Coupons (mini-modules) experimental data
Adhesion testing results on mini-module coupons (cell/encapsulant/glass laminates) that were aged under the different accelerated aging conditions (outlined more in the DataHub URL).
Engineering topics
Publications and source records attributed to Dauskardt, Reinhold.
Adhesion testing results on mini-module coupons (cell/encapsulant/glass laminates) that were aged under the different accelerated aging conditions (outlined more in the DataHub URL).
Open-air plama processing for large-area solar modules
By using an ultra-fast scalable open-air plasma deposition technique to deposit the perovskite layer and combining that with monolithic scribing, we are able to achieve high efficiency and large area perovskite solar modules.
Our research is focused on fundamental studies related to the molecular design, synthesis, characterization and modeling of molecular-reinforced hybrid glass films for superior mechanical and fracture properties. Molecular-reinforced hybrid glass films exhibit unique electro-optical properties while maintaining excellent thermal stability. They have important technological application for emerging nanoscience and energy technologies including anti-reflective and ultra-barrier layers in photovoltaics, display technologies, as well as quantum technologies. However, they are often inherently brittle in nature, do not adhere well to adjacent substrates, and exhibit poor mechanical properties. Furthermore, a robust understanding of the underlying mechanisms of deformation, fracture and fatigue has been lacking particularly given their mechanically fragile nature. The related lack of structure-property relationships between molecular structure, mechanical properties and processing represents a fundamental challenge to their integration into device technologies, compromises their thermomechanical reliability and has thwarted efforts to improve mechanical and, particularly, fracture properties.
We report on a scalable, low-temperature TiOx electron transport layer (ETL) produced directly on top of perovskite in an inverted architecture device by an open-air chemical vapor deposition (OA-CVD) process. The OA-CVD pyrolysis of a titanium ethoxide precursor forms a fully inorganic, conformal, and compact TiOx film. The resultant film is mechanically robust and exhibits a fracture toughness 30-fold higher than commonly used fullerene-based ETL films. The TiOx is an effective barrier layer against environmental degradation—unencapsulated devices with the TiOx ETL retain 60% of their initial efficiency after 1000 hours in ambient aging conditions—compared to devices with a fullerene ETL which were inoperable after 144 hours. Inverted architecture devices with an optimized TiOx ETL thickness of 70nm exhibited high open-circuit voltages of 1.08V. We comment on the photocatalytic properties of TiOx and the influence of an amorphous film on maximum power point stability.
Intrinsically and fully stretchable active-matrix-driven displays are an important element to skin electronics that can be applied to many emerging fields, such as wearable electronics, consumer electronics and biomedical devices. Here, we show for the first time a fully stretchable active-matrix-driven organic light-emitting electrochemical cell array. Briefly, it is comprised of a stretchable light-emitting electrochemical cell array driven by a solution-processed, vertically integrated stretchable organic thin-film transistor active-matrix, which is enabled by the development of chemically-orthogonal and intrinsically stretchable dielectric materials. Our resulting active-matrix-driven organic light-emitting electrochemical cell array can be readily bent, twisted and stretched without affecting its device performance. When mounted on skin, the array can tolerate to repeated cycles at 30% strain. This work demonstrates the feasibility of skin-applicable displays and lays the foundation for further materials development.
Ethylene vinyl acetate (EVA) has for decades been the preferred material for photovoltaic (PV) module encapsulation. However, while it is relatively inexpensive and initially adheres well to module components, EVA discolors with age and - as interfacial adhesion degrades - becomes susceptible to delamination, ultimately resulting in reduced module efficiency and shortened service lifetimes. As potential replacements for EVA, ionomer thermoplastic materials cure faster, are more resistant to discoloration and potential induced degradation, and do not evolve corrosive acetic acid, making them compatible with new device materials such as perovskites. Since there is limited information on ionomer durability for PV module applications, a series of field and accelerated laboratory aging studies were conducted to assess ionomer interface stability in the presence of terrestrial environmental stressors. It is shown that adhesion to the glass and cell interfaces of PV modules is inferior to EVA, both before and after aging, rendering ionomers particularly susceptible to delamination after short timeframes. Potential solutions to improve ionomer adhesion are discussed.
