Search NASA⌕ Search

Engineering topics

Cordova, Elsa A

Publications and source records attributed to Cordova, Elsa A.

Tc-99 Adsorption on Selected Activated Carbons - Batch Testing Results

CH2M HILL Plateau Remediation Company (CHPRC) is currently developing a 200-West Area groundwater pump-and-treat system as the remedial action selected under the Comprehensive Environmental Response, Compensation, and Liability Act Record of Decision for Operable Unit (OU) 200-ZP-1. This report documents the results of treatability tests Pacific Northwest National Laboratory researchers conducted to quantify the ability of selected activated carbon products (or carbons) to adsorb technetium-99 (Tc-99) from 200-West Area groundwater. The Tc-99 adsorption performance of seven activated carbons (J177601 Calgon Fitrasorb 400, J177606 Siemens AC1230AWC, J177609 Carbon Resources CR-1240-AW, J177611 General Carbon GC20X50, J177612 Norit GAC830, J177613 Norit GAC830, and J177617 Nucon LW1230) were evaluated using water from well 299-W19-36. Four of the best performing carbons (J177606 Siemens AC1230AWC, J177609 Carbon Resources CR-1240-AW, J177611 General Carbon GC20X50, and J177613 Norit GAC830) were selected for batch isotherm testing. The batch isotherm tests on four of the selected carbons indicated that under lower nitrate concentration conditions (382 mg/L), Kd values ranged from 6,000 to 20,000 mL/g. In comparison. Under higher nitrate (750 mg/L) conditions, there was a measureable decrease in Tc-99 adsorption with Kd values ranging from 3,000 to 7,000 mL/g. The adsorption data fit both the Langmuir and the Freundlich equations. Supplemental tests were conducted using the two carbons that demonstrated the highest adsorption capacity to resolve the issue of the best fit isotherm. These tests indicated that Langmuir isotherms provided the best fit for Tc-99 adsorption under low nitrate concentration conditions. At the design basis concentration of Tc 0.865 µg/L(14,700 pCi/L), the predicted Kd values from using Langmuir isotherm constants were 5,980 mL/g and 6,870 mL/g for for the two carbons. These Kd values did not meet the target Kd value of 9,000 mL/g. Tests conducted to ascertain the effects of changing pH showed that at pH values of 6.5 and 7.5, no significant differences existed in Tc-adsorption performance for three of the carbons, but the fourth carbon performed better at pH 7.5. When the pH was increased to 8.5, a slight decline in performance was observed for all carbons. Tests conducted to ascertain the temperature effect on Tc-99 adsorption indicated that at 21 ºC, 27 ºC, and 32 ºC there were no significant differences in Tc-99 adsorption for three of the carbons. The fourth carbon showed a noticeable decline in Tc-99 adsorption performance with increasing temperature. The presence of volatile organic compounds (VOCs) in the source water did not significantly affect Tc-99 adsorption on either of two carbons tested. Technetium-99 adsorption differed by less than 15% with or without VOCs present in the test water, indicating that Tc-99 adsorption would not be significantly affected if VOCs were removed from the water prior to contact with carbon.

54 ENVIRONMENTAL SCIENCES↗

Uranium Adsorption on Ion-Exchange Resins - Batch Testing

The uranium adsorption performance of five resins (Dowex 1, Dowex 21K 16-30 [fresh], Dowex 21K 16-30 [regenerated], Purofine PFA600/4740, and ResinTech SIR-1200) were tested using unspiked, nitrate-spiked, and nitrate-spiked/pH adjusted source water from well 299-W19-36. These batch tests were conducted in support of a resin selection process in which the best resin to use for uranium treatment in the 200-West Area groundwater pump-and-treat system will be identified. The results from these tests are as follows: • The data from the high-nitrate (1331 mg/L) tests indicated that Dowex 1, Dowex 21K 16-30 (fresh), Purofine PFA600/4740, and ResinTech SIR-1200 all adsorbed uranium similarly well with Kd values ranging from ~15,000 to 95,000 ml/g. All four resins would be considered suitable for use in the treatment system based on uranium adsorption characteristics. • Lowering the pH of the high nitrate test conditions from 8.2 to 7.5 did not significantly change the uranium adsorption isotherms for the four tested resins. The Kd values for these four resins under high nitrate (1338 mg/L), lower pH (7.5) ranged from ~15,000 to 80,000 ml/g. • Higher nitrate concentrations greatly reduced the uranium adsorption on all four resins. Tests conducted with unspiked (no amendments; nitrate at 337 mg/L and pH at 8.2) source water yielded Kd values for Dowex 1, Dowex 21K 16-30 (fresh), Purofine PFA600/4740, and ResinTech SIR-1200 resins ranging from ~800,000 to >3,000,000 ml/g. These values are about two orders of magnitude higher than the Kd values noted from tests conducted using amended source water. • Compared to the fresh resin, the regenerated Dowex 21K 16-30 resin exhibited significantly lower uranium-adsorption performance under all test conditions. The calculated Kd values for the regenerated resin were typically an order of magnitude lower than the values calculated for the fresh resin. • Additional testing using laboratory columns is recommended to better resolve differences between the adsorption abilities of the resins and to develop estimates of uranium loading on the resins. By determining the quantity of uranium that each resin can adsorb and the time required to reach various levels of loading, resin lifetime in the treatment system can be estimated.

