Search NASA⌕ Search

Engineering topics

Gao, Hongcai

Publications and source records attributed to Gao, Hongcai.

Formation of Stable Interphase of Polymer-in-Salt Electrolyte in All-Solid-State Lithium Batteries

The integration of solid-polymer electrolytes into all-solid-state lithium batteries is highly desirable to overcome the limitations of current battery configurations that have a low energy density and severe safety concerns. Polyacrylonitrile is an appealing matrix for solid-polymer electrolytes; however, the practical utilization of such polymer electrolytes in all-solid-state cells is impeded by inferior ionic conductivity and instability against a lithium-metal anode. In this work, we show that a polymer-in-salt electrolyte based on polyacrylonitrile with a lithium salt as the major component exhibits a wide electrochemically stable window, a high ionic conductivity, and an increased lithium-ion transference number. The growth of dendrites from the lithium-metal anode was suppressed effectively by the polymer-in-salt electrolyte to increase the safety features of the batteries. In addition, we found that a stable interphase was formed between the lithium-metal anode and the polymer-in-salt electrolyte to restrain the uncontrolled parasitic reactions, and we demonstrated an all-solid-state battery configuration with a LiFePO 4 cathode and the polymer-in-salt electrolyte, which exhibited a superior cycling stability and rate capability.

Gao, Hongcai↗

Na 3 MnZr(PO 4 ) 3 : A High-Voltage Cathode for Sodium Batteries

Sodium batteries have been regarded as promising candidates for large-scale energy storage application, provided cathode hosts with high energy density and long cycle life can be found. Herein, we report NASICON-structured Na 3 MnZr(PO 4 ) 3 as a cathode for sodium batteries that exhibits an electrochemical performance superior to those of other manganese phosphate cathodes reported in the literature. Both the Mn 4+ /Mn 3+ and Mn 3+ /Mn 2+ redox couples are reversibly accessed in Na 3 MnZr(PO 4 ) 3 , providing high discharge voltage plateaus at 4.0 and 3.5 V, respectively. A high discharge capacity of 105 mAh g –1 was obtained from Na 3 MnZr(PO 4 ) 3 with a small variation of lattice parameters and a small volume change on extraction of two Na + ions per formula unit. Moreover, Na 3 MnZr(PO 4 ) 3 exhibits an excellent cycling stability, retaining 91% of the initial capacity after 500 charge/discharge cycles at 0.5 C rate. On the basis of structural analysis and density functional theory calculations, we have proposed a detailed desodiation pathway from Na 3 MnZr(PO 4 ) 3 where Mn and Zr are disordered within the structure. We further show that the cooperative Jahn–Teller distortion of Mn 3+ is suppressed in the cathode and that Na 2 MnZr(PO 4 ) 3 is a stable phase

Chemistry↗

Room‐Temperature Liquid Na–K Anode Membranes

Abstract The Na–K alloy is a liquid at 25 °C over a large compositional range. The liquid alloy is also immiscible in the organic‐liquid electrolytes of an alkali‐ion rechargeable battery, providing dendrite‐free liquid alkali‐metal batteries with a liquid–liquid anode‐electrolyte interface at room temperature. The two liquids are each immobilized in a porous matrix. In previous work, the porous matrix used to immobilize the alloy was a carbon paper that is wet by the alloy at 420 °C; the alloy remains in the paper at room temperature. Here we report a room‐temperature vacuum infiltration of the alloy into a porous Cu or Al membrane and a reversible stripping/plating of the liquid alloy with the immobilized organic‐liquid electrolyte; no self‐diacharge is observed since the liquid Na–K does not dissolve into the liquid carbonate electrolytes. The preparation and stripping/plating of the liquid alkali‐metal anode can both now be done safely at room temperature.

Xue, Leigang↗

A High‐Energy‐Density Potassium Battery with a Polymer‐Gel Electrolyte and a Polyaniline Cathode

Abstract A safe, rechargeable potassium battery of high energy density and excellent cycling stability has been developed. The anion component of the electrolyte salt is inserted into a polyaniline cathode upon charging and extracted from it during discharging while the K + ion of the KPF 6 salt is plated/stripped on the potassium‐metal anode. The use of a p‐type polymer cathode increases the cell voltage. By replacing the organic‐liquid electrolyte in a glass‐fiber separator with a polymer‐gel electrolyte of cross‐linked poly(methyl methacrylate), a dendrite‐free potassium anode can be plated/stripped, and the electrode/electrolyte interface is stabilized. The potassium anode wets the polymer, and the cross‐linked architecture provides small pores of adjustable sizes to stabilize a solid‐electrolyte interphase formed at the anode/electrolyte interface. This alternative electrolyte/cathode strategy offers a promising new approach to low‐cost potassium batteries for the stationary storage of electric power.

