Contribution from Ising domains overlapping out-of-plane to perpendicular magnetic anisotropy in Mn 4 N thin films on MgO(001)

Single phase ε-Mn4N thin and ultrathin films are grown on MgO(001) using molecular beam epitaxy. Reflection high-energy electron diffraction and outof-plane x-ray diffraction measurements are taken for each sample in order to determine the in- and out-of-plane strain for each sample. Vibrating sample magnetometry and superconducting quantum interference device measurements, which are performed on the thin and ultrathin films respectively, are used to plot the magnetization of each sample versus both in- and out-of-plane $\vec H$-fields and to determine the magnitude of perpendicular magnetic anisotropy in these films. Three significant components of perpendicular magnetic anisotropy are observed in these films and are attributed to sample strain (1 component) and shape (2 components). Among these components, the most significant component (0.8 to 4.9 $\frac{Merg}{cm^3}$) is identified as a second term of shape anisotropy, which possesses a negative linear relationship with sample thickness over the range from 9 nm to 310 nm. Atomic (magnetic) force microscopy measurements show the presence of a surface localized magnetic polarization (22% to 82%), which increases with decreasing thickness, when the net magnetization of the films is zero. The second term of shape anisotropy as well as the surface localized polarization, which each depend on sample thickness, are each regarded as a consequence of Ising domains overlapping out-of-plane in these films.

Materials Science↗

Structural and magnetic properties of ferrimagnetic ε-phase Mn 4 N and antiferromagnetic ζ-phase Mn10N thin films on MgO(001)

Single phase ε-Mn 4 N and ζ-Mn 10 N thin films are grown on MgO(001) using molecular beam epitaxy. The films are identified and characterized using reflection high-energy electron diffraction, x-ray diffraction, back scattered electron scanning electron microscopy, atomic/magnetic force microscopy and Rutherford backscattering spectrometry. These films are found to be highly smooth with root-mean-squared roughnesses 3.39 nm and below. The quality of ε-Mn 4 N grown is strongly dependent on substrate temperature during growth. Epitaxial growth of substantial grains composed of the antiferromagnetic η-phase Mn 3 N 2 side by side with ferrimagnetic ε-phase grains is observed when growth temperature is below 480 °C. Ising domains isolated within areas roughly 0.5 μm across are observed in the ferrimagnetic ε-phase grains of samples consisting of a mix of η- and ε-phase grains. Magnetic domains following semi-continuous paths, which are 0.7–7.2 μm across, are observed in single phase ε-Mn4N. Measurements of the ζ-phase detail the structure and magnetism of the material as high Mn content γ-type ζ-phase with a regular surface corrugation along the [100]-direction and antiferromagnetic.