36 MATERIALS SCIENCE↗

Experimental Determination of the Effect of the Ratio of B/Al on Glass Dissolution along the Nepheline (NaAlSiO 4 ) – Malinkoite (NaBSiO 4 ) Join

The dissolution kinetics of five glasses along the NaAlSiO 4 -NaBSiO 4 join were used to evaluate how the structural variations associated with boron-aluminum substitution affect the rate of dissolution. The composition of each glass varied inversely in mol% of Al 2 O 3 (5 to 25 mol%) and B 2 O 3 (20 to 0 mol%) with Na 2 O (25 mol%) and SiO 2 (50 mol%) making up the remaining amount, in every case Na/(Al+B) = 1.0. Single-pass flow-through experiments (SPFT) were conducted under dilute conditions as a function of solution pH (from 7.0 to 12.0) and temperature (from 23° to 90°C). Analysis by 27 Al and 29 Si MAS-NMR suggests Al (~98% [4] Al) and Si atoms (~100% [4] Si) occupy a tetrahedral coordination whereas, B atoms occupy both tetrahedral ([4]B) and trigonal ( [3] B) coordination. The distribution of [3]B fractionated between [3] B(ring) and [3] B(non-ring) moieties, with the [3] B(ring)/ [3] B(non-ring) ratio increases with the B/Al ratio. The MAS-NMR results also indicated an increase in the fraction of [4] B with an increase in the B/Al ratio. But despite the changes in the B/Al ratio and B coordination, the 29 Si spectra maintain a chemical shift between -88 to -84 ppm for each glass. Unlike the 29 Si spectra, the 27 Al resonances shift to more positive values with an increase in the B/Al ratio which suggests mixing between the [4] Al and [3] B sites, assuming avoidance between tetrahedral trivalent cations ( [4] Al-O- [4] B avoidance). Raman spectroscopy was use to augment the results collected from MAS-NMR and demonstrated that NeB4 (glass sample with the highest B content) was glass-glass phase separated (e.g., heterogeneous glass). Results from SPFT experiments suggest a forward rate of reaction and pH power law coefficients,η, that are independent of B/Al under these neutral to alkaline test conditions for all homogeneous glasses. The temperature dependence shows an order of magnitude increase in the dissolution rate with a 67°C increase in temperature and suggests dissolution is controlled by a surface-mediated reaction, evident by the activation energy, E a , being between 44±8 and 48±7 kJ/mol. Forward dissolution rates, based on Na and Si release, for homogeneous glasses are independent of the B/Al ratio, whereas dissolution rates based on Al and B release are not. Dissolution rates based on B release increase with an increase in the fraction of [3] B(ring). Finally in accord with previous studies, the data discussed in this manuscript suggest rupture of the Al-O and Si-O bond as the rate-limiting step controlling the dissolution of these glasses.

