Search NASA⌕ Search

Engineering topics

Colclasure, Andrew M.

Publications and source records attributed to Colclasure, Andrew M..

At least 37 records · Page 2

Laser ablation for structuring Li-ion electrodes for fast charging and its impact on material properties, rate capability, Li plating, and wetting

Laser ablation is a scalable technique for decreasing the effective tortuosity of electrodes by selectively removing material with high precision. Applied to ≈ 110 um thick electrode coatings, this work focuses on understanding the impact of laser ablation on electrode material properties at the beginning of life and synergistic impacts of ablated channels on cell performance throughout their cycle life. Post laser ablation, local changes in chemistry, crystallography, and morphology of the laser-impacted electrode regions are investigated. It is shown that femtosecond pulsed laser ablation can achieve high-rate material removal with minor material damage locally at the interface of the impacted zones. The capacity achieved during a 6C (10 min) constant-current constant-voltage charge to 4.2 V improved from 1 mAh cm -2 for the non-ablated electrodes to almost 2 mAh cm -2 for the ablated electrodes. This benefit is attributed to a synergistic effect of enhanced wetting and decreased electrode tortuosity. The benefit was maintained for over 120 cycles, and upon disassembly decreased Li-plating on the graphite anode was observed. Finally, multi-physics modeling in conjunction with wetting analyses showed that laser ablating either one of the electrodes led to substantial improvements in wetting and rate capability, indicating that substantial performance benefits can be achieved by ablating only the graphite anode as apposed to both electrodes.

25 ENERGY STORAGE↗

A Comprehensive Understanding of the Aging Effects of Extreme Fast Charging on High Ni NMC Cathode

As the battery industry shifts toward high Ni content cathodes, such as LiNi 0.8 Mn 0.1 Co 0.1 O 2 [NMC811], a complete understanding of the degradation mechanisms of NMC811 under extreme fast charging (XFC) (XFC, ≤10–15 min charging) conditions is needed. Such comprehensive understanding would identify the most critical materials gaps that need to be addressed for enabling XFC long-life cells for electric vehicles. This study maps out the key aging mechanisms for NMC811 cycled at different XFC conditions (between 1C and 9C) for up to 1000 cycles. To acquire a fundamental understanding of utilization and degradation, cells are evaluated using a range of electrochemical techniques, and multimodal and multiscale microscopy techniques to quantify chemical, structural, and crystallographic degradation as a function of cycling conditions for the NMC cathode. When comparing NMC811 to NMC532, it is observed that NMC811 has a greater subsurface crystallographic degradation and displays a similar magnitude of subparticle cracking. However, the NMC811 maintains superior performance despite those advanced degradations. Here, the superior cycle life performance is attributed to the NMC811 particles having radially oriented grains and improved transport properties. NMC811 shows between 4.6× and 3.15× reduction in capacity fade than NMC532 for charging rates between 4C (e.g., 15-min charging) and 6C (10-min charging).

25 ENERGY STORAGE↗

Quantification of Dead Lithium on Graphite Anode under Fast Charging Conditions

A series of computational and experimental studies were conducted to understand the onset of lithium plating and subsequent quantification of dead lithium on graphite electrodes in the design of fast charging batteries. The experiments include titration and relaxation studies for detecting initiation of lithium metal plating for various SOC and C-rates, which are compared against the thermodynamically consistent phase field computational results. The collaborative study on "model graphite electrode" with 2.18 mAh cm-2 nominal capacity at 25 degrees C demonstrates: (1) the macroscopic voltage response during relaxation studies indicate the reintercalation of plated lithium into the graphite anode; (2) for SOC below 60% and low C-Rates, there is no dead lithium; (3) for SOC between 60% to 80%, and C-Rates in the range of 4C-6C show dead lithium both in experiments and simulations; (4) at 100% SOC and 4C-6C rates, large amounts of dead lithium are observed. The study presented here allows us to evaluate the effects of the physical properties of the electrochemical system on plating and stripping kinetics and the amount of dead lithium on graphite electrodes, which determines the cell capacity loss under fast charge.

batteries↗

Developing extreme fast charge battery protocols – A review spanning materials to systems

