Anomalous Thermal Decomposition Behavior of Polycrystalline LiNi 0.8 Mn 0.1 Co 0.1 O 2 in PEO-Based Solid Polymer Electrolyte

we report that replacing liquid electrolytes (LEs) with polymer electrolytes has been considered a promising approach to developing next-generation lithium-ion batteries (LIBs) with high energy density and superior safety. Nevertheless, compared with the extensive research on the electrochemical stability of the cathode/polymer electrolyte interfaces, reports on their thermal behaviors are rare to date. Herein, this work systematically investigates the thermal stability of two typical layered oxide cathodes, LiCoO 2 (LCO) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), with poly(ethylene oxide) (PEO) electrolyte and with carbonate LEs, respectively. It is found that the oxygen release from the cathodes plays a central role in thermal runaway. Replacing the LE with PEO electrolyte can considerably improve the thermal stability of LCO, but surprisingly, deteriorate that of NMC811. The reason is that the surface of single-crystalline LCO particles can be effectively passivated by the PEO electrolyte during heating, but PEO cannot sufficiently passivate all the primary particles of NMC811 owing to insufficient interface wettability of PEO electrolyte within the polycrystalline secondary NMC811 particles. The findings in this work collectively formulate valuable guidance for improving the safety of polymer-electrolyte-based as well as other types of all-solid-state lithium-ion batteries.

25 ENERGY STORAGE↗

Enabling Stable Cycling of 4.2 V High-Voltage All-Solid-State Batteries with PEO-Based Solid Electrolyte

Poly(ethylene oxide) (PEO)-based solid electrolytes are expected to be exploited in solid-state batteries with high safety. Its narrow electrochemical window, however, limits the potential for high voltage and high energy density applications. In this paper, the electrochemical oxidation behavior of PEO and the failure mechanisms of LiCoO 2 -PEO solid-state batteries are studied. It is found that although for pure PEO it starts to oxidize at a voltage of above 3.9 V versus Li/Li + , the decomposition products have appropriate Li + conductivity that unexpectedly form a relatively stable cathode electrolyte interphase (CEI) layer at the PEO and electrode interface. The performance degradation of the LiCoO 2 -PEO battery originates from the strong oxidizing ability of LiCoO 2 after delithiation at high voltages, which accelerates the decomposition of PEO and drives the self-oxygen-release of LiCoO 2 , leading to the unceasing growth of CEI and the destruction of the LiCoO 2 surface. When LiCoO 2 is well coated or a stable cathode LiMn 0.7 Fe 0.3 PO 4 is used, a substantially improved electrochemical performance can be achieved, with 88.6% capacity retention after 50 cycles for Li 1.4 Al 0.4 Ti 1.6 (PO 4 ) 3 coated LiCoO 2 and 90.3% capacity retention after 100 cycles for LiMn 0.7 Fe 0.3 PO 4 . The results suggest that, when paired with stable cathodes, the PEO-based solid polymer electrolytes could be compatible with high voltage operation.

25 ENERGY STORAGE↗