Lateral cracks during sliding indentation on various optical materials

A series of static and sliding indentation (ie, scratching) was performed and characterized on a wide range of optical workpiece materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 –Al 2 O 3 –P 2 O 5 –Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 –Al 2 O 3 –K 2 O–BaO (Phosphate)] at various applied loads using various indenters (Vickers, 10 µm conical, and 200 µm conical). Despite having different load dependencies, the lateral crack depth formed during sliding indentation quantitatively scales with that formed during static indentation, explaining why static indentation has been historically effective in describing various grinding parameters. Depending on the indenter geometry, the amount of residual trench damage (plastic deformation and local fracturing) during sliding indentation was often enhanced by more than an order of magnitude compared with static indentation. A simple ploughing scratch model, which considers both tangential and normal stresses (where the tangential stress is amplified by relatively small tangential contact area), explains this enhancement and other observed trends. Accounting for the high correlation between residual trench depth and volumetric fracturing, the model is extended to estimate the amount of fracture damage as a function of the material properties of the workpiece, indenter geometry, and applied load. Such a model has utility in the design of optimized grinding processes, particularly the abrasive geometry. Finally, at higher loads (>1 N), lateral cracks were often observed to preferentially propagate in the forward scratching direction, as opposed to perpendicular to the scratch as typically observed. High-speed imaging of the scratch process confirms that these cracks propagate ahead of the sliding indenter during the scratching event. Finite element stress analysis suggests the ploughing frictional forces increase the mode I tensile stresses at the leading edge of the sliding indenter explaining the direction of crack propagation of such cracks.

36 MATERIALS SCIENCE↗

Polishing slurry preventing agglomeration of charged colloids without loss of surface activity

A method for chemically stabilizing polishing slurries in aqueous suspension to prevent their agglomeration while maintaining their surface activity is disclosed. The method prevents the formation of irreversible particle agglomerates during drying and permits the subsequent re-suspension of dried particles with no impact on the particle size distribution. The stabilization method can be customized based on knowledge of the colloid surface charge at suspension pH conditions, addition of a charged species having like charge to the colloid at the suspension conditions, and control of the concentrations of the charged species and other ions in suspension.

Dylia-Spears, Rebecca↗

Towards predicting removal rate and surface roughness during grinding of optical materials

A series of controlled grinding experiments, utilizing loose or fixed abrasives of either alumina or diamond at various particle sizes, were performed on a wide range of optical workpiece materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 -Al 2 O 3 -P 2 O 5 -Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 -Al 2 O 3 -K 2 O-BaO (Phosphate)]. The material removal rate, surface roughness, and the morphology of surface fractures were measured. Separately, Vickers indentation was performed on the workpieces, and the depths of various crack types as a function of applied load was measured. Single pass grinding experiments showed distinct differences in the spatial pattern of surface fracturing between the loose alumina abrasive (isolated indent-type lateral cracking) and the loose or fixed diamond abrasive (scratch-type elongated lateral cracking). Each of the grinding methods had a removal rate and roughness that scaled with the lateral crack slope, sℓ (i.e. the rate of increase in lateral crack depth with the applied load) of the workpiece material. A grinding model (based on the volumetric removal of lateral cracks accounting for neighboring lateral crack removal efficiency and the fraction of abrasive particles leading to fracture initiation) and a roughness model (based on the depth of lateral cracks or the interface gap between the workpiece and lap) are shown to quantitatively describe the material removal rate and roughness as a function of workpiece material, abrasive size, applied pressure and relative velocity. This broad, multi-process variable grinding model can serve as a predictive tool for estimating grinding rates and surface roughness for various grinding processes on different workpiece materials

36 MATERIALS SCIENCE↗

Influence of partial charge on the material removal rate during chemical polishing