We report on the development of an aqeuous spray coating process to deposit mechanically robust NiO for efficient perovskite solar cells.
Implementing open-air processing to develop high efficiency, stable, large-area perovskite solar modules
Here, this study begins to investigate the role of environmental factors, such as temperature and humidity, on the delamination kinetics of the ethylene vinyl acetate (EVA)/silicon-photovoltaic (Si-PV) cell interface. A fracture mechanics approach based on a single cantilever beam technique is employed to measure the delamination rate as a function of applied driving force. To glean insight into the mechanisms of bonding and degradation at this interface, and the effect of manufacturing variability and quality, we consider a high-quality pristine EVA and two EVAs formulated with reduced amounts of its adhesion promoter, silane. Results indicate that a bulk change in the viscoelastic properties of the EVA dominates the delamination kinetics at high driving forces and low humidity and the effect of a chemical reaction only becomes apparent at higher humidity and lower driving forces. These findings suggest that only interfacial phenomenon of susceptible, degraded material may have to be considered to adequately model PV module delamination failure.
A significant challenge facing the solar industry is developing a reliable method to accurately predict photovoltaic module reliability over decades-long operating lifetimes. For the specific case of encapsulant adhesion-where interface delamination directly leads to reduced module efficiency- predictive models are critical for assessing long term reliability of new module materials over time frames conducive to research and development. We thus present a framework for modelling the temporal evolution of encapsulant adhesion by accounting for chemicaldegradation mechanisms at the molecular level. The model is developed though an unprecedented survey of encapsulant adhesion energy measurements from lab and field- aged modules with agingtimes spanning months to nearly three decades. Chemical analyses of new and aged EVA encapsulants are conducted to identify the dominant degradation mechanisms for modelling interface adhesion: deactivation, polymer chain scission, and hydrolytic polymerization. The strength of this framework is in the model's modularity, which renders it adaptable to any type of aging environment and encapsulation material.
Delamination of encapsulant materials from PV cell surfaces often appears to originate at regions with metallization. Using a fracture mechanics based metrology, the adhesion of EVA encapsulant to screen printed silver metallization was evaluated. At room temperature, the fracture energy, G c [J/m 2 ], of the EVA/silver interface (952 J/m 2 ) was ~70% lower than that of the EVA/AR coating (>2900 J/m 2 ) and ~60% lower than that of the EVA to the surface of cell (2265 J/m 2 ). After only 300 hours of damp heat aging, the adhesion energy of the silver interface dropped to and plateaued at ~50-60 J/m 2 , while that of the EVA/AR coating and EVA/cell remained mostly unchanged. Elemental surface analysis showed that the EVA separates from the silver in a purely adhesive manner, indicating that bonds at the interface were likely displaced in the presence of humidity and chemical byproducts at elevated temperature, which in part accounts for the propensity of metallized surfaces to delaminate in the field.
Extending photovoltaic (PV) module lifetimes beyond 30 years is a goal of significant priority. A challenge that must first be addressed, however, is the development of a predictive reliability model that captures the synergy of terrestrial stressors on module degradation, particularly at encapsulant interfaces. Using a metrology designed specifically for PV modules, a comprehensive study of the widely used ethylene vinyl acetate encapsulant was performed in which encapsulant adhesion was evaluated as a function of environmental stressors (UV exposure, temperature, and humidity) for modules aged both under accelerated lab and internationally located field conditions for months to nearly 3 decades. Mechanical and chemical characterization methods are combined with fundamental polymer reaction engineering to unravel the degradation processes active at the molecular scale that lead to encapsulant delamination. An analytical and modular model framework is put forward enabling the prediction of long-term PV module durability, starting from fundamental principles at the molecular level and explicitly accounting for bond rupture events in the bulk encapsulant and at the encapsulant interfaces. Successful parameter tuning to adhesion data indicates a dominant occurrence of deacetylation, β-scission, and hydrolytic depolymerization, respectively. The model contributes to the longstanding challenge of predicting module lifetimes in any geographic location while minimizing time-consuming and costly aging studies.