58 GEOSCIENCES↗

Dissolution Kinetics of Meta-Torbernite under Circum-neutral to Alkaline Conditions

Autunite group minerals have been identified in contaminated sediments as the long-term controlling phase of uranium. Meta-torbernite, has been identified in subsurface environments which were subjected to co-contaminant disposal practices from past nuclear weapons and fuel operations. Under these conditions the mobility of uranium in subsurface pore waters is limited by the rate of meta-torbernite dissolution; however, there are no known investigations which report the dissolution behavior of meta-torbernite. The purpose of this investigation was to conduct a series of single-pass flow-through (SPFT) tests to 1) quantify the effect of temperature (23 - 90oC) and pH (6 -10) on meta-torbernite dissolution, 2) compare the dissolution of meta-torbernite to other autunite-group minerals, and 3) evaluate the effect of aqueous phosphate on the dissolution kinetics of meta-torbernite. Results presented here illustrate meta-torbernite dissolution rates increase by ~100X over the pH interval of 6 to 10 (eta = 0.59 ± 0.07), irrespective of temperature. The power law coefficient for meta-torbernite, eta = 0.59 ± 0.07, is greater than that quantified for Ca-meta-autunite, eta = 0.42 ± 0.12. This suggests the stability of meta-torbernite is greater than that of meta-autunite, which is reflected in the predicted stability constants. The rate equation for the dissolution of meta-torbernite as a function of aqueous phosphate concentration is log rdissol (mol m-2 sec-1) = -4.7 x 10-13 + 4.1 x 10-10 [PO43-].

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

Cementitious Wasteforms for Immobilization of Low-Activity Radioactive Wastes

Solidification of low-activity wastes with cementitious materials is a widely accepted technique that contains and isolates waste from the hydrologic environment. The radionuclides I-129, Se-75, Tc-99, and U-238 are identified as long-term dose contributors. The anionic nature of these radionuclides in aqueous solutions allows them to readily leach into the subsurface environment. Any failure of concrete encasement may result in water intrusion and consequent mobilization of radionuclides from the waste packages via mass flow and/or diffusion into the surrounding subsurface environment. Assessing the long-term performance of waste grouts for encasement of radionuclides requires understanding the: (1) speciation and interaction of the radionuclides within the concrete wasteform, (2) diffusion of radionuclide species when contacted with vadose zone porewater or groundwater under environmentally relevant conditions, and (3) long-term durability and weathering of concrete waste forms. An improved understanding of the interactions of long-lived radionuclides in cementitious matrices will improve predictions of the long-term fate of these sequestered contaminants. An integrated laboratory investigation has been conducted including: (1) a multifaceted spectroscopic investigation to interrogate the speciation and interaction of radionuclides within concrete wasteforms, (2) solubility tests to quantify the stability of solid phases identified as radionuclide-controlling phases, (3) quantify the diffusion of radionuclides from concrete wasteforms into surrounding subsurface sediment under realistic moisture contents (4%, 7%, and 15% by weight moisture content), (4) quantify the long-term durability of concrete waste forms as a function environmental parameters relevant to depository conditions, and (5) identify the formation of secondary phases or processes (microcracking) that influence radionuclide retention. Data obtained from this investigation provides valuable information for understanding the speciation, behavior, and fate of radionuclides immobilized within concrete wasteforms under vadose zone conditions and underscores the necessity for robust, multi-disciplinary performance assessments for concrete waste forms.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

300 Area Treatability Test: Laboratory Development of Polyphosphate Remediation Technology for In Situ Treatment of Uranium Contamination in the Vadose Zone and Capillary Fringe

This report presents results from bench-scale treatability studies conducted under site-specific conditions to optimize the polyphosphate amendment for implementation of a field-scale technology demonstration to stabilize uranium within the 300 Area vadose and smear zones of the Hanford Site. The general treatability testing approach consisted of conducting studies with site sediment and under site conditions, to develop an effective chemical formulation and infiltration approach for the polyphosphate amendment under site conditions. Laboratory-scale dynamic column tests were used to 1) quantify the retardation of polyphosphate and its degradation products as a function of water content, 2) determine the rate of polyphosphate degradation under unsaturated conditions, 3) develop an understanding of the mechanism of autunite formation via the reaction of solid phase calcite-bound uranium and aqueous polyphosphate remediation technology, 4) develop an understanding of the transformation mechanism, the identity of secondary phases, and the kinetics of the reaction between uranyl-carbonate and -silicate minerals with the polyphosphate remedy under solubility-limiting conditions, and 5) quantify the extent and rate of uranium released and immobilized based on the infiltration rate of the polyphosphate remedy and the effect of and periodic wet-dry cycling on the efficacy of polyphosphate remediation for uranium in the vadose zone and smear zone.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Preparation and Characterization of Chemical Plugs Based on Selected Hanford Waste Simulants

