. Specifically, in the final three years of COFFEI we pursued two integrated thrusts, with complementary focus. Thrust I focused on failure-resistant electrochemomechanical composites, while Thrust II focused on strain-modulated conductivity and reactivity across interfaces. In contrast to our initial COFFEI focus, these thrusts concentrated wholly on solid-state material interfacial interactions and included greater integration of multiscale visualization including in situ electron microscopy of strained structures/interactions and mesoscale simulations. Successful development of functionally superior and long-lived battery and fuel cell systems and stress adaptable oxides requires a deeper, fundamental understanding of the coupling among the historically important subfields of solid-state electrochemistry, transport kinetics, and mechanical deformation for nonstoichiometric metal oxide electrodes. In this program, the understanding and the application of chemomechanical coupling of defect concentrations, ionic transport, electro-catalytic activity and stored elastic energy, particularly acute in the far-from-equilibrium conditions typical of energy device applications, are being refined and implications for device operation clarified, including for miniaturized solid-state batteries and fuel cells.
Semi-solid alkali metal electrodes enabling high critical current densities in solid electrolyte batteries
The need for higher energy density rechargeable batteries has generated interest in alkali metal electrodes paired with solid electrolytes. However, metal penetration and electrolyte fracture at low current densities have emerged as fundamental barriers. Here, we show that for pure metals in the Li-Na-K system, the critical current densities scale inversely to mechanical deformation resistance. Furthermore, we demonstrate two electrode architectures in which the presence of a liquid phase enables high current densities while preserving the shape retention and packaging advantages of solid electrodes. First, biphasic Na-K alloys show K + critical current densities (with K-β*-Al 2 O 3 electrolyte) that exceed 15 mA∙cm -2 . Second, introducing a wetting interfacial film of Na-K liquid between Li metal and Li 6.75 La 3 Zr 1.75 Ta 0.25 O 12 (LLZTO) solid electrolyte doubles the critical current density and permits cycling at areal capacities exceeding 3.5 mAh∙cm -2 . These design approaches hold promise for overcoming electro-chemo-mechanical stability issues that have heretofore limited performance of solid-state metal batteries.
Phase-field model for diffusion-induced grain boundary migration: An application to battery electrodes
Diffusion-induced grain boundary migration is a phenomenon in which a grain boundary moves in response to the driving forces generated by diffusing solute species. For example, diffusing solute species change the atomic volume in the host material, either by filling a vacancy with a misfitting solute atom or by expanding host lattices through interstitial diffusion. These volume changes are inhomogeneous and are stored as elastic energy in the material that drives grain boundaries. In this paper, we introduce our previously developed Cahn-Hilliard–phase-field-crystal model (CH-PFC) as a computational tool to investigate diffusion-induced grain boundary migration in crystalline materials. This multiscale phase-field model couples the composition field of a diffusing species with the crystallographic texture of a host material. We apply the CH-PFC model to battery electrodes and investigate whether interstitial solute diffusion induces grain growth in FePO 4 /LiFePO 4 electrodes. To this end, we compute grain growth in 60 FePO 4 electrodes by conducting two parallel trials: In the first trial, we cycle the electrode and calculate diffusion-induced grain growth. In the second trial, we do not cycle the electrode and calculate curvature-driven grain growth. We find a statistically significant grain growth in the cycled electrodes and negligible grain growth in the noncycled electrodes. Altogether, we show that the CH-PFC model not only predicts electrode microstructures as a function of the Li composition, but also predicts the crystallographic features of an electrode during battery operation.
Gravity induced flow cell
The flow cell includes first and second reservoirs having a selected volume containing a flowable redox electrode. A membrane separates charged and discharged material. An energy-extraction region includes electronically conductive porous current collectors through or adjacent to which the flowable redox electrodes flow and to which charge transfer occurs. Structure is provided for altering orientation of the flow cell whereby gravity induces flow of the flowable redox electrode between the first and second reservoirs to deliver power. By varying the angle of the cell, flow rate and power delivered on discharge or the charge rate on charge may be varied.
