Search NASA⌕ Search

Engineering topics

Garg, Anita

Publications and source records attributed to Garg, Anita.

At least 19 records

Durability of YSZ Coated Ti2AlC in 1300 °C Mach 0.3 Burner Rig Tests

A thermal barrier coating system survived burner rig testing at 1300 °C for 500 h. A 160 µm thick yttria stabilized zirconia (YSZ) coating was applied to a Ti2AlC MAX phase bar sample by plasma spray physical vapor deposition (PS-PVD) and tested face-on in an atmospheric Mach 0.3 jet fuel burner, using 5-h thermal cycles. No thermal barrier coating (TBC) spallation or recession was observed, only a 2.4 mg/cm2 mass gain. The modest weight gain precluded severe volatility losses under high velocity burner conditions. The coating surface exhibited colonies of (111)flourite fiber-textured columns separated by craze patterns, with no visible moisture attack. The metastable tetragonal t' YSZ phase was obtained initially, transitioning to equilibrium teq and cubic YSZ, but with little detrimental monoclinic. The thickness of the alumina TGO was ~21 to 23 μm under the heated YSZ face and ~13 to 15 μm on the uncoated, cooler backside. The backside exhibited removal of initial transient TiO2 nodules and partial etching of the underlying Al2O3 scale by volatile hydroxides formed in high temperature, high velocity water vapor. Aerodynamic forces produced some bending of the cantilevered sample via creep. The test indicated exceptional stability of YSZ coatings on Ti2AlC under turbine conditions, with thermal expansion matching playing a key role. The purpose of this study was to demonstrate long term durability of YSZ/MAX phase system in aggressive high temperature burner rig testing. MAX phases have been keenly studied because of their unique crystal structure and intriguing properties (Refs. 1 and 2). Having Mn+1(Al,Si)(C,N)n general composition, they are defined as ceramics, but possess unusual desirable attributes such as high conductivity, thermal shock resistance, easy machinability, and deformation tolerance. The mechanical properties derive from weak M-(Al,Si) bonding in the basal plane that leads to sliding and kinking in preference to catastrophic crack growth. Like most ceramics they are phase stable at high temperatures, generally up to 1500 °C. High temperature oxidation resistance is excellent for alumina-forming Ti3AlC2, Ti2AlC, and Cr2AlC, as reviewed by Tallman, et al. (Ref. 3). Compatibility with α-Al2O3 scales is further enhanced in cyclic exposures by a close matching of thermal expansion coefficients, (Ref. 4) i.e., (~9.3, 10.2, 11.3×10–6/K for Al2O3, Ti2AlC, and YSZ, to be discussed). Turbine environments generally contain 10 percent water vapor in the combustion gases, therefore moisture effects can be a concern for some materials (Ref. 5). Furnace tests of MAX phases in high temperature steam generally showed little effect on Al2O3 scale growth (Ref. 6). However, high velocity and high pressure gas can influence scale losses by the formation of volatile reaction products, such as TiO(OH)2 and Al(OH)3 (Refs. 7 to 10). This phenomenon had been discussed for 1100 to 1300 °C high pressure burner rig tests of Ti2AlC (Ref. 11). A single cubic growth rate parameter kcubic was measurably lower than comparable furnace TGA data, but it could be matched reasonably well if corrected for a slight volatility term. In general, a two-parameter cubic-linear growth-volatility law was believed to apply. Corresponding scale volatility loss rates, directly measured at 1300 °C on a pre-oxidized sample, were moderate (0.012 mg/cm2/h) and largely attributed to removal of the initial TiO2 transient scale. A related CH4 burner study of high purity Cr2AlC MAX phase demonstrated 1200 °C durability after 500 rapid (5 min. heat and 2 min. cool) thermal shock cycling (29 h hot time) (Ref. 12). Heating and cooling rates were ~1000 and 500 °C per minute, with a gas velocity of 5 m/s, producing a 75 °C/mm gradient. A 7 μm Al2O3 surface scale and a 13 μm Cr7C3 depletion zone formed with no signs of failure. No evidence of scale volatility was evident, although weight change was not provided, the velocity was moderate, and the total hot time was not extensive. The same high gradient BRT was used to produce 1400 °C surface temperatures for a YSZ/Cr2AlC/IN738 system in the first study of MAX phases used as bond coats for thermal barrier coatings (TBC) (Ref. 25). Here TBC failure was reported after 745 cycles, with only a 1.5 μm Al2O3 scale entrained within a porous, Cr7C3 bondcoat depletion phase. YSZ thermal barrier coatings have been considered to be a compatible complement to Al-MAX phases because of thermal expansion matching and extremely low volatility in water vapor. Initial studies showed superior oxidative stability up to 1300 °C, for long times (at least 500 h) for Ti2AlC substrates and less (268 h) for Cr2AlC, while withstanding large alumina TGO scale thickness (~35 to 40 μm) (Refs. 13 and 14). By comparison, typical superalloy systems can only survive 1150 °C maximum interface temperatures for extended periods, with a maximum sustained TGO below 10 μm (Ref. 15). High temperature SiC based systems are known to form slow-growing SiO2 scales. But these are subject to rate enhancement and volatile Si(OH)4 products in the presence of water vapor, as described comprehensively by Opila, et al. (Refs. 5, 16 to 19). Net weight losses are generally observed in high velocity, high pressure burner rig studies (e.g., 0.084 mg/cm2/h at 1300 °C) (Ref. 20). Furthermore, the loss rates have been shown from chemical physics to scale with v1/2 and pH2O 2 (Ref. 16). Low activity, moisture-resistant environmental barrier coatings (EBC), such as rare earth silicates, are needed to prevent substrate recession under turbine conditions (Refs. 21 to 23).

