Reversible Losses in Proton Exchange Membrane Water Electrolysis

Lower anode catalyst loadings and higher current densities are essential to lowering the levelized cost of H 2 production via proton exchange membrane water electrolysis (PEMWE). However, these approaches can induce significant durability challenges. Here, we show that cell degradation can include large reversible voltage losses across a variety of conditions, including low loadings and high currents. Although there is limited published discussion of reversible voltage losses in PEMWE, we demonstrate that they are an important consideration in cell efficiency and durability. Understanding the mechanisms of reversible losses and developing mitigation strategies is therefore a key priority for enabling low-cost PEMWE.

08 HYDROGEN↗

Shelf-life of ball-milled catalyst inks for the fabrication of fuel cell electrodes

A major factor driving fuel cell costs is the quantity of precious metal required. Therefore, it is important to understand a timeframe where inks can be reused. Here, in this work, we explore differences between a freshly prepared catalyst ink and one that has been stored for over a year – comparing ink properties, cathode catalyst layer microstructure, and their respective fuel cell performance. Ink studies revealed smaller agglomerate sizes and a decrease in shear viscosity for the aged ink. Longer storage time also results in fewer cracks and a more uniform ionomer distribution, as evidenced by microscopy characterization of rod-coated electrodes. Lastly, polarization curves show improved performance at higher current densities for the electrode prepared from the aged ink. We rationalize such effect in terms of enhanced ionomer adsorption onto the catalyst over time.

08 HYDROGEN↗

X-ray Photoelectron Spectroscopy Analysis of Nafion-Containing Samples: Pitfalls, Protocols, and Perceptions of Physicochemical Properties

X-ray photoelectron spectroscopy (XPS) is one of the most common techniques used to analyze the surface composition of catalysts and support materials used in polymer electrolyte membrane (PEM) fuel cells and electrolyzers, providing important insights for further improvement of their properties. Characterization of catalyst layers (CLs) is more challenging, which can be at least partially attributed to the instability of ionomer materials such as Nafion during measurements. This work explores the stability of Nafion during XPS measurements, illuminating and addressing Nafion degradation concerns. The extent of Nafion damage as a function of XPS instrumentation, measurement conditions, and sample properties was evaluated across multiple instruments. Results revealed that significant Nafion damage to the ion-conducting sulfonic acid species (>50% loss in sulfur signal) may occur in a relatively short time frame (tens of minutes) depending on the exact nature of the sample and XPS instrument. This motivated the development and validation of a multipoint XPS data acquisition protocol that minimizes Nafion damage, resulting in reliable data acquisition by avoiding significant artifacts from Nafion instability. The developed protocol was then used to analyze both thin film ionomer samples and Pt/C-based CLs. Comparison of PEM fuel cell CLs to Nafion thin films revealed several changes in Nafion spectral features attributed to charge transfer due to interaction with conductive catalyst and support species. This study provides a method to reliably characterize ionomer-containing samples, facilitating fundamental studies of the catalyst-ionomer interface and more applied investigations of structure-processing-performance correlations in PEM fuel cell and electrolyzer CLs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Aging gracefully? Investigating iridium oxide ink's impact on microstructure, catalyst/ionomer interface, and PEMWE performance

Here, in this study, we conducted a thorough investigation of the impact of aging iridium oxide (IrO 2 ) perfluorosulfonic acid ionomer ink for up to 14 days on the properties of the ink and the resulting catalyst layers. We examined ink properties, such as zeta potential, dynamic light scattering (DLS), density, surface tension, and rheology, as functions of ink aging time. To evaluate the microstructure and catalyst/ionomer interface, we employed transmission electron microscopy (TEM), X-ray scattering, and X-ray photoelectron spectroscopy (XPS) techniques. Furthermore, we assessed the effect of ink aging on the performance of proton exchange membrane water electrolyzers (PEMWEs). Our findings reveal that most ink properties remain stable for 14 days. The variations in PEMWE cell performance are minimal, and no clear trend is observed in relation to ink aging time. This study demonstrates that the effects of aging the inks for 14 days on ink properties, catalyst layer structure, catalyst/ionomer interface, and PEMWE performance are negligible, indicating a substantial time window after ink preparation without any significant changes in its properties. These insights provide crucial guidance for the commercial production and coating processes of ink, which is necessary for scaling up PEM technologies to meet future demand.

30 DIRECT ENERGY CONVERSION↗