Final inspection of foils 3K32-N8-XL8V-F1 and 3K32-N8-XL8V-F2 [Slides]
Abstract not provided.
Engineering topics
Publications and source records attributed to Forsyth, Robert Thomas.
Abstract not provided.
Microwave-cast material dating from the latest prototype development period and subsequent TRL 7 advancement testing was sent to LANL for additional characterization. The initial characterization described here is considered a supplement to and verification of that performed by Y-12 during the Technology Readiness Assessment process. The carbon chemistry results from Y-12 and LANL regarding early prototype microwave cast test object (CTO) and cylinder castings match within expectations. Only one fully intact as-cast CTO was available for examination in which carbon chemistry does not appear to vary spatially, at least at relatively low carbon levels (hypoeutectic). The large as-cast grain size leads to relatively poor grain size statistics and similar difficulties were encountered during the TRA. Small, isolated gas pores were observed in four of the five metallographic samples in prototype CTO casting PT-01. Finally, the next phase of characterization work, which focuses on corrosion behavior, has started and is described briefly.
Herein we report a high density MgO ceramic substrate produced by the tape casting technology. The tape casting formulation and process produced a uniform tape free of cracking. Y 2 O 3 and SiO 2 were used as the sintering aid for the pressureless sintering of the green tape. X-ray diffraction phase identification indicates that MgO is the main phase, while both Y 2 O 3 and SiO 2 sintering aids react with MgO to form MgY 4 Si 3 O 13 as the second phase. Liquid phase sintering occurs in the temperature range from 1030°C to ~1500°C, which is confirmed by the simultaneous Thermal Gravitation Analysis/ Differential Scanning Calorimeter (TGA/DSC) and the percent linear shrinkage and densification. A 96.5% theoretical density was achieved by presureless sintering at 1650°C for 2 hours, which was further increased to a fully dense structure using hotisostatic- pressing(HIP) at 1650°C and 207 MPa in argon. Scanning electron microscopy (SEM) and energy dispersive(EDS) spectroscopic analysis on the HIP’ed sample show that MgY 4 Si 3 O 13 is located at the MgO grain boundary and the sample has a fully dense structure. The refractive indices and extinction coefficient were measured on the HIP’ed sample along with thermal properties and dielectric properties. Thermal diffusivity and heat capacity were measured to calculate the thermal conductivity.
On 2 April 2018, a high explosive violent reaction (HEVR) occurred during routine pressing of a 1-in -diameter cylindrical pellet of PBX 9501 high explosive. Fragments of the die set (die body and stemples) involved in the event were sent to Sigma Division for metallurgical analysis. A handheld x-ray fluorescence alloy tester confirmed the die set material to be A2 tool steel. Light optical microscopy revealed what appear to be pre-existing flaws on the inner diameter of the die body. Scanning Electron Microscopy could neither confirm nor exclude the presence of fatigue cracking in the vicinity of these potential flaws. Energy Dispersive Spectroscopy indicated the presence of a carbon-bearing residue on fracture surfaces; nitrogen-bearing residue was also found. Optical microscopy revealed that the microstructure of the stemple and inner diameter of the die body contained large stringers and non-uniform grain size; this was distinct from the relatively clean and uniform microstructure seen at the outer diameter of the die body, and also other A2 tool steel stock (pedigree unknown and with no known connection to any HE pressing hardware) that was examined for additional comparison. Rockwell hardness testing indicated the material was heat treated properly. Metallographic analysis alone could not positively identify the root cause of the event, but, coupled with accounts provided by the operator and the successful history with the particular lot of HE involved in the event, points to ward mechanical failure of the die set due to pre -existing flaw as the most likely precipitating event. Suggestions for additional analyses and future qualification techniques are discussed.
