Sequential Fe Reduction, Involving Two Different Fe + Intermediates, in the Conversion Reaction of Prussian Blue in Lithium-Ion Batteries

In this work, ex situ X-ray absorption spectroscopy and in operando 57 Fe-Mössbauer spectroscopy measurements are conducted to examine in detail the ongoing reaction mechanism of potassium Prussian blue (K-PB) within the narrow [1.6–0.005 V] voltage range, and so to determine whether this material truly undergoes a conversion reaction, as we proposed elsewhere. The generation of Fe 0 is confirmed by both techniques, finding that 40 to 58% of iron gets reduced to metallic iron at 5 mV. The elucidation of the mechanism by in situ 57 Fe-Mössbauer spectroscopy further reveals a sequential process for the reduction (lithiation) of the two different iron species initially present in Prussian blue. Both high-spin Fe 2+ –N first and low-spin Fe II –C next go through the unusual Fe 1+/I formal oxidation state during the reduction process, before forming surface Fe 0 nanoparticles (NPs) below 0.48 V. Upon charge, Fe 0 NPs preferentially oxidizes into Fe + –N. Interestingly, these surprising Fe + species play an important role in decreasing the overpotential during the charge (delithiation) process with respect to other conversion systems.

25 ENERGY STORAGE↗

Revisiting metal fluorides as lithium-ion battery cathodes

Metal fluorides, promising lithium-ion battery cathode materials, have been classified as conversion materials due to the reconstructive phase transitions widely presumed to occur upon lithiation. We challenge this view by studying FeF 3 using X-ray total scattering and electron diffraction techniques that measure structure over multiple length scales coupled with density functional theory calculations, and by revisiting prior experimental studies of FeF 2 and CuF 2 . Metal fluoride lithiation is instead dominated by diffusion-controlled displacement mechanisms, and a clear topological relationship between the metal fluoride F- sublattices and that of LiF is established. Initial lithiation of FeF3 forms FeF2 on the particle's surface, along with a cation-ordered and stacking-disordered phase, A-Li x Fe y F 3 , which is structurally related to alpha-/beta-LiMn 2+ Fe 3+ F 6 and which topotactically transforms to B- and then C-Li x Fe y F 3 , before forming LiF and Fe. Lithiation of FeF 2 and CuF 2 results in a buffer phase between FeF 2 /CuF 2 and LiF. Overall, the resulting principles will aid future developments of a wider range of isomorphic metal fluorides.

25 ENERGY STORAGE↗