Separation and/or sequestration apparatus and methods

Apparatus for separating CO.sub.2 from an electrolyte solution are provided. Example apparatus can include: a vessel defining an interior volume and configured to house an electrolyte solution; an input conduit in fluid communication with the interior volume; an output conduit in fluid communication with the interior volume; an exhaust conduit in fluid communication with the interior volume; and an anode located within the interior volume. Other example apparatus can include: an elongated vessel having two regions; an input conduit extending outwardly from the one region; an output conduit extending outwardly from the other region; an exhaust conduit in fluid communication with the one region; and an anode located within the one region. Methods for separating CO.sub.2 from an electrolyte solution are provided. Example methods can include: providing a CO.sub.2 rich electrolyte solution to a vessel containing an anode; and distributing hydrogen from the anode to acidify the electrolyte solution.

54 ENVIRONMENTAL SCIENCES↗

High Power Planar Sodium-Nickel Chloride Battery

Widespread penetration of renewable energy and increasing demands on reliability/security of the electrical grid require extensive advances in energy storage technologies. One most promising technology is the sodium-beta batteries (NBBs) based on a sodium-ion conducting β''-Al2O3 solid electrolyte (BASE) and operated at elevated temperatures (300-350oC). Current NBBs, constructed on a 1-3 mm thick tubular electrolyte, have high capital cost, performance/safety issues and relatively high operating temperature that limit market penetration of the technology. In this work we report a new generation NBB that utilizes a planar design, incorporating a thinner BASE that reduces the area of specific resistance and may be operated at reduced temperatures. The lower operating temperatures allows for use of more cost-effective cell materials and decreases adverse temperature effects that impact cycle life and overall cost. We here present recent progress generated from planar NBB button cells, including initial cell performance, cathode design and chemistry.

25 ENERGY STORAGE↗

Calcium- and Cobalt-doped Yttrium Chromites as an Interconnect Material for Solid Oxide Fuel Cells

The structural, thermal and electrical characteristics of calcium- and cobalt-doped yttrium chromites were studied for a potential use as the interconnect material in high temperature solid oxide fuel cells (SOFCs) as well as other high temperature electrochemical and thermoelectric devices. The Y0.8Ca0.2Cr1-xCoxO3±δ (x=0, 0.1, 0.2, 0.3) compositions had single phase orthorhombic perovskite structures in the wide range of oxygen pressures. Sintering behavior was remarkably enhanced upon cobalt doping and densities 95% and 97% of theoretical density were obtained after sintering at 1300oC in air, when x was 0.2 and 0.3, respectively. The electrical conductivity in both oxidizing and reducing atmospheres was significantly improved with cobalt content, and values of 49 and 10 S/cm at 850oC and 55 and 14 S/cm at 950oC in air and forming gas, respectively, were reported for x=0.2. The conductivity increase was attributed to the charge carrier density increase upon cobalt substitution for chromium confirmed with Seebeck measurements. The thermal expansion coefficient (TEC) was increased with cobalt content and closely matched to that of an 8 mol% yttria-stabilized zirconia (YSZ) electrolyte for 0.1 ≤ x ≤ 0.2. The chemical compatibility between Y0.8Ca0.2Cr1-xCoxO3±δ and YSZ was evaluated firing the two at 1400oC and no reaction products were found if x value was kept lower than 0.2.

30 DIRECT ENERGY CONVERSION↗

Degradation Mechanisms of SOFC Anodes in Coal Gas Containing Phosphorus

The interaction of phosphorus in synthetic coal gas with the nickel-based anode of solid oxide fuel cells has been investigated. Tests with both anode-supported and electrolyte-supported button cells were performed at 700 to 800oC in synthetic coal gas containing 0.5 to 10 ppm phosphorus, introduced as phosphine. Two primary modes of degradation were observed. The most obvious was the formation of a series of bulk nickel phosphide phases, of which Ni3P, Ni5P2, Ni12P5 and Ni2P were identified. Phosphorus was essentially completely captured by the anode, forming a sharp boundary between converted and unconverted anode portions. These products partially coalesced into large grains, which eventually affected electronic percolation through the anode support. Thermodynamic calculations predict that formation of the first binary nickel phosphide phase is possible at sub-parts per billion concentrations in coal gas at temperatures relevant to fuel cell operation. A second mode of degradation is attributed to surface diffusion of phosphorus to the active anode/electrolyte interface to form an adsorption layer. Direct evidence for the presence of such an adsorption layer on nickel was obtained by surface spectroscopies on fracture surfaces. Further, cell performance losses were observed well before the entire anode was converted to bulk nickel phosphide. Impedance spectroscopy revealed that these losses were primarily due to growth in electrodic resistance, whereas large ohmic increases were visible when the entire anode was converted to nickel phosphide phases. The rate of resistance growth for anode-supported cells showed a very low dependence on phosphorus concentration, attributed to phosphorus activity control within the anode by bulk nickel phosphide products.

