All solid thick oxide cathodes based on low temperature sintering for high energy solid batteries

Solid-state batteries (SSBs) could significantly improve the safety and energy density over conventional liquid cells. One key enabling technology is the use of solid electrolytes. NASICON-type Li 1.3 Al 0.3 Ti 1.7 (PO 4 ) 3 (LATP) is a very attractive solid-state electrolyte for the cathode side due to its high oxidation potential and high ionic conductivity. The usage, however, is limited by its large interfacial resistance against most of the cathode materials as well as the thermodynamic instability during high temperature sintering needed to achieve high mass density. Here we construct thin, percolative, and mixed conductive interphases through in situ low-melting-point liquid sintering. These mixed conductive interphases drastically improve the kinetics, leading to high-loading solid LATP/LiCoO 2 cathodes achieving capacity loading of up to ~6 mA h cm –2 . The technique is also applicable to Ni-rich cathode materials, achieving up to ~10 mAh cm –2 , which can lead to more than 400 W h kg –1 cells in SSBs. Furthermore, our composite cathodes show a ten-times and three-times area capacity improvement over the state-of-the-art cathodes using oxide and sulfide SSEs, respectively.

25 ENERGY STORAGE↗

Time-resolved analysis of thickness-dependent dewetting and ablation of silver films upon nanosecond laser irradiation

Nanosecond pulsed laser dewetting and ablation of thin silver films is investigated by time-resolved imaging. Laser pulses of 532 nm wavelength and 5 ns temporal width are irradiated on silver films of different thicknesses (50 nm, 80 nm, and 350 nm). Below the ablation threshold, it is observed that the dewetting process does not conclude until 630 ns after the laser irradiation for all samples, forming droplet-like particles in the spot central region. At higher laser intensities, ablative material removal occurs in the spot center. Cylindrical rims are formed in the peripheral dewetting zone due to the solidification of transported matter at about 700 ns following the laser pulse exposure. In addition to these features, droplet fingers are superposed upon irradiation of 350-nm thick silver films with higher intensity.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Strong electroluminescence from direct band and defects in Ge n+/p shallow junctions at room temperature

Strong room temperature electroluminescence with two emission peaks at around 0.786 eV and 0.747 eV from Ge n+/p shallow junctions was reported. The peak at around 0.786 eV comes from direct band luminescence (DBL) in n + Ge regions, while the peak fixing at 0.747 eV is resulted from defects induced by ion implantation. Heavy n-type doping in Ge renders realization of strong defect-related luminescence (DRL) feasible. The peak intensity ratio of DRL/DBL decreases with increase of injection current since more electrons are filled in Γ valley. Above all, the Ge n+/p shallow junction is fully compatible with the source and drain in Ge metal-oxide-semiconductor field effect transistors.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High (1 1 1) orientation poly-Ge film fabricated by Al induced crystallization without the introduction of AlO{sub x} interlayer

High (1 1 1) orientation poly-Ge film was fabricated by Al induced crystallization (AIC), where Al and amorphous Ge (a-Ge) layers were continuously deposited by magnetron sputtering, avoiding the deliberate introduction of an AlO{sub x} interlayer. To improve the quality of poly-Ge film, the ratio of thicknesses of Al and a-Ge was adjusted. Electron backscattered diffraction (EBSD) results revealed that the (1 1 1) fraction of poly-Ge film reached 97% and the average crystal grain size surpassed 100 μm.

36 MATERIALS SCIENCE↗

Ohmic contact formation of metal/amorphous-Ge/n-Ge junctions with an anomalous modulation of Schottky barrier height

The modulation of Schottky barrier height of metal/Ge inserting an amorphous Ge layer has been demonstrated. It is interested that the Schottky barrier height of Al/amorphous-Ge/n-Ge junctions is oscillated with increase of the a-Ge thickness from 0 to 10 nm, and when the thickness reaches above 10 nm, the Al/amorphous-Ge/n-Ge shows ohmic characteristics. Electron hopping through localized states of a-Ge layer, the alleviation of metal induced gap states, as well as the termination of dangling bonds at the amorphous-Ge/n-Ge interface are proposed to explain the anomalous modulation of Schottky barrier height.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Formation of nickel germanide on SiO{sub 2}-capped n-Ge to lower its Schottky barrier height

In this Letter, NiGe/SiO{sub 2}/n-Ge ohmic contacts were demonstrated with Ge, rather than Ni, diffusion through the ion-implanted SiO{sub 2} films to form NiGe. The equivalent Schottky barrier height reduced from 0.58 eV for NiGe/n-Ge to ohmic contact. The anomalous diffusion behavior and accumulation of Ge in the SiO{sub 2} near the NiGe/SiO{sub 2} interface can be explained by vacancy-enhanced Ge diffusion. It is proposed that the presence of vacancies and Ge atoms embedded in the SiO{sub 2} layer play a significant role in the current enhancement by generation of multiple levels in the SiO{sub 2} band gap.

36 MATERIALS SCIENCE↗