A partial charge-based chemical polishing model has been developed, which can serve as metric for describing the relative polishing material removal rate for different combinations of slurries and workpieces. A series of controlled polishing experiments utilizing a variety of colloidal polishing slurries (SiO 2 , CeO 2 , ZrO 2 , MgO, Sb 2 O 5 ) and optical materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 -Al 2 O 3 -P 2 O 5 -Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 -Al 2 O 3 -K 2 O-BaO (Phosphate)] was performed and its material removal rate was measured. As previously proposed by Cook (J Non-Cryst Solids. 1990;120:152), for many polishing systems, the removal rate is governed by a series of chemical reactions which include the formation of a surface hydroxide, followed by condensation of that hydroxyl moiety with the polishing particle, and a subsequent hydrolysis reaction. The rate of condensation can often be the rate limiting step, thus it can determine the polishing material removal rate. By largely keeping the numerous other factors that influence material removal rate fixed (such as due to particle size distributions, interface interactions, pad topography, kinematics, and applied pressure), the material removal rate is shown to scale exponentially with the partial charge difference (δ wp-s ) between the workpiece and polishing slurry particle for many of the slurry-workpiece combinations indicating that condensation rate is the rate limiting step. The partial charge (δ) describes the equilibrium distribution of electron density between chemically bonded atoms and is related to the electronegativity of the atoms chemically bonded to one another. This partial charge model also explains the age-old experimental finding of why cerium oxide is the most effective polishing slurry for chemical removal of many workpieces. Finally, some of the slurry-workpiece combinations that did not follow the partial charge dependence offer insight to other removal mechanisms or rate limiting reaction pathways.

36 MATERIALS SCIENCE↗

Relationship between surface μ‐roughness and interface slurry particle spatial distribution during glass polishing

Abstract During optical glass polishing, a number of interactions between the workpiece (i.e., glass), polishing slurry, and pad can influence the resulting workpiece roughness at different spatial scale lengths. In our previous studies, the particle size distribution of the slurry, the pad topography, and the amount of material removed by a single particle on the workpiece were shown to strongly correlate with roughness at AFM scale lengths (nm‐μm) and weakly at μ‐roughness scale lengths (μm‐mm). In this study, the polishing slurry pH and the generation of glass removal products are shown to influence the slurry particle spatial and height distribution at the polishing interface and the resulting μ‐roughness of the glass workpiece. A series of fused silica and phosphate glass samples were polished with various ceria and colloidal silica slurries over a range of slurry pH , and the resulting AFM roughness and μ‐roughness were measured. The AFM roughness was largely invariant with pH , suggesting that the removal function of a single particle is unchanged with pH . However, the μ‐roughness changed significantly, increasing linearly with pH for phosphate glass and having a maximum at an intermediate pH for fused silica. In addition, the spatial and height distribution of slurry particles on the pad (as measured by laser confocal microscopy) was determined to be distinctly different at low and high pH during phosphate glass polishing. Also, the zeta potential as a function of pH was measured for the workpiece, slurry, and pad with and without surrogate glass products (K 3 PO 4 for phosphate glass and Si( OH ) 4 for silica) to assess the role of interfacial charge during polishing. The addition of K 3 PO 4 significantly raised the zeta potential, whereas addition of Si( OH ) 4 had little effect on the zeta potential. An electrostatic DLVO three‐body force model, using the measured zeta potentials, was used to calculate the particle–particle, particle–workpiece, and particle–pad attractive and repulsive forces as a function of pH and the incorporation of glass products at the interface. The model predicted an increase in particle–pad attraction with an increase in pH and phosphate glass products consistent with the measured slurry distribution on the pads during phosphate glass polishing. Finally, a slurry “island” distribution gap ( IDG ) model has been formulated which utilizes the measured interface slurry distributions and a load balance to determine the interface gap, the contact area fraction, and the load on each slurry “island”. The IDG model was then used to simulate the workpiece surface topography and μ‐roughness; the results show an increase in roughness with pH similar to that observed experimentally.

Suratwala, Tayyab↗