Extreme fast charging (XFC) has become a focal research point in the lithium-battery community over the last several years. As adoption of electric vehicles increases, fast charging has become a key driver in enhancing consumer recharge experience. Recently, the research community has made significant improvements in developing charge protocols to support XFC. New charge protocol designs derived using a combination of advanced, physically derived models, and electrochemical and secondary characterization methods, increase charge acceptance and decrease aging. By coordinating these methods and modifying protocols to account for different material constraints, including lithium plating and cathode particle degradation, novel charge protocols have increased the energy accepted during charging by over 25% in 10 min and increased the charge acceptance prior to a constant-voltage step by approximately 3x. Here, we review several charge-protocol advances, aging factors which are enhanced by XFC and advances which will enable adoption of XFC capable vehicles. These advances include implementing machine learning and other detection algorithms to reduce and classify lithium plating, which is known to significantly degrade cell performance and reduce cell life. The review concludes by discussing full-system fast charge requirements, including electric vehicle service equipment needs for implementing XFC protocols.

25 ENERGY STORAGE↗

Impact of Electrode Thickness and Temperature on the Rate Capability of Li 4 Ti 5 O 12 /LiMn 2 O 4 Cells

Growing demand for stationary energy storage systems requires the development of low cost, long cycle life, safe batteries. Lithium-ion batteries (LiBs) utilizing Li 4 Ti 5 O 12 /LiMn 2 O 4 (LMO) cathode are promising candidates providing critical-material-free chemistry, high power capability, and long lifespan. However, their low energy density is a major drawback. In this work, we evaluate the rate performance of LTO/LMO cells fabricated with electrode loadings from 1.7 to 4.2 mAh cm -2 toward the development of high energy density and low cost LTO/LMO cells. The operating temperature is varied from 30 °C to 55 °C to evaluate the impact of electrode thickness vs temperature limitations on the electrode utilization. In addition, Newman modeling is performed to provide detailed understandings of the cell performance. Combining experimental and simulated results, we show the rate capability of the thicker electrodes is limited by the electrolyte transport. When the cells are discharged by applying pulsed current, Li + ion depletion is mitigated and the discharge capacity increases. Thus, high energy density LTO/LMO cells for BTMS applications can operate more efficiently when intermittent rest is applied. Finally, overcoming electrolyte transport limitations will be the key to enabling the development of high energy density LTO/LMO cells using thick electrodes.

25 ENERGY STORAGE↗

Lithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes

This paper develops a physically justified reduced-order capacity fade model from accelerated calendar- and cycle-aging data for 32 lithium-ion (Li-ion) graphite/nickel-manganese-cobalt (NMC) cells. The large data set reveals temperature-, charge C-rate-, depth-of-discharge-, and state of charge (SOC)-dependent degradation patterns that would be unobserved in a smaller test matrix. Model structure is informed by incremental capacity analysis that shows loss of lithium inventory and cathode-material loss as the dominant capacity fade mechanisms. The model includes terms attributable to solid-electrolyte interface (SEI) growth, electrode cracking, cycling-driven acceleration of SEI growth, and "break-in" mechanisms that slightly decrease or increase available Li inventory early in life. The study explores what mathematical couplings of these mechanisms best describe calendar aging, cycle aging, and mixed calendar/cycle aging. Various approaches are discussed for extracting relevant stress factors from complex cycling profiles to predict lifetime during real-world battery loads using models trained on constant-current laboratory test results. The complexity of the present human-driven model identification process motivates future work in machine learning to more widely search and statistically discern the optimal model that correctly extrapolates capacity fade based on physical knowledge.