This report presents the results of preparation and characterization of chemical plugs based on selected Hanford Site waste simulants. Included are the results of chemical plug bench testing conducted in support of the M1/M6 Flow Loop Chemical Plugging/Unplugging Test (TP-RPP-WTP-495 Rev A). These results support the proposed plug simulants for the chemical plugging/ unplugging tests. Based on the available simulant data, a set of simulants was identified that would likely result in chemical plugs. The three types of chemical plugs that were generated and tested in this task consisted of: 1. Aluminum hydroxide (NAH), 2. Sodium aluminosilicate (NAS), and 3. Sodium aluminum phosphate (NAP). While both solvents, namely 2 molar (2 M) nitric acid (HNO3) and 2 M sodium hydroxide (NaOH) at 60°C, used in these tests were effective in dissolving the chemical plugs, the 2 M nitric acid was significantly more effective in dissolving the NAH and NAS plugs. The caustic was only slightly more effecting at dissolving the NAP plug. In the bench-scale dissolution tests, hot (60°C) 2 M nitric acid was the most effective solvent in that it completely dissolved both NAH and NAS chemical plugs much faster (1.5 – 2 x) than 2 M sodium hydroxide. So unless there are operational benefits for the use of caustic verses nitric acid, 2 M nitric acid heated to 60°C C should be the solvent of choice for dissolving these chemical plugs. Flow-loop testing was planned to identify a combination of parameters such as pressure, flush solution, composition, and temperature that would effectively dissolve and flush each type of chemical plug from preformed chemical plugs in 3-inch-diameter and 4-feet-long pipe sections. However, based on a review of the results of the bench-top tests and technical discussions, the Waste Treatment Plant (WTP) Research and Technology (R&T), Engineering and Mechanical Systems (EMS), and Operations concluded that flow-loop testing of the chemically plugged pipe sections would not provide any additional information or useful data. The decision was communicated through a Sub Contract Change Notice (SCN-070) that included a revised scope as follows: • Photographing the chemical plugs in the pipes before extrusion to compare the morphology of aged gels with that of fresh gels. • Setting up an extrusion apparatus and extruding the chemical plugs. • Documenting the qualitative observations on the efforts to remove the chemical plug materials from the pipe sections. • Performing X-ray diffraction (XRD) analysis of extruded gel samples to detect any crystallization of gel during storage. • Disposing of the extruded gel as a waste. • Documenting the analytical results in a test report. There were no significant morphological differences between the fresh and aged plugs except for an overgrowth of small transparent crystals on the surface of the aged NAS gel plug. An initial pressure of <150 psi was required to start extruding the aged NAS and NAP plugs, whereas the NAH plug began to extrude with the application of minimal pressure. The shear strength of extruded samples ranged from ~9 to >15 KPa for the NAS plug and from ~2 to 6 KPa for the NAH plug. Following extrusion, the NAP plug sections were thixotropic. The bulk of all the aged gel plugs consisted of amorphous material with nitratine constituting the crystalline phase. A separate question about the whether the current in-tank waste conditions will bound the future multi-tank blended feed conditions for the Waste Treatment Plant is outside the scope of this study.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Aluminoborosilicate Waste Glass Dissolution under Alkaline Conditions at 40°C: Implications for a Chemical Affinity-Based Rate Equation

Single-pass flow-through (SPFT) experiments were conducted with aluminoborosilicate waste glasses to evaluate how changes in solution composition affect the dissolution rate (r) at 40°C and pH(23°C) = 9.0. The three prototypic low-activity waste (LAW) glasses; LAWE-1A, -95A, and -290A, used in these experiments span a wide range covering the expected processing composition of candidate immobilized low-activity waste (ILAW) glasses. Results suggest incongruent release of Al, B, Na, and Si at low flow-rate (q) to sample surface area (S) [log10 (q/S) < -8.9 (m s-1)] whereas congruent release was observed at high q/S [log10 (q/S) > -7.9 (m s-1)]. Dissolution rates increase from log10 (q/S) ≈ -9.3 to -8.0 (m s-1) and then become constant at log10 (q/S) > -7.9 (m s-1). Forward (maximum) dissolution rates, based on B release, are the same irrespective of glass composition, evident by the dissolution rates being within the experimental error of one another (r1A = 0.0301 ±0.0153 g m-2 d-1, r95A = 0.0248 ±0.0125 g m-2 d-1, and r290A = 0.0389 ±0.0197 g m-2 d-1). Finally these results support the use of a chemical affinity based rate law to describe glass dissolution as a function of solution composition.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