Search NASA⌕ Search

Engineering topics

Ewert, Uwe

Publications and source records attributed to Ewert, Uwe.

X-ray tomographic in-service inspection of girth welds - The European project TomoWELD

The new standard 'ISO 17636-2:2013: Non-destructive testing of welds - Radiographic testing - Part 2: X- and gamma-ray techniques with digital detectors', defines the practice for radiographic inspection of welded pipes for manufacturing and in-service inspection. It is applied in Europe for inspections of pipe welds in nuclear power plants as well as in chemical plants and allows a faster inspection with digital detector arrays (DDA) than with film. Nevertheless, it does not allow the evaluation of the depth and shape of volumetric and planar indications. In 2001 a planar tomography scanner, TomoCAR, was introduced for mechanized radiographic testing (RT) inspection and non-destructive measurement of cross sections. The project TomoWELD is based on a new concept of the scan geometry, an enhanced GPU based reconstruction, and the application of a new generation of photon counting DDAs based on CdTe crystal CMOS hybrids. The new detector permits the selection of energy thresholds to obtain an optimum energy range and reduction of the influence of scattered radiation. The concept and first measurements are presented. Flaw depth and shape of volumetric and planar irregularities can be determined.

36 MATERIALS SCIENCE↗

Observer POD for radiographic testing

The radiographic testing (RT) is a non-destructive testing (NDT) method capable of finding volumetric and open planar defects depending on their orientation. The radiographic contrast is higher for larger penetrated length of the defect in a component. Even though, the detectability of defects does not only depend on the contrast, but also on the noise, the defect area and the geometry of the defect. The currently applied Probability of Detection (POD) approach uses a detection threshold that is only based on a constant noise level or on a constant contrast threshold. This does not reflect accurately the results of evaluations by human observers. A new approach is introduced, using the widely applied POD evaluation and additionally a detection threshold depending on the lateral area and shape of the indication. This work shows the process of calculating the POD curves with simulated data by the modeling software aRTist and with artificial reference data of different defect types, such as ASTM E 476 EPS plates, flat bottom holes and notches. Additional experiments with different operators confirm that the depth of a defect, the lateral area and shape of its indication contribute with different weight to the detectability of the defect if evaluated by human operators on monitors.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Measuring microfocal spots using digital radiography

Measurement of microfocus spot size can be important for several reasons: (1) Quality assurance during manufacture of microfocus tubes; (2) Tracking performance and stability of microfocus tubes; (3) Determining magnification is especially important for digital radiography where the native spatial resolution of the digital system is not adequate for the application; and (4) Knowledge of unsharpness from the focal spot alone. The European Standard EN 12543-5 is based on a simple geometrical method of calculating focal spot size from unsharpness of high magnification film radiographs. The following equations are used for the focal spot size measurement: By similar triangles the following equations are presupposed: f/a = U/b and M = (a+b)/a. These equations can be combined to yield the well known expression: U = f(M - 1). Solving for f, f = U/(M-1). Therefore, the focal spot size, f, can be calculated by measuring the radiographic unsharpness and magnification of a known object. This is the basis for these tests. The European standard actually uses one-half of the unsharpness (which are then added together) from both sides of the object to avoid additional unsharpness contributions due to edge transmission unsharpness of the round test object (the outside of the object is measured). So the equation becomes f = (1/2 U{sub 1} + 1/2 U{sub 2})/(M-1). In practice 1/2 U is measured from the 50% to the 90% signal points on the transition profile from ''black'' to ''white,'' (positive image) or attenuated to unattenuated portion of the image. The 50% to 90% points are chosen as a best fit to an assumed Gaussian radiation distribution from the focal spot and to avoid edge transmission effects. 1/2 U{sub 1} + 1/2 U{sub 2} corresponds about to the full width at half height of a Gaussian focal spot. A highly absorbing material (Tungsten, Tungsten Alloy, or Platinum) is used for the object. Either wires or a sphere are used as the object to eliminate alignment issues. One possibility is to use the wires in the ASTM E2002 unsharpness gage and take two orthogonal images. The signal levels in the image need to be linear with radiation exposure and so may need conversion if a nonlinear detector is used to acquire the image.

47 OTHER INSTRUMENTATION↗