High-temperature treatment of In-doped CZT crystals grown by the high-pressure Bridgman method

We evaluated the effect of high-temperature treatment of Cd0.9Zn0.1Te:In single crystals using Hall-effect measurements, medium- and high-temperature annealing under various deviations from stoichiometry, and infra-red (IR) transmission microscopy Annealing at ~730 K sharply increased the electrical conductivity (by ~1-2 orders-of-magnitude). Plots of the temperature- and cadmium-pressure dependences of the electrical conductivity, carrier concentration, and mobility were obtained. Treating previously annealed Cd-samples under a Te overpressure at 1070 K allowed us to restore their resistance to its initial high values. The main difference in comparing this material with CdTe was its lowered electron density. We explained our results within the framework of Kröger’s theory of quasi-chemical reactions between point defects in solids.

60 APPLIED LIFE SCIENCES↗

Drift time variations in CdZnTe detectors measured with alpha-particles: Their correlation with the detector’s responses

Homogeneity of properties related to material crystallinity is a critical parameter for achieving high-performance CdZnTe (CZT) radiation detectors. Unfortunately, this requirement is not always satisfied in today's commercial CZT material due to high concentrations of extended defects, in particular subgrain boundaries, which are believed to be part of the causes hampering the energy resolution and efficiency of CZT detectors. In the past, the effects of subgrain boundaries have been studied in Si, Ge and other semiconductors. It was demonstrated that subgrain boundaries tend to accumulate secondary phases and impurities causing inhomogeneous distributions of trapping centers. It was also demonstrated that subgrain boundaries result in local perturbations of the electric field, which affect the carrier transport and other properties of semiconductor devices. The subgrain boundaries in CZT material likely behave in a similar way, which makes them responsible for variations in the electron drift time and carrier trapping in CZT detectors. In this work, we employed the transient current technique to measure variations in the electron drift time and related the variations to the device performances and subgrain boundaries, whose presence in the crystals were confirmed with white beam X-ray diffraction topography and infrared transmission microscopy.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Nanosecond in situ transmission electron microscope studies of the reversible Ge{sub 2}Sb{sub 2}Te{sub 5} crystalline <==> amorphous phase transformation

Chalcogenide-based phase-change materials have wide use in optical recording media and are growing in importance for use in non-volatile electronic memory. For both applications, rapid switching between the amorphous and crystalline phases is necessary, and understanding the changes during rapidly driven phase transitions is of scientific and technological significance. Laser-induced crystallization and amorphization occur rapidly and changes in atomic structure, microstructure, and temperature are difficult to observe experimentally and determine computationally. We have used nanosecond-scale time-resolved diffraction with intense electron pulses to study Ge{sub 2}Sb{sub 2}Te{sub 5} during laser crystallization. Using a unique and unconventional specimen geometry, cycling between the amorphous and crystalline phases was achieved, enabling in situ transmission electron microscope (TEM) study of both microstructural and crystallographic changes caused by repeated switching. Finite element analysis was used to simulate interactions of the laser with the nano-structured specimens and to model the rapidly changing specimen temperature. Such time-resolved experimental methods combined with simulation of experimentally inaccessible physical characteristics will be fundamental to advancing the understanding of rapidly driven phase transformations.

36 MATERIALS SCIENCE↗

Effect of Extended Defects in Planar and Pixelated CdZnTe Detectors

We evaluated a spectroscopy-grade 15 x 15 x 7 mm{sup 3} CdZnTe (CZT) crystal with a high {mu}{tau}-product, > 10{sup -2} cm{sup 2}/V, but impaired by microscopic extended defects, such as walls of dislocations, low-angle and sub-grain boundaries, and Te inclusions. First, we evaluated a planar detector fabricated from this crystal using a Microscale X-ray Detector Mapping (MXDM) technique. Then, we fabricated from the same crystal a pixel detector to study local non-uniformities of the electric field. The measured X-ray response maps confirmed the presence of non-uniformities in the charge transport, and they showed that the global- and local-distortions of the internal E-field correlated to the extended defects and space-charge buildup on the side surfaces.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Effect of Te Inclusions in CdZnTe Crystals at Different Temperatures

CdZnTe crystals often exhibit nonuniformities due to the presence of Te inclusions and dislocations. High concentrations of such defects in these crystals generally entail severe charge-trapping, a major problem in ensuring the device's satisfactory performance. In this study, we employed a high-intensity, high-spatial-resolution synchrotron x-ray beam as the ideal tool to generate charges by focusing it over the large Te inclusions, and then observing the carrier's response at room- and at low-temperatures. A high spatial 5-{micro}m resolution raster scan revealed the fine details of the presence of extended defects, like Te inclusions and dislocations in the CdZnTe crystals. A noticeable change was observed in the efficiency of electron charge collection at low temperature (1 C), but it was hardly altered at room-temperature.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Defect Levels of Indium-doped CdMnTe Crystals

Using photoluminescence (PL) and current deep-level transient spectroscopy (I-DLTS), we investigated the electronic defects of indium-doped detector-grade CdMnTe:In (CMT:In) crystals grown by the vertical Bridgman method. We similarly analyzed CdZnTe:In (CZT:In) and undoped CdMnTe (CMT) crystals grown under the amount of same level of excess Te and/or indium doping level to detail the fundamental properties of the electronic defect structure more readily. Extended defects, existing in all the samples, were revealed by synchrotron white beam x-ray diffraction topography and scanning electron microscopy. The electronic structure of CMT is very similar to that of CZT, with shallow traps, A-centers, Cd vacancies, deep levels, and Te antisites. The 1.1-eV deep level, revealed by PL in earlier studies of CZT and CdTe, were attributed to dislocation-induced defects. In our I-DLTS measurements, the 1.1-eV traps showed different activation energies with applied bias voltage and an exponential dependence on the trap-filling time, which are typical characteristics of dislocation-induced defects. We propose a new defect-trap model for indium-doped CMT crystals.

36 MATERIALS SCIENCE↗

Correlations Between Crystal Defects and Performance of CdZnTe Detectors

Poor crystallinity remains a major problem affecting the availability and cost of CdZnTe (CZT) detectors. Point defects are responsible for small gradual charge loss and correlated with the electron clouds' drift times, which allows electronic correction of the output signals to achieve high spectral-resolution even with large-volume CZT detectors. In contrast, extended defects causes significant charge losses, which typically are uncorrelated, and, thus, result in much greater fluctuations of the output signals that cannot be corrected. Although extended defects do not affect all the interaction events, their fraction rapidly increases with the crystal's thickness and volume. In this paper, we summarize our recent results from testing CZT material and detectors that emphasize the particular roles of two types of extended defects, and their contributions to the device's overall performance.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Hybrid Contacts for CZT Virtual Frisch-grid Detectors

In our previous design of virtual Frisch-grid CdZnTe (CZT) detectors, the charge drift-lines can be terminated at the side surfaces before the carriers reach the collecting anode; this results in a loss of signal from the interacting events near the detector's edges. Here, we describe our new design for the anode contact that reduces these edge effects by focusing the electric field towards the detectors' central axes. Four detectors were fabricated with the new hybrid anode contact, and their performances were evaluated and compared to those from the previous design for our virtual Frisch-grid detectors. The results obtained for all four showed similar improvement: therefore, we illustrate them with the findings from one detector.