Smialek, James L.↗

Investigation of Alpha Silicon Carbide / Carbon Fiber Proposed (2H & 6H-SiC) / C

A commercially available alpha silicon carbide coated carbon 12k fiber tow was subjected to rigorous inspection and testing. The pyrolized polyacrylonitrile (PAN) fiber had gone through a conversion process that resulted in a thin layer of SiC forming on the exterior of the fiber. The fibers? surface was characterized by x-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES) and scanning electron microscopy (SEM). Powdered x-ray diffraction (XRD) examined the bulk material properties. Transmission electron microscopy (TEM) coupled with energy-dispersive X-ray spectroscopy (EDS) examined the crystallinity of the SiC. A number of pristine samples were used to determine elongation rate and tensile strength.

Trunek, Andrew↗

Precipitation Strengthenable NiTiPd High Temperature Shape Memory Alloys

In binary NiTi alloys, it has long been known that Ni-rich alloys can be heat treated to produce precipitates which both strengthen the matrix against dislocations and improve the behavior of the material under thermal and mechanical cycling. Within recent years, the same effect has been observed in Ni-rich NiTiHf high temperature shape memory alloys and heat treatment regimens have been defined which will reliably produce improved properties. In NiTiPd alloys, precipitation has also been observed, but studies are still underway to define reliable heat treatments and compositions which will provide a balance of strengthening and good thermomechanical properties. For this study, a series of NiTi-32 at.Pd alloys was produced to determine the effect of changing nickeltitanium content on the transformation behavior and heat treatability of the material. Samples were aged at temperatures between 350C and 450C for times up to 100 hours. Actuation type behavior was evaluated using uniaxial constant force thermal cycling (UCFTC) to determine the effect of composition and aging on the material behavior. TEMSEM was used to evaluate the microstructure and determine the types of precipitates formed. The correlation between composition, heat treat, microstructure, and thermomechanical behavior will be addressed and discussed.

