Search NASA⌕ Search

Engineering topics

Dryepondt, Sebastien

Publications and source records attributed to Dryepondt, Sebastien.

41 records · Page 3

High Temperature Oxidation Lifetime Modelling of thin-walled components

High temperature material solutions for future power generation applications require longer component lifetimes at higher temperatures to improve durability and efficiency. From a research and development point of view, the lifetimes are too long for experimental verification. Thus, accurate lifetime models are needed. Examples are provided where modeling is being applied to lifetime prediction of thin-walled NiCr wrought alloy components. Specific laboratory experiments have been conducted for alloy X at 900°-950°C in dry air and air with water vapor with cycle times from 1 to 500 h. Along with microstructure characterization, comparisons are made between experiment and model predictions. The eventual goal is to predict both oxidation and mechanical behavior.

Pillai, Rishi↗

High Temperature Oxidation Lifetime Modeling of Commercial Wrought NiCr

To increase efficiency, a wide range of energy-related applications is pushing components to higher temperatures where environmental degradation can be life limiting. Unlike mechanical properties such as creep, there is no simple degradation parameter to capture the time-temperature-thickness limitations of candidate alloys. An initial model has been proposed and additional work is in progress to validate the model with longer-term exposures at 900°C and modify the model to capture additional service parameters such as cycle frequency and the effect of water vapor. Additional issues are discussed including the minimum data required for a new alloy to be modeled in the proposed manner.

Pint, Bruce↗

3D Microscopy to Assess the Effect of High Temperature Cyclic Oxidation on the Deformation of Cast and ODS FeCrAlY Alloys

Specimen deformation, oxide scale growth, and scale cracking were monitored for cyclic oxidation exposures at 1200 °C of three cast FeCrAlY(Hf) alloys and two oxide dispersion strengthened (ODS) FeCrAl alloys. Evolution of both the specimen geometry and surface deformation was quantified using 3D optical microscopy. The stress in the alumina scale was also measured using photo-stimulated luminescence piezospectroscopy. The goal was to examine the effect of stress generation and stress relaxation on scale spallation for FeCrAl materials with drastic differences in terms of high temperature strengths. After 1000, 1-h cycles, the cast alloys exhibited significant deformation with a convoluted oxide scale, leading for the two Hf-free FeCrAlY alloys to undergo crack formation and spallation. For the Hf-containing FeCrAlY, limited spallation was observed due to the localization of spallation at grain boundaries, the large grain structure, and the beneficial effect of Hf on scale adhesion. On the other hand, limited deformation was measured for the ODS FeCrAl alloys, with minimal cracking and scale spallation for alloy PM2000 after 1000 h. A higher spallation rate was observed for ODS MA956, which was attributed to a high defect concentration in the alumina scale that formed. The mechanisms leading to spallation during cyclic oxidation for the cast and ODS FeCrAlY alloys are described.

36 MATERIALS SCIENCE↗

Characterization of the Martensitic Transformation in NiPtAl Alloy Using Digital Holographic Imaging

Surface reliefs due to phase transformations in a 56.8Ni-5.6Pt-37.6Al at. pct alloy were characterized in situ using digital holographic imaging during thermal cycling from room temperature up to 405 K (132 °C). The 3D images of the surface revealed that the austenite plates formed during heating are exactly the same for each cycle, which is not the case for the martensite plates formed during cooling. The martensite start temperature was found to vary by up to ~ 20 K from one grain to another within the same specimen. The absence of Ni 3 Al γ' precipitates, due to the relatively high Al content, results in the propagation of the martensitic transformation over grains up to a millimeter in size. Bright-field optical imaging showed the formation of large martensite plates in some grains, with cracks perpendicular to these plates, upon cycling. Cracks were also observed at grain boundaries and could be related to the height variations across the grain boundaries.

36 MATERIALS SCIENCE↗

New Creep-Resistant Cast Alloys with Improved Oxidation Resistance in Water Vapor at 650–800°C

Cast stainless steel CF8C-Plus (19wt%Cr/12%Ni) has excellent creep properties, but limited oxidation resistance above 700 C in environments containing H 2 O. One strategy to improve the alloy oxidation performance is to increase the Cr and Ni concentration. Two new alloys, with, respectively, 21wt%Cr 15wt%Ni and 22wt%Cr 17.5wt%Ni were therefore developed and their long-term oxidation behaviors in humid air were compared with the oxidation behavior of five other cast alloys. Also, at 650 C and 700 C, all the alloys formed internal Cr-rich nodules, and outer nodules or layers rich in Fe and Ni, but they grew a protective Cr-rich inner layer over time. At 750 C, the lower alloyed steels such as CF8C-Plus showed large metal losses, but the two new alloys still exhibited a protective oxidation behavior. The 21Cr 15Ni alloy was severely oxidized in locations at 800 C, but that was not the case for the 22Cr 17.5Ni alloy. Thus, the two new modified alloys represent a potential operating temperature gain of, respectively, 50 C and 100 C in aggressive environments compared with the CF8C-Plus alloy.

36 MATERIALS SCIENCE↗