25 ENERGY STORAGE↗

Evaluating temperature dependent degradation mechanisms of silicon-graphite electrodes and the effect of fluoroethylene carbonate electrolyte additive

Understanding and overcoming the relatively high rate of degradation observed with silicon (Si)-based anodes in lithium (Li)-ion batteries (LiBs) is crucial for developing cells with increased energy density. The capacity fade of Si-graphite (Gr) electrodes in electrolytes with and without 10 wt% fluoroethylene carbonate (FEC) is explored during cycling at temperatures of 25, 45, and 70 °C, focusing on the complex degradation modes arising from loss of active material, loss of Li inventory, and cell resistance growth. We first show the common half-cell testing cannot be used at elevated temperatures as the performance of Li metal overshadows the behavior of Si-Gr electrode. Symmetric cell configuration successfully eliminates the effect of foreign materials, and reveals that while the presence of FEC provides better passivation of Si, it also results in greater parasitic reactions at 70 °C and faster capacity fade. The electrolyte without FEC, on the other hand, shows higher capacity retention at 70 °C. Finally, we propose a multi-step test protocol which can successfully deconvolute the information on loss of Li inventory and of active material. By combining half-cell and symmetric cell test methods, we demonstrate that loss of active material is reduced at higher temperatures and the dominant mechanisms of capacity loss for Si-Gr electrodes at elevated temperatures is loss of Li inventory.

25 ENERGY STORAGE↗

Methodologies for Design, Characterization and Testing of Electrolytes that Enable Extreme Fast Charging of Lithium-ion Cells

Selection, testing and validation of electrolyte candidates for Li-ion cells are discussed, based on a 10-minute target for extreme fast charge (XFC). A combination of modeling and laboratory measurements create a timely and synergistic approach to identifying candidate electrolyte formulations. Multi-solvent systems provide a balanced set of properties, wherein lower molecular-weight solvents offer reduced viscosity, increased species diffusivity, and mitigation of concentration polarization at high charge rates. Carefully selected formulations can exhibit peak conductivity and usable conductivity range of two to three times that of the baseline EC-EMC (3:7, wt.) + LiPF 6 . Candidates are also chosen based on stability and longevity within the cell environment. Lab testing coincides with property predictions from the Advanced Electrolyte Model (AEM) and a macro-scale cell model. Furthermore, cell testing utilized coin and pouch cells having NMC532 or NMC811 cathodes with graphite electrodes. Results indicate combinations of low-molecular weight solvents are key for fast-charge electrolytes as they extend the useful conductivity range to both low and higher salt concentrations, and possess higher self-diffusivities compared to conventional solvents. This reduces impacts from concentration polarization. The choice of electrolyte also influences the tendency for lithium metal deposition at the anode, as showcased by experimental and modeling results herein.

25 ENERGY STORAGE↗

Comprehensive Insights into Nucleation, Autocatalytic Growth, and Stripping Efficiency for Lithium Plating in Full Cells

Synchrotron high-energy X-ray diffraction is used to enable nondestructive detection and quantification of heterogeneous lithium plating in working batteries. In this study a LiNi 0.5 Mn 0.3 Co 0.2 O 2 /graphite pouch cell was operated under 6C fast-charge rate for greater than 1200 cycles. The magnitude and spatial distribution of lithium plating, lithium stripping, and the effect of metallic lithium deposition on lithium intercalation into graphite were quantified. Fully intercalated graphite (LiC 6 ) was detected after discharge with a lateral distribution closely correlated with lithium plating, which can be used as a higher-sensitivity indicator for lithium plating. Over an extended cycle life, the overall metallic lithium concentration followed a sigmoidal curve indicating two-stage continuous nucleation and autocatalytic growth. The lithium stripping efficiency underwent an exponential decay as a function of cycle life as the buildup of metallic lithium hindered the efficient dissolution back into the electrolyte. The findings provide direct insights into the characteristics of lithium plating and stripping under realistic fast-charge conditions.

25 ENERGY STORAGE↗

Calendar aging of silicon-containing batteries

High-energy batteries for automotive applications require cells to endure well over a decade of constant use, making their long-term stability paramount. This is particularly challenging for emerging cell chemistries containing silicon, for which extended testing information is scarce. While much of the research on silicon anodes has focused on mitigating the consequences of volume changes during cycling, comparatively little is known about the time-dependent degradation of silicon-containing batteries. Here we discuss a series of studies on the reactivity of silicon that, collectively, paint a picture of how the chemistry of silicon exacerbates the calendar aging of lithium-ion cells. Assessing and mitigating this shortcoming should be the focus of future research to fully realize the advantages of this battery technology.