01 COAL, LIGNITE, AND PEAT↗

Ni/YSZ Anode Interactions with Impurities in Coal Gas

Performance of solid oxide fuel cell (SOFC) with nickel/zirconia anodes on synthetic coal gas in the presence of low levels of phosphorus, arsenic, selenium, sulfur, hydrogen chloride, and antimony impurities were evaluated. The presence of phosphorus and arsenic led to the slow and irreversible SOFC degradation due to the formation of secondary phases with nickel, particularly close to the gas inlet. Phosphorus and antimony surface adsorption layers were identified as well. Hydrogen chloride and sulfur interactions with the nickel were limited to the surface adsorption only, whereas selenium exposure also led to the formation of nickel selenide for highly polarized cells.

01 COAL, LIGNITE, AND PEAT↗

Performance of Lanthanum Strontium Manganite Electrodes at High Pressure

The high-pressure performance of lanthanum strontium manganite (LSM), LSM-zirconia, and LSM/ceria composite electrodes was studied by impedance spectroscopy and dc methods. Electrode resistances decreased in proportion to P(O2)1/2 for the LSM electrode in both cathodic and anodic directions to at least 100 atm, a decrease that was attributed to dissociative oxygen adsorption, surface diffusion, and related phenomena. For the LSM-20/zirconia composite electrode, resistances decreased in proportion to P(O2)1/4 across the entire pressure range considered. Two principal features appeared in the impedance spectra, one that showed a P(O2)1/4 dependence attributed to charge transfer reactions, and one that was nearly pressure-independent, possibly due to transport in the zirconia portion of the composite. For the LSM-20/ceria composite electrode, resistances decreased as P(O2)0.3-0.4 at high pressure, depending on temperature. Two features appeared in the impedance spectra: one at low to intermediate frequency having a P(O2)1/2 dependence and one at high frequency having a P(O2)1/4 dependence. These features are attributed to dissociative oxygen adsorption and to charge transfer reactions, respectively. Results suggest that cathodic losses can be substantially lowered by operation of solid oxide fuel cells at greater than ambient pressure.

lanthanum manganite, LSM, cathode, oxygen electrod↗

Interactions of nickel/zirconia solid oxide fuel cell anodes with coal gas containing arsenic

The performance of anode-supported and electrolyte-supported solid oxide fuel cells was investigated in synthetic coal gas containing 0 to 10 ppm arsenic introduced as arsine. Arsenic was found to interact strongly with nickel in the anode, resulting in the formation of nickel-arsenic solid solution, Ni5As2 and Ni11As8, depending on temperature, arsenic concentration, and reaction time. For anode-supported cells, loss of electrical connectivity in the anode support was the principal mode of degradation, as nickel was converted to nickel arsenide phases that migrated to the surface to form large grains. Cell failure occurred well before the entire anode was converted to nickel arsenide, and followed a reciprocal square root of arsenic partial pressure dependence consistent with a diffusion-based rate-limiting step. Failure occurred more quickly with electrolyte-supported cells, which have a substantially smaller nickel inventory. For these cells, time to failure varied linearly with the reciprocal arsenic concentration in coal gas, and occurred when arsenic reached the anode/electrolyte interface. Test performed with nickel/zirconia coupons showed that arsenic was essentially completely captured in a narrow band near the fuel gas inlet.

Environmental Molecular Sciences Laboratory↗

Anode Interactions with Coal Gas Contaminants

This report describes efforts to characterize the interactions nickel anodes with phosphorus in coal gas using three different button cell configurations to emphasize particular degradation modes. Important parameters addressed included contaminant concentration, temperature, reaction time, fuel utilization, and current density. In addition, coupon tests in flow-through and flow-by arrangements were conducted to complement cell tests. The studies have involved extensive electrochemical testing using both dc and ac methods. Post-test analyses to determine the composition and extent of nickel modification are particularly important to understanding reactions that have occurred. This report also provides a thermodynamic assessment of contaminant reactions with nickel in a coal gas environment with regard to alteration phase formation. Contaminants addressed were phosphorus, arsenic, sulfur, selenium, and antimony. Phosphorus was found to interact strongly with nickel and result in extensive alteration phase formation, consistent with expectations based on thermodynamic properties. Even in button cell tests where the fuel utilization was low, phosphorus was found to be nearly completely captured by the nickel anode. For anode-supported cells, an important degradation mode involved loss of electronic percolation, the result of nickel phosphide formation, grain growth, and inducement of micro-fractures within the anode support. Even with excessive anode support conversion, electrochemical degradation rates were often very low. This is attributed to a “shadowing effect,” whereby a dense structure such as current leads prevent phosphorus from reacting with the nickel directly underneath. This effect maintains an electrical pathway to the active interface, and allows the cell to operate with minimal degradation until the anode is essentially completely consumed. In a planar stack, ribs on the interconnect plate would be expected to provide this conductive pathway in the event of phosphorus exposure. When phosphorus interactions proceeded to the active interface, most easily observed in tests with electrolyte-supported cells having a thin anode, the electrochemical performance decreased considerably.