Metallographic characterization was performed on wrought depleted uranium (DU) samples taken from the longitudinal and transverse orientations from specific locations on two specimens. Characterization of the samples included general microstructure, inclusion analysis, grain size analysis, and microhardness testing. Comparisons of the characterization results were made to determine any differences based on specimen, sample orientation, or sample location. In addition, the characterization results for the wrought DU samples were also compared with data obtained from the metallographic characterization of cast DU samples previously characterized. No differences were observed in microstructure, inclusion size, morphology, and distribution, or grain size in regard to specimen, location, or orientation for the wrought depleted uranium samples. However, a small difference was observed in average hardness with regard to orientation at the same locations within the same specimen. The longitudinal samples were slightly harder than the transverse samples from the same location of the same specimen. This was true for both wrought DU specimens. Comparing the wrought DU sample data with the previously characterized cast DU sample data, distinct differences in microstructure, inclusion size, morphology and distribution, grain size, and microhardness were observed. As expected, the microstructure of the wrought DU samples consisted of small recrystallized grains which were uniform, randomly oriented, and equiaxed with minimal twinning observed in only a few grains. In contrast, the cast DU microstructure consisted of large irregularly shaped grains with extensive twinning observed in most grains. Inclusions in the wrought DU samples were elongated, broken and cracked and light and dark phases were observed in some inclusions. The mean inclusion area percentage for the wrought DU samples ranged from 0.08% to 0.34% and the average density from all wrought DU samples was 1.62E+04/cm 2 . Inclusions in the cast DU samples were equiaxed and intact with light and dark phases observed in some inclusions. The mean inclusion area percentage for the cast DU samples ranged from 0.93% to 1.00% and the average density from all wrought DU samples was 2.83E+04/cm 2 . The average mean grain area from all wrought DU samples was 141 μm 2 while the average mean grain area from all cast DU samples was 1.7 mm2. The average Knoop microhardness from all wrought DU samples was 215 HK and the average Knoop microhardness from all cast DU samples was 264 HK.
Chloride-induced stress corrosion cracking (SCC) has been investigated as a potential failure mechanism for the SAVY 4000 and the Hagan containers used to store plutonium-bearing materials at Los Alamos National Laboratory. This report discusses the regions of the container bodies most susceptible to SCC and the magnitude of the residual stresses in those regions. Boiling MgCl2 testing indicated that for both containers the region near the top weld was most susceptible to SCC. The Hagan showed through wall cracking after 22-24 hours of exposure both parallel (axial stresses) and perpendicular (hoop stresses) to the weld. The SAVY 4000 container showed significant cracking above and below the weld after 47 hours of exposure but there was no visual evidence of a through wall crack and the cracks did not leak water. Two through wall holes formed in the bottom of the SAVY 4000 container after 44-46 hours of exposure. For both containers, average “through wall” residual stresses were determined from hole drilling data 4 mm below the weld. In the Hagan body, average tensile hoop stresses were 194 MPa and average compressive axial stresses were -120 MPa. In the SAVY 4000 body, average compressive hoop stresses were 11 MPa and average tensile axial stresses were 25 MPa. Results suggest that because the Hagan container exhibited through wall cracking in a shorter time in boiling MgCl2 and had the higher average tensile stress, 194 MPa hoop stress, it is more susceptible to SCC than the SAVY 4000 container.
Complicating factors that have stymied understanding of uranium-niobium’s aging response are briefly reviewed, including (1) niobium inhomogeneity, (2) machining damage effects on tensile properties, (3) early-time transients of ductility increase, and (4) the variety of phase transformations. A simple Logistic-Arrhenius model was applied to predict yield and ultimate tensile strengths and tensile elongation of U-4Nb as a function of thermal age. Lastly, fits to each model yielded an apparent activation energy that was compared with phase transformation mechanisms.
U-10 wt. % Mo (U-10Mo) alloys are being developed as low enrichment monolithic fuel for the CONVERT program. Optimization of processing for the monolithic fuel is being pursued with the use of electrical discharge machining (EDM) under CONVERT HPRR WBS 1.2.4.5 Optimization of Coupon Preparation. The process is applicable to manufacturing experimental fuel plate specimens for the Mini-Plate-1 (MP-1) irradiation campaign. The benefits of EDM are reduced machining costs, ability to achieve higher tolerances, stress-free, burr-free surfaces eliminating the need for milling, and the ability to machine complex shapes. Kerf losses are much smaller with EDM (tenths of mm) compared to conventional machining (mm). Reliable repeatability is achievable with EDM due to its computer-generated machining programs.