25 ENERGY STORAGE↗

Fast-Charging Aging Considerations: Incorporation and Alignment of Cell Design and Material Degradation Pathways

Fast charging of batteries for electric vehicles is seen as one of the most direct ways to enhance adoption. Currently, fast charging is limited by increased cell aging, which is primarily driven by Li plating and degradation of cathode materials. Here, using combined sets of experimental and computational analysis and a suite of different charge protocols, we begin to examine the interplay between failure mode, cell designs, and ultimately aging mechanisms. Slight variation in cell design and the subsequent impacts that charge protocols have on aging can create distinct cell-to-cell variation. As little as 2% difference in porosity change at the cell negative electrode during cycling due to early Li metal plating has been found to alter the aging pathway and either accelerate or inhibit the loss due to Li plating.

25 ENERGY STORAGE↗

Quantifying the Influence of Charge Rate and Cathode-Particle Architectures on Degradation of Li-Ion Cells Through 3D Continuum-Level Damage Models

In this article, we develop a 3D, continuum-level damage model implemented on statistically generated LiNi 0.5 Mn 0.3 Co 0.2 O (NMC 532) secondary cathode particles. The primary motivation of the particle-level model is to inform cathode-particle design through detailed exploration of the influence of secondary and primary particle sizes on the damage predicted during operation, and determine charging profiles that reduce cathode fracture. The model considers NMC 532 secondary particles containing an agglomeration of anisotropic, randomly oriented grains. These brittle, Ni-based cathodes are prone to mechanical degradation, which reduces overall battery cycle life. The model predicts that secondary-particle fracture is primarily due to non-ideal grain interactions and high-rate charge demands. The model predicts that small secondary-particles with large grains develop significantly less damage than larger secondary particles with small grains. The model predicts most of the chemo-mechanical damage accumulates in the first few cycles. The chemo-mechanical model predicts monotonically increasing capacity fade with cycling and rate. Comparing to experimental results, the model is well suited for capturing initial capacity fade mechanisms, but additional physics is required to capture long-term capacity fade effects.

25 ENERGY STORAGE↗

Revealing causes of macroscale heterogeneity in lithium ion pouch cells via synchrotron X-ray diffraction

Heterogeneous battery performance is a critical issue for maximization of cell lifetime capacity and safety. Using high energy synchrotron X-ray diffraction, the influence of charge rate, voltage limit, uneven stack pressure, and gas generation on the lithium transport properties was quantified in single-layer graphite/LiNi 0.5 Mn 0.3 Co 0.2 O 2 pouch cells. A freshly formatted cell tracked in operando during initial fast charge cycles indicated variable position-dependent performances, while lateral mapping showed a significant fast charge (6C) heterogeneity compared to slow charge (C/2). Pressure effects were non-dominant compared to charge rate. Maps of previously aged and rested cells indicate that lateral heterogeneity slowly equilibrates at rest, but regenerates upon further cycling at fast charge rate. Furthermore, an unformatted cell was mapped at charge and discharge during its first formation cycle to analyze the effect of byproduct gases on the heterogeneous lithium transport. Gas was observed as randomly interspersed “bubbles” which locally hindered lithium intercalation and caused significant heterogeneity. Electrode architectures and charging protocols that promote homogeneous intercalation are critical for predictable high-performance and long-life batteries.

25 ENERGY STORAGE↗

Extended cycle life implications of fast charging for lithium-ion battery cathode

Enabling extreme fast charging (XFC, =10–15 min charging) requires a comprehensive understanding of its implications. While lithium plating is a key bottleneck for the anode, the full extent of limitations for the cathode are not well-understood, particularly in extended-cycle settings with well-defined battery designs and conditions. This article presents cycle-life implications of XFC on cathodes at multiple length scales, combining electrochemical analyses, degradation modeling, and post-test characterizations. The comprehensive test matrix includes 41 well-defined gr/NMC pouch cells under varied fast-charge rates (1–9C) and state-of-charges cycled up to 1000 times. Cathode issues remain minimal in early cycling, but begin to accelerate in later life, when distinct cracking is found and identified as a fatigue mechanism. The bulk structure of cathodes remains intact, but distinct particle surface reconstruction is observed; however, this shows less pronounced effect on cathode aging than does cracking.