Gao, Hongcai↗

A Plastic–Crystal Electrolyte Interphase for All‐Solid‐State Sodium Batteries

Abstract The development of all‐solid‐state rechargeable batteries is plagued by a large interfacial resistance between a solid cathode and a solid electrolyte that increases with each charge–discharge cycle. The introduction of a plastic–crystal electrolyte interphase between a solid electrolyte and solid cathode particles reduces the interfacial resistance, increases the cycle life, and allows a high rate performance. Comparison of solid‐state sodium cells with 1) solid electrolyte Na 3 Zr 2 (Si 2 PO 4 ) particles versus 2) plastic–crystal electrolyte in the cathode composites shows that the former suffers from a huge irreversible capacity loss on cycling whereas the latter exhibits a dramatically improved electrochemical performance with retention of capacity for over 100 cycles and cycling at 5 C rate. The application of a plastic–crystal electrolyte interphase between a solid electrolyte and a solid cathode may be extended to other all‐solid‐state battery cells.

Gao, Hongcai↗

A Plastic-Crystal Electrolyte Interphase for All-Solid-State Sodium Batteries

The development of all-solid-state rechargeable batteries is plagued by a large interfacial resistance between a solid cathode and a solid electrolyte that increases with each charge–discharge cycle. The introduction of a plastic–crystal electrolyte interphase between a solid electrolyte and solid cathode particles reduces the interfacial resistance, increases the cycle life, and allows a high rate performance. In this work, comparison of solid-state sodium cells with 1) solid electrolyte Na 3 Zr 2 (Si 2 PO 4 ) particles versus 2) plastic–crystal electrolyte in the cathode composites shows that the former suffers from a huge irreversible capacity loss on cycling whereas the latter exhibits a dramatically improved electrochemical performance with retention of capacity for over 100 cycles and cycling at 5 C rate. The application of a plastic–crystal electrolyte interphase between a solid electrolyte and a solid cathode may be extended to other all-solid-state battery cells.

25 ENERGY STORAGE↗

Low-Cost High-Energy Potassium Cathode

Potassium has as rich an abundance as sodium in the earth, but the development of a K-ion battery is lagging behind because of the higher mass and larger ionic size of K + than that of Li + and Na + , which makes it difficult to identify a high-voltage and high-capacity intercalation cathode host. Here we propose a cyanoperovskite K x MnFe(CN) 6 (0 ≤ x ≤ 2) as a potassium cathode: high-spin Mn III /Mn II and low-spin Fe III /Fe II couples have similar energies and exhibit two close plateaus centered at 3.6 V; two active K + per formula unit enable a theoretical specific capacity of 156 mAh g -1 ; Mn and Fe are the two most-desired transition metals for electrodes because they are cheap and environmental friendly. As a powder prepared by an inexpensive precipitation method, the cathode delivers a specific capacity of 142 mAh g -1 . Lastly, the observed voltage, capacity, and its low cost make it competitive in large-scale electricity storage applications.

25 ENERGY STORAGE↗

An Aqueous Symmetric Sodium-Ion Battery with NASICON-Structured Na 3 MnTi(PO 4 ) 3

A symmetric sodium-ion battery with an aqueous electrolyte is demonstrated; it utilizes the NASICON-structured Na 3 MnTi(PO 4 ) 3 as both the anode and the cathode. The NASICON-structured Na 3 MnTi(PO 4 ) 3 possesses two electrochemically active transition metals with the redox couples of Ti 4+ /Ti 3+ and Mn 3+ /Mn 2+ working on the anode and cathode sides, respectively. The symmetric cell based on this bipolar electrode material exhibits a well-defined voltage plateau centered at about 1.4 V in an aqueous electrolyte with a stable cycle performance and superior rate capability. The advent of aqueous symmetric sodium-ion battery with high safety and low cost may provide a solution for large-scale stationary energy storage.

25 ENERGY STORAGE↗