The impact of solvent doping on the morphology and performance of spray-coated PEDOT:dPSS: A USANS and SANS study
Not Available
Engineering topics
Publications and source records attributed to Etampawala, Thusitha.
Not Available
It is generally believed that the strength of the polymer nanoparticle interaction controls the modification of near-interface segmental mobility in polymer nanocomposites (PNCs). However, little is known about the effect of covalent bonding on the segmental dynamics and glass transition of matrix-free polymer-grafted nanoparticles (PGNs), especially when compared to PNCs. In this article, we directly compare the static and dynamic properties of poly(2-vinylpyridine)/silica-based nanocomposites with polymer chains either physically adsorbed (PNCs) or covalently bonded (PGNs) to identical silica nanoparticles (RNP = 12.5 nm) for three different molecular weight (MW) systems. Interestingly, when the MW of the matrix is as low as 6 kg/mol (RNP/Rg = 5.4) or as high as 140 kg/mol (RNP/Rg= 1.13), both small-angle X-ray scattering and broadband dielectric spectroscopy show similar static and dynamic properties for PNCs and PGNs. However, for the intermediate MW of 18 kg/mol (RNP/Rg = 3.16), the difference between physical adsorption and covalent bonding can be clearly identified in the static and dynamic properties of the interfacial layer. We ascribe the differences in the interfacial properties of PNCs and PGNs to changes in chain stretching, as quantified by self-consistent field theory calculations. These results demonstrate that the dynamic suppression at the interface is affected by the chain stretching; that is, it depends on the anisotropy of the segmental conformations, more so than the strength of the interaction, which suggests that the interfacial dynamics can be effectively tuned by the degree of stretching a parameter accessible from the MW or grafting density.
The kinetics of the formation of novel porous metal organic nanotubes, [Ag2(4,4 -(1,4-(xylene)diyl)bis- (1,2,4-triazole) (NO3)2] NMP, was investigated by means of ex-situ time-resolved small-angle X-ray scattering (SAXS) and scanning electron microscopy (SEM). The SAXS results were modeled using the Gualtieri model, which decouples the nucleation and growth processes giving additional insight into the crystal formation mechanism. The results show that the semirigid 4,4 -(1,4-(xylene)diyl)bis(1,2,4-triazole) ligand (L) binds with silver ions, adopting a seesaw geometry to form a polydisperse isotropic framework immediately after mixing the ligands and metal ions. In addition, the SEM imaging demonstrates that the microcrystals grow anisotropically, with nucleation along the edge of the 3D aggregate. These combined data demonstrate that the growth of this MONT occurs in two steps: a rapid formation of an isotropic porous structure immediately after mixing the reactant, which then develops anisotropically as the aggregates of nanorods grow in a preferred direction. The anisotropic growth of the crystal is autocatalytic and determined by the rate of nucleation of new growth sites on the crystals. Moreover, the results of this analysis elucidate, for the rst time, the exact order of the competing processes that occur in the synthesis of these MONTs, showing that their anisotropic growth occurs on the initial 3D aggregate and appears to be directed by the interplay between the surface energies that exist during the MONT formation process. This insight is crucial to the use of crystal engineering to guide the crystal formation processes in MONTs to targeted structures, properties, and applications.
Our work reports on the detailed molecular dynamic behavior of miscible blends of Poly(3-hexylthiophene) (P3HT) and [6,6]-phenyl-C61-butyric acid methyl ester (PCBM) and their pure counterparts by quasi-elastic neutron scattering measurements (QENS). The study provides the measure of relaxation processes on pico-to-nanosecond time scales. A single relaxation process was observed in pure P3HT and PCBM while two relaxation processes, one fast and one slow, were observed in the blends. The fast process was attributed to the dynamics of P3HT while the slow process was correlated to the dynamics of PCBM. The results show that the relaxation process is a balance between two opposing effects: increased mobility due to thermal activation of P3HT molecules and decrease mobility due to the presence of PCBM which is correlated to the percent crystallinity of P3HT and local packing density of PCBM in the amorphous phase. The threshold for the domination of the thermally activated relaxation is between 5 and 9 vol.% of PCBM loading. Two distinct spatial dependences of the relaxation processes, in which the crossover length scale depends neither on temperature nor composition, were observed for all the samples. They were attributed to the collective motions of the hexyl side chains and the rotational motions of the C-C single bonds of the side chains. Finally, these results provide an understanding of the effects of PCBM loading and temperature on the dynamics of the polymer-fullerene blends which provides a tool to optimize the efficiency of charge carrier and exciton transport within the organic photovoltaic (OPV) active layer to improve the high performance of organic solar cells.
Structured polymers offer a means to tailor transport pathways within mechanically stable manifolds. Here we examine the building block of such a membrane, namely a single large pentablock co-polymer that consist of a center block of a randomly sulfonated polystyrene, designed for transport, tethered to poly-ethylene-r-propylene and end-capped by poly-t-butyl styrene, for mechanical stability,using molecular dynamics simulations. The polymer structure in a cyclohexane-heptane mixture, a technologically viable solvent, and in water, a poor solvent for all segments and a ubiquitous substance is extracted. In all solvents the pentablock collapsed into nearly spherical aggregates where the ionic block is segregated. In hydrophobic solvents, the ionic block resides in the center, surrounded by swollen intermix of flexible and end blocks. In water all blocks are collapsed with the sulfonated block residing on the surface. Our results demonstrate that solvents drive different local nano-segregation, providing a gateway to assemble membranes with controlled topology.
Abstract not provided.
Abstract not provided.