Mechanical instability of electrode-electrolyte interfaces in solid-state batteries
Not Available
Mesoscopic Phase Transition Kinetics in Secondary Particles of Electrode-Active Materials in Lithium-Ion Batteries
Many compounds used as battery storage electrodes undergo large composition changes during use that are accompanied by a first-order phase transition. Most studies of these phase transitions have focused on the unit cell to single-crystallite scale, whereas real battery electrodes are typically composed of mesoscopic assemblies of nanocrystallites, for which phase transformation mechanisms are poorly understood. Here in this work, a systematic study is conducted of the potentiostatic (constant driving force) kinetics of phase transition in secondary particles of representative intercalation compounds: LiFePO 4 , LiMn 1–x Fe x PO 4 , and Li 4 Ti 5 O 7 . Storage kinetics are studied as a function of overpotential, material composition, primary particle size, and temperature. We find that in regimes where phase transformation occurs, the results can be self-consistently explained as nucleation and growth kinetics within the framework of the Johnson–Mehl–Avrami–Kolmogorov model. This implies that despite the common secondary particle topology, the electrochemically driven phase transformations occur by nucleation and growth with little apparent resistance to phase propagation across the grain boundaries. Growth appears to be one-dimensional in nature, consistent with a hybrid growth model in which rapid surface propagation is followed by slower growth into particles.
Combining phase-field crystal methods with a Cahn-Hilliard model for binary alloys
Diffusion-induced phase transitions typically change the lattice symmetry of the host material. In battery electrodes, for example, Li ions (diffusing species) are inserted between layers in a crystalline electrode material (host). This diffusion induces lattice distortions and defect formations in the electrode. The structural changes to the lattice symmetry affect the host material’s properties. We propose a 2D theoretical framework that couples a Cahn-Hilliard (CH) model, which describes the composition field of a diffusing species, with a phase-field crystal (PFC) model, which describes the host-material lattice symmetry. We couple the two continuum models via coordinate transformation coefficients. We introduce the transformation coefficients in the PFC method to describe affine lattice deformations. These transformation coefficients are modeled as functions of the composition field. Using this coupled approach, we explore the effects of coarse-grained lattice symmetry and distortions on a diffusion-induced phase transition process. In this paper, we demonstrate the working of the CH-PFC model through three representative examples: First, we describe base cases with hexagonal and square symmetries for two composition fields. Next, we illustrate how the CH-PFC method interpolates lattice symmetry across a diffuse phase boundary. Finally, we compute a Cahn-Hilliard type of diffusion and model the accompanying changes to lattice symmetry during a phase transition process.
Random Walk Analysis of the Effect of Mechanical Degradation on All-Solid-State Battery Power
Mechanical and electrochemical phenomena are coupled in defining the battery reliability, particularly for solid-state batteries. Micro-cracks act as barriers to Li-ion diffusion in the electrolyte, increasing the average electrode’s tortuosity. In our previous work, we showed that solid electrolytes are likely to suffer from mechanical degradation if their fracture energy is lower than 4 J m -2 [G. Bucci, T. Swamy, Y.-M. Chiang, and W. C. Carter, J. Mater. Chem. A (2017)]. Here we study the effect of electrolyte micro-cracking on the effective conductivity of composite electrodes. Via random analyzes, we predict the average diffusivity of lithium in a solid-state electrode to decrease linearly with the extension of mechanical degradation. Furthermore, the statistical distribution of first passage times indicates that the microstructure becomes more and more heterogeneous as damage progresses. In addition to power and capacity loss, a non-uniform increase of the electrode tortuosity can lead to heterogeneous lithiation and further stress localization. Finally, the understanding of these phenomena at the mesoscale is essential to the implementation of safe high-energy solid-state batteries.