25 ENERGY STORAGE↗

Long-term cyclability of Li 4 Ti 5 O 12 /LiMn 2 O 4 cells using carbonate-based electrolytes for behind-the-meter storage applications

Li 4 Ti 5 O 12 /LiMn 2 O 4 (LTO/LMO) chemistry was evaluated as a potential candidate for behind-the-meter storage (BTMS) applications. Its long-term cycle performance at 45 °C was tested using ethylene carbonate (EC) and propylene carbonate (PC) solvent electrolytes. Over 1000 cycles, LTO/LMO cells exhibited ~80% capacity retention and Coulombic efficiency higher than 99.96%. Electrochemical test results showed the major degradation mode of LTO/LMO cells arises from continuous electrolyte decomposition at the LTO anode and loss of Li inventory. EC and PC electrolytes created distinct surface layers, where the EC reduction products were more effective in passivating the LTO electrode surface. Dissolution and migration of Mn from the cathode was probed as Mn 2+ species distributed throughout the surface layer at the anode. By utilizing a prelithiated LTO electrode, the LTO/LMO cell performance was significantly enhanced with EC electrolyte. On the other hand, PC electrolyte resulted in accelerated electrolyte decomposition at the lithiated LTO surface due to the lack of surface passivation. Thus, mitigating parasitic reactions at the LTO electrode is the key to developing successful LTO/LMO cells.

25 ENERGY STORAGE↗

A Review of Existing and Emerging Methods for Lithium Detection and Characterization in Li-Ion and Li-Metal Batteries

Whether attempting to eliminate parasitic Li metal plating on graphite (and other Li-ion anodes) or enabling stable, uniform Li metal formation in ‘anode-free’ Li battery configurations, the detection and characterization (morphology, microstructure, chemistry) of Li that cannot be reversibly cycled is essential to understand the behavior and degradation of rechargeable batteries. In this review, various approaches used to detect and characterize the formation of Li in batteries are discussed. Each technique has its unique set of advantages and limitations, and works towards solving only part of the full puzzle of battery degradation. Going forward, multimodal characterization holds the most promise towards addressing two pressing concerns in the implementation of the next generation of batteries in the transportation sector (viz. reducing recharging times and increasing the available capacity per recharge without sacrificing cycle life). Such characterizations involve combining several techniques (experimental- and/or modeling-based) in order to exploit their respective advantages and allow a more comprehensive view of cell degradation and the role of Li metal formation in it. Additionally, it is also discussed which individual techniques, or combinations thereof, can be implemented in real-world battery management systems on-board electric vehicles for early detection of potential battery degradation that would lead to failure.

25 ENERGY STORAGE↗

How Fast Can a Li-Ion Battery Be Charged? Determination of Limiting Fast Charging Conditions

Fast-charge protocols that prevent lithium plating are needed to extend the life span of lithium-ion batteries. Here, we describe a simple experimental method to estimate the minimum charging time below which it is simply impossible to avoid plating at a given temperature. We demonstrate that, by gauging and correcting the ohmic drop that is intrinsic to reference electrodes, the local potential at the anode surface can be reasonably approximated. This finer anode control enables the determination of the maximum average rate at which lithium deposition can be mitigated, establishing realistic boundaries that can inform the development of advanced charging protocols.

25 ENERGY STORAGE↗

Significant life extension of lithium-ion batteries using compact metallic lithium reservoir with passive control

Both traditional graphite-based lithium-ion batteries and next generation silicon-based chemistries suffer significant capacity fade from loss of cyclable lithium due to continued solid-electrolyte interphase growth. A possible engineering solution to maintaining the capacity of cells is incorporating a metallic lithium reservoir and discharging the reservoir into a working electrode to make up for lost cyclable lithium. Here, metallic lithium reservoirs are inserted into both pouch- and cylindrical-format cells. Significant capacity recovery and lifetime extension are demonstrated for traditional graphite and Si/graphite-based cells. In this work, a combination of post-mortem characterization and modeling provide insight into how the lithium distribution as a function of position from reservoir vary with recovery rate. The potential of using passive control to potentially eliminate the need for extra wiring for the third electrode is explored using a simple resistor.

25 ENERGY STORAGE↗