Microstructural Engineering and Accelerated Test Method Development to Achieve Low Cost, High Performance Solutions for Hydrogen Storage and Delivery

This project made advancements in developing lower cost steel alloys with novel microstructural design for use in hydrogen refueling infrastructure such as storage, compressors, and dispensing components, and utilizing accelerated test methods to efficiently evaluate variations in alloy and microstructure design. The project specifically sought to design alloys with lower nickel contents to reduce alloy cost, which was accomplished through substituting manganese for nickel along with other alloy additions to control deformation characteristics known to be important for hydrogen embrittlement resistance. Through Mn substitutions for nickel, austenitic and duplex austenite-ferrite steels were successfully developed with lower cost than currently available commercial stainless steel products that are employed for hydrogen refueling infrastructure. The steels were processed to achieve comparable strength and toughness in hydrogen environments as the commercially available steels containing high Ni contents. To evaluate mechanical performance in hydrogen, a testing methodology was employed to compare ubiquitous laboratory testing using electrochemical hydrogen charging in a liquid electrolyte to less accessible high pressure gaseous testing. While the application of these steels is in high pressure gaseous environments, the electrochemical hydrogen charging tests produced comparable results. Additionally, the Los Alamos Neutron Scatting Center enabled characterization of deformation mechanisms of the steel alloys in the presence of hydrogen, which has been associated with steel alloy characteristics associated with hydrogen embrittlement. Finally, a fracture mechanics based test bed model was developed to predict the influence of hydrogen gas pressure and fatigue conditions on fatigue lifetimes of pressure vessel steels. Together, these developments can be employed to enable lower cost hydrogen fueling infrastructure and more reliable prediction of steel alloy components in hydrogen service conditions. In particular, the newly alloys have the potential to replace stainless steels, having demonstrated comparable performance at substantially reduced cost.

08 HYDROGEN↗

Microstructural Engineering of Mn-Alloyed Austenitic Steel for Hydrogen Storage and Delivery

Austenitic stainless steels are commonly used for hydrogen storage and transportation. These alloys have a high nickel (Ni) content, which increases alloy cost. In this study, high manganese (Mn) austenitic alloys were evaluated as potential lower cost alternatives. Two heats of high Mn alloys with different stacking fault energies (SFE) of ~29 mJ·m -2 and 49 mJ·m -2 were acquired. Additionally, a new vanadium (V)-microalloyed high Mn alloy was designed to achieve a SFE of 47 mJ·m -2 to minimize planar slip deformation mechanisms. Post-processing via cold working in conjunction with aging was also performed on the V-microalloyed high Mn steel. Hydrogen embrittlement sensitivity was investigated using circumferential notch tensile specimens cathodically charged with hydrogen in a 0.05M NaOH electrolytic solution. The alloys were compared to a cold-worked 316L stainless steel, which exhibited no strength loss due to hydrogen. The high Mn alloys with SFE of ~29 mJ·m 2 and 49 mJ·m -2 had notch strength losses of 11 and 6 pct, respectively. The V-microalloyed high Mn steel in the as-hot-rolled condition had a notch strength loss of 17 pct. Furthermore, the V-microalloyed high Mn steel in the cold worked and aged condition indicated no notch strength loss in hydrogen, which was comparable to the performance of the 316L stainless steel.

36 MATERIALS SCIENCE↗

Hydrogen Embrittlement of Medium Mn Steels

Recent research efforts to develop advanced–/ultrahigh–strength medium-Mn steels have led to the development of a variety of alloying concepts, thermo-mechanical processing routes, and microstructural variants for these steel grades. However, certain grades of advanced–/ultrahigh–strength steels (A/UHSS) are known to be highly susceptible to hydrogen embrittlement, due to their high strength levels. Hydrogen embrittlement characteristics of medium–Mn steels are less understood compared to other classes of A/UHSS, such as high Mn twinning–induced plasticity steel, because of the relatively short history of the development of this steel class and the complex nature of multiphase, fine-grained microstructures that are present in medium–Mn steels. The motivation of this paper is to review the current understanding of the hydrogen embrittlement characteristics of medium or intermediate Mn (4 to 15 wt pct) multiphase steels and to address various alloying and processing strategies that are available to enhance the hydrogen-resistance of these steel grades.