Transformation strain↗

Oxidation of Alumina-Forming MAX Phases in Turbine Environments

Protective coatings for high temperature turbine components are based on YSZ thermal barriers and oxidation resistant, alumina-forming NiAl or NiCoCrAlY bond coats. Ti2AlC and Cr2AlC MAX phases are thus of special interest because of good oxidation resistance and CTE that can match Al2O3 and YSZ. Their alumina scales grow according to cubic kinetics due to grain growth in the scale, with initial heating dominated by fast TiO2 growth. Protective cubic kinetics are also found in high pressure burner rig tests of MAXthal 211 Ti2AlC, but with reduced rates due to volatile TiO(OH)2 formation in water vapor. YSZ-coatings on bulk Ti2AlC exhibit remarkable durability up to 1300C in furnace tests and at least a 25x life advantage compared to superalloys. At another extreme, Cr2AlC is resistant to low temperature Na2SO4 hot corrosion and exhibits thermal cycling stability bonded to a superalloy disk material. Accordingly, sputtered Cr2AlC coatings on disk specimens prevented hot corrosion detriments on LCF. Breakaway oxidation (Ti2AlC), scale spallation (Cr2AlC), interdiffusion, and processing as coatings still present serious challenges. However the basic properties of MAX phases provide some unusual opportunities for use in high temperature turbines.

ceramics↗

Materials Characterization of Electron Beam Melted Ti-6Al-4V

An in-depth material characterization of Electron Beam Melted (EBM) Ti-6Al-4V material has been completed on samples fabricated on an ARCAM A2X EBM machine. The specimens were fabricated under eight separate builds with the material divided into two lots for material testing purposes. Hot Isostatic Pressing (HIP) was utilized to close porosity from fabrication and also served as a material heat treatment to obtain the desired microstructure. The changes in the microstructure and chemistry from the powder to pre-HIP and post-HIP material have been analyzed. Several nondestructive evaluation (NDE) techniques were utilized to characterize the samples both before and after HIP. The test matrix included tensile, high cycle fatigue, low cycle fatigue, fracture toughness, and fatigue crack growth at cryogenic, room, and elevated temperatures. The mechanical properties of the EBM Ti-6Al-4V are compared to conventional Ti-6Al-4V in the annealed condition. Fractography was performed to determine failure initiation site. The EBM Ti-6Al-4V had similar or superior mechanical properties compared to conventionally manufactured Ti-6Al-4V.

Titanium↗

Extreme Oxidative Durability of TBCs on Ti2AlC MAX Phases

APS and PS-PVD YSZ thermal barrier coatings, applied directly to oxidation resistant Ti2AlC substrates, were oxidized in interrupted furnace tests. Temperature was advanced in 50C intervals from 1100 to 1300C, each 500 h long with eleven cooling cycles. Damage only initiated on the APS coating at 1300C after 15 h, with complete delamination after 500 h. The PS-PVD coating survived all testing. Weight change and metallographic analyses indicate that the YSZ-Ti2AlC systems sustained alumina scale growth of 30-40 m. In comparison, widely used Pt-aluminide bondcoats on single crystal superalloy turbine blades exhibit TBC lives equivalent to alumina scale growth up to 7 m, equivalent to just 200 h at 1200C. It is demonstrated that 25x TBC life improvement (or 180C temperature increase) resulted from the close CTE match of Ti2AlC with those of alumina and YSZ.

protective coating↗

Materials Characterization of Electron Beam Melted Ti-6Al-4V

An in-depth material characterization of Electron Beam Melted (EBM) Ti-6Al-4V material has been completed. Hot Isostatic Pressing (HIP) was utilized to close porosity from fabrication and also served as a material heat treatment to obtain the desired microstructure. The changes in the microstructure and chemistry from the powder to pre-HIP and post-HIP material have been analyzed. Computed tomography (CT) scans indicated porosity closure during HIP and high-density inclusions scattered throughout the specimens. The results of tensile and high cycle fatigue (HCF) testing are compared to conventional Ti-6Al-4V. The EBM Ti-6Al-4V had similar or superior mechanical properties compared to conventionally manufactured Ti-6Al-4V.

Titanium↗

Microstructure and Oxidation