Develop and demonstrate manufacturing processes for fabricating graphite filament reinforced polymide (Gr/PI) composite structural elements

A study was conducted to assess the merits of using graphite/polyimide, NR-150B2 resin, for structural applications on advanced space launch vehicles. The program was divided into two phases: (1) Fabrication Process Development; and (2) Demonstration Components. The first phase of the program involved the selection of a graphite fiber, quality assurance of the NR-150B2 polyimide resin, and the quality assurance of the graphite/polyimide prepreg. In the second phase of the program, a limited number of components were fabricated before the NR-150B2 resin system was removed from the market by the supplier, Du Pont. The advancement of the NR-150B2 polyimide resin binder was found to vary significantly based on previous time and temperature history during the prepregging operation. Strength retention at 316C (600F) was found to be 50% that of room temperature strength. However, the composite would retain its initial strength after 200 hours exposure at 316C (600F). Basic chemistry studies are required for determining NR-150B2 resin binder quality assurance parameters. Graphite fibers are available that can withstand high temperature cure and postcure cycles.

Chase, V. A.↗

Composite seals for liquid hydrogen and nuclear radiation environments.

Description of plastic composite seals for service in a liquid-hydrogen and nuclear-radiation environment. The radiation-resistant aromatic heterocyclic class of polymers, including polyimide, polybenzimidazole, and polyquinoxaline, were evaluated for this application. The seal developed is based on a design involving a resin-starved laminate consisting of alternating layers of woven glass fabric and polymer film. This design imparts a mechanical spring characteristic to the seal, resulting in essentially complete elastic recovery when unloaded, and eliminates cold flow. Encapsulating techniques employing the polyquinoxaline polymer were developed which rendered the seal impervious to liquid hydrogen. The seals were tested before and after gamma irradiation up to 10 to the 10th ergs/g. Load/deflection and leakage tests were performed over a temperature range from -423 through +500 F.

Van Auken, R. L.↗