Insights into Prismatic Loop Formation in Irradiated Fe–Cr Alloys from Hypothesis-Driven Active Learning and Causal Analysis

Neutron and electron irradiation experimental studies conducted on body-centered cubic Fe and Fe–Cr alloys have established two prismatic dislocation loop populations, which have Burgers vectors of either a/2$\langle$111$\rangle$ or a$\langle$100$\rangle$. Here, the loop formation depends on factors such as dose (D), dose rate (D rt ), temperature (T), chromium content (Cr%), and other alloying elements. Hence, it is important to understand how irradiation-induced dislocation loops evolve conditional upon the loop characteristics, such as loop density (DD), average loop size d̅, and irradiation parameters (D, D rt , T, and irradiation type), which is still an active area of research. To understand these complex structure–property relationships, machine learning (ML) is employed in a three-step approach. This includes imputing missing data with a k-nearest neighbor, generating functionalized features, and assessing feature importance with random forest classification and regression. Physics-based features are incorporated in a hypothesis-driven active learning scheme to overcome data unavailability challenges. Insights obtained from ML models (i) to categorize dislocation loop types, show the highest correlation with d̅; (ii) Log(DD), obtained through mathematical formulations involving D, Cr%, d̅, and T (e.g., Log(DD) ~ D + exp(-Cr%) + 1/d̅ and log(DD) ~ D + exp(-Cr%) + 1/T). Hypothesis-driven active learning is able to predict Log(DD) in which the experimental date is not known. Causal models verify cause–effect relationships for dislocation loop classification and irradiation factors in FeCr alloys.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Development of multi-scale computational frameworks to solve fusion materials science challenges

Over the past two decades, the US-DOE has funded multiple projects that rely on high-performance computing and exascale computing platforms to accelerate scientific discoveries and address grand scientific challenges, such as harnessing fusion energy. In this article, we review in detail one of these efforts aimed at enhancing our capability to model plasma-facing materials subject to plasma and high-energy ion/neutron irradiation. The plasma surface interactions project has built a multi-scale modeling framework where many of the plasma- and high-energy ion/neutron irradiation-induced effects occurring in tungsten are explored. Here, this knowledge is used to develop atomistically-informed, high-fidelity continuum and meso-scale models that can be validated against experiments. We review the developments within this project, with attention to experimental validation efforts, and specifically highlight activities associated with: helium bubble bursting and equation of state, and hydrogen-helium interactions in tungsten; atomistically-informed model development for beryllium-tungsten material mixing; coupling of scrape-of-layer plasma, sheath and material models; and coupling of stochastic cluster-dynamics and crystal plasticity models to address radiation effects in tungsten under stress. Finally, we present how the project is preparing for future computational architectures, for instance through efforts to adapt atomistic methods to exascale computing.

36 MATERIALS SCIENCE↗

Assessment of the literature about Be-W mixed material layer formation in the fusion reactor environment

All plasma facing surfaces in a fusion reactor, whether initially pure or an alloy, will rapidly evolve into a mixed material due to plasma-induced erosion, migration and redeposition. Beryllium (Be) erosion from the main chamber, and its transport and deposition on to a tungsten (W) divertor results in the growth of mixed Be-W layers, which can evolve to form beryllides. These Be-W mixed materials exhibit generally less desirable properties than pure tungsten or pure beryllium, such as lower melting points. In order to better understand the parameter space for growth of these alloys, this paper reviews the literature on Be-W mixed material formation experiments—in magnetically confined fusion reactors, in linear plasma test stands, and during thin-film deposition—and on computational modeling of Be-W interactions, as well as briefly assesses the Be-W growth kinetics. We conclude that the following kinetic steps drive the material mixing: adsorption of the implanted/deposited ion on the metal surface; diffusion of the implanted/deposited ion from surface into the bulk, which is accelerated by defects; and loss of deposited material through erosion. Adsorption dominates (or prevents) material mixing in thin-film deposition experiments, whereas diffusion drives material mixing in plasma exposures due to the energetic ion implantation.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Equation of state for He bubbles in W and model of He bubble growth and bursting near W{100} surfaces derived from molecular dynamics simulations

Abstract Molecular dynamics (MD) simulations are performed to derive an equation of state (EOS) for helium (He) bubbles in tungsten (W) and to study the growth of He bubbles under a W(100) surface until they burst. We study the growth as a function of the initial nucleation depth of the bubbles. During growth, successive loop-punching events are observed, accompanied by shifts in the depth of the bubble towards the surface. Subsequently, the MD data are used to derive models that describe the conditions that cause the loop punching and bursting events. Simulations have been performed at 500, 933, 1500, 2000, and 2500 K to fit the parameters in the models. To compute the pressure in the bubble at the loop punching and bursting events from the models, we derive an EOS for He bubbles in tungsten with an accompanying volume model to compute the bubble volume for a given number of vacancies ( $$N_\text {V}$$ N V ), He atoms ( $$N_\text {He}$$ N He ), and temperature ( T ). To derive the bubble EOS, we firstly derive the EOS for a free He gas. The derived free-gas EOS can accurately predict all MD data included in the analysis (which span up to 54 GPa at 2500 K). Subsequently, the bubble EOS is derived based on the free-gas EOS by correcting the gas density to account for the interaction between He and W atoms. The EOS for the bubbles is fitted to data from MD simulations of He bubbles in bulk W that span a wide range of gas density and sizes up to about 3 nm in diameter. The pressure of subsurface bubbles at the loop punching events as calculated using the bubble-EOS and the volume model agrees well with the pressure obtained directly from the MD simulations. In the loop punching model, for bubbles consisting of $$N_\text {V}$$ N V vacancies and $$N_\text {He}$$ N He helium atoms, the $$N_\text {He}/N_\text {V}$$ N He / N V ratio that causes the event, the resulting increase in $$N_\text {V}$$ N V , and the associated shift of the bubble depth are formulated as a function of $$N_\text {V}$$ N V and T . In the bursting model, a bubble must simultaneously reach a certain depth and $$N_\text {He}/N_\text {V}$$ N He / N V ratio in order to burst. The burst depth and $$N_\text {He}/N_\text {V}$$ N He / N V are also modeled as a function of $$N_\text {V}$$ N V and T . The majority of the loop punching events occur at bubble pressures between 20 and 60 GPa, depending on the bubble size and temperature. The larger the bubble and the higher the temperature, the lower the bubble pressure. Furthermore, our results indicate that at a higher temperature, a bubble can burst from a deeper region.

36 MATERIALS SCIENCE↗

Thermal gradient effect on helium and self-interstitial transport in tungsten

First-wall materials in a fusion reactor are expected to withstand harsh conditions, with high heat and particle fluxes that modify the materials microstructure. These fluxes will create strong gradients of temperature and concentration of diverse species. Besides the He ash and the hydrogenic species, neutron particles generated in the fusion reaction will collide with the material creating intrinsic defects, such as vacancies, self-interstitials atoms (SIAs), and clusters of such point defects. These defects and the He atoms will then migrate in the presence of the aforementioned gradients. In this study, we use nonequilibrium molecular dynamics to analyze the transport of He and SIAs in the presence of a thermal gradient in tungsten. We observe that, in all cases, the defects and impurity atoms tend to migrate toward the hot regions of the tungsten sample. The resulting species concentration profiles are exponential distributions, rising toward the hot regions of the sample, in agreement with irreversible thermodynamics analysis. For both He atoms and SIAs, we find that the resulting species flux is directed opposite to the heat flux, indicating that species transport is governed by a Soret effect (thermal-gradient-driven diffusion) characterized by a negative heat of transport that drives species diffusion uphill (from the cooler to the hot regions of the sample). Here, we demonstrate that the steady-state species profiles obtained accounting for the Soret effect vary significantly from those where temperature-gradient-driven transport is not considered and discuss the implications of such a Soret effect on the response to plasma exposure of plasma-facing tungsten.

36 MATERIALS SCIENCE↗

Effects of elastic softening and helium accumulation kinetics on surface morphological evolution of plasma-facing tungsten

Based on a continuous-domain model, capable of accessing the spatiotemporal scales relevant to fuzz formation on the surface of plasma-facing component (PFC) tungsten, we report self-consistent simulation results that elucidate the effects of elastic softening and helium (He) accumulation kinetics on the surface morphological response of PFC tungsten. The model accounts for the softening of the elastic moduli in the near-surface region of PFC tungsten, including both thermal softening at high temperature and softening due to He accumulation upon He implantation. The dependence of the elastic moduli on the He content follows an exponential scaling relation predicted by molecular-dynamics simulations, while the He content in the near-surface region of PFC tungsten evolves according to a first-order saturation kinetics, consistent with experimental and simulation results reported in the literature. We establish that this elastic softening accelerates both nanotendril growth on the PFC surface and the onset of fuzz formation. We also explore the role of the rate of He accumulation to a saturation level in the near-surface region of irradiated tungsten in the onset of fuzz formation. For PFC tungsten surfaces such as W(110) where, under typical irradiation conditions, the characteristic time scale for stress-driven surface diffusion is comparable to the characteristic time scale for He accumulation, we find that accelerating the rate of He accumulation accelerates the growth rate of nanotendrils emanating from the surface. Additionally, we present a systematic parametric study of the PFC surface morphological response to explore its dependence on the He accumulation kinetics that is controlled by the irradiation conditions for low-energy implantation. Finally, we introduce an incubation time for nanotendril growth on the PFC surface, a concept equivalent to that of incubation fluence discussed in the literature, to predict and explain the minimum exposure time required to observe fuzz formation on PFC tungsten surfaces.

36 MATERIALS SCIENCE↗