Modeling of internal mechanical failure of all-solid-state batteries during electrochemical cycling, and implications for battery design
This study is the first quantitative analysis of mechanical reliability of all-solid state batteries. Mechanical degradation of the solid electrolyte (SE) is caused by intercalation-induced expansion of the electrode particles, within the constrains of a dense microstructure. A coupled electro-chemo-mechanical model was implemented to quantify the material properties that cause an SE to fracture. The treatment of microstructural details is essential to the understanding of stress-localization phenomena and fracture. A cohesive zone model is employed to simulate the evolution of damage. In the numerical tests, fracture is prevented when electrode-particle's expansion is lower than 7.5% (typical for most Li-intercalating compounds) and the solid-electrolyte's fracture energy higher than G c = 4 J m -2 . Perhaps counter-intuitively, the analyses show that compliant solid electrolytes (with Young's modulus in the order of E SE = 15 GPa) are more prone to micro-cracking. This result, captured by our non-linear kinematics model, contradicts the speculation that sulfide SEs are more suitable for the design of bulk-type batteries than oxide SEs. Mechanical degradation is linked to the battery power-density. Fracture in solid Li-ion conductors represents a barrier for Li transport, and accelerates the decay of rate performance.
High energy density redox flow device
Redox flow devices are described including a positive electrode current collector, a negative electrode current collector, and an ion-permeable membrane separating said positive and negative current collectors, positioned and arranged to define a positive electroactive zone and a negative electroactive zone; wherein at least one of said positive and negative electroactive zone comprises a flowable semi-solid composition comprising ion storage compound particles capable of taking up or releasing said ions during operation of the cell, and wherein the ion storage compound particles have a polydisperse size distribution in which the finest particles present in at least 5 vol % of the total volume, is at least a factor of 5 smaller than the largest particles present in at least 5 vol % of the total volume.
Metal sulfide electrodes and energy storage devices thereof
The present invention generally relates to energy storage devices, and to metal sulfide energy storage devices in particular. Some aspects of the invention relate to energy storage devices comprising at least one flowable electrode, wherein the flowable electrode comprises an electroactive metal sulfide material suspended and/or dissolved in a carrier fluid. In some embodiments, the flowable electrode further comprises a plurality of electronically conductive particles suspended and/or dissolved in the carrier fluid, wherein the electronically conductive particles form a percolating conductive network. An energy storage device comprising a flowable electrode comprising a metal sulfide electroactive material and a percolating conductive network may advantageously exhibit, upon reversible cycling, higher energy densities and specific capacities than conventional energy storage devices.
Solvent effects on polysulfide redox kinetics and ionic conductivity in lithium-sulfur batteries
Lithium-sulfur (Li-S) batteries have high theoretical energy density and low raw materials cost compared to present lithium-ion batteries and are thus promising for use in electric transportation and other applications. A major obstacle for Li-S batteries is low rate capability, especially at the low electrolyte/sulfur (E/S) ratios required for high energy density. Herein, we investigate several potentially rate-limiting factors for Li-S batteries. We study the ionic conductivity of lithium polysulfide solutions of varying concentration and in different ether-based solvents and their exchange current density on glassy carbon working electrodes. We believe this is the first such investigation of exchange current density for lithium polysulfide in solution. Exchange current densities are measured using both electrochemical impedance spectroscopy and steady-state galvanostatic polarization. In the range of interest (1-8 M [S]), the ionic conductivity monotonically decreases with increasing sulfur concentration while exchange current density shows a more complicated relationship to sulfur concentration. The electrolyte solvent dramatically affects ionic conductivity and exchange current density. Finally, the measured ionic conductivities and exchange current densities are also used to interpret the overpotential and rate capability of polysulfide-nanocarbon suspensions; this analysis demonstrates that ionic conductivity is the rate-limiting property in the solution regime (i.e. between Li 2 S 8 and Li 2 S 4 ).
Formulation of the coupled electrochemical–mechanical boundary-value problem, with applications to transport of multiple charged species
Not Available