Delamination of encapsulant materials from PV cell surfaces often appears to originate at regions with metallization. Using a fracture mechanics based metrology, the adhesion of ethylene vinyl acetate (EVA) encapsulant to screen-printed silver metallization was evaluated. At room temperature, the fracture energy Gc [J/m2] of the EVA/silver interface (952 J/m2) was ~70% lower than that of the EVA/antireflective (AR) coating (>2900 J/m2) and ~60% lower than that of the EVA to the surface of cell (2265 J/m2). After only 300 h of damp heat aging, the adhesion energy of the silver interface dropped to and plateaued at ~50-60 J/m2 while that of the EVA/AR coating and EVA/cell remained mostly unchanged. Elemental surface analysis showed that the EVA separates from the silver in a purely adhesive manner, indicating that bonds at the interface were likely displaced in the presence of humidity and chemical byproducts at elevated temperature, which in part accounts for the propensity of metalized surfaces to delaminate in the field.
The width-tapered cantilever beam method is used to quantify the debond energy (adhesion) of encapsulant and backsheet structures of 32 modules collected from the field. The collected population of modules contains both those that have remained intact and those with instances of either or both encapsulant and backsheet delamination. From this survey, initial threshold values (an adhesion value above which a module should remain intact throughout its lifetime) for encapsulant and backsheet interfaces are proposed. For encapsulants this value is ~ 160J/m 2 and for backsheets ~ 10J/m 2 . Here, it is expected that these values will continue to be refined and evolve as the width-tapered cantilever beam method gets adopted by the PV industry, and that they may aid in the future improvement of accelerated lifetime tests and the development of new, low-cost materials.
Delamination of encapsulant materials from PV cell surfaces often appears to originate at regions with metallization. Using a fracture mechanics based metrology, the adhesion of EVA encapsulant to screen printed silver metallization was evaluated. At room temperature, the fracture energy, Gc [J/m2], of the EVA/silver interface (952 J/m2) was ~70% lower than that of the EVA/AR coating (>2900 J/m2) and ~60% lower than that of the EVA to the surface of cell (2265 J/m2). After only 300 hours of damp heat aging, the adhesion energy of the silver interface dropped to and plateaued at ~50-60 J/m2, while that of the EVA/AR coating and EVA/cell remained mostly unchanged. Elemental surface analysis showed that the EVA separates from the silver in a purely adhesive manner, indicating that bonds at the interface were likely displaced in the presence of humidity and elevated temperature, and may explain the propensity for delamination to occur at metallized surfaces in the field.
A fracture mechanics based approach for quantifying adhesion at every interface within the PV module laminate is presented. The common requirements of monitoring crack length and specimen compliance are circumvented through development of a width-tapered cantilever beam method. This technique may be applied at both the module and coupon level to yield a similar, quantitative, measurement. Details of module and sample preparation are described and first results on field-exposed modules deployed for over 27 years presented.
Photovoltaic modules are designed to operate for decades in terrestrial environments. However, mechanical stress, moisture, and ultraviolet radiation eventually degrade protective materials in modules, particularly their adhesion properties, eventually leading to reduced solar cell performance. Despite the significance of interfacial adhesion to module durability, currently there is no reliable technique for characterizing module adhesion properties. We present a simple and reproducible metrology for characterizing adhesion in photovoltaic modules that is grounded in fundamental concepts of beam and fracture mechanics. Using width-tapered cantilever beam fracture specimens, interfacial adhesion was evaluated on relevant interfaces of encapsulation and backsheet structures of new and 27-year-old historic modules. The adhesion energy, Gc [J/m 2 ], was calculated from the critical value of the strain energy release rate, G, using G = βP 2 , where β (a mechanical and geometric parameter of the fracture specimen) and P (the experimentally measured critical load) are constants. Under some circumstances where testing may result in cracking of brittle layers in the test specimen, measurement of the delamination length in addition to the critical load was necessary to determine G. Relative to new module materials, backsheet adhesion was 95% and 98% lower for historic modules that were exposed (operated in the field) and unexposed (stored on-site, but out of direct sunlight), respectively. Encapsulation adhesion was 87-94% lower in the exposed modules and 31% lower in the unexposed module. As a result, the metrology presented here can be used to improve module materials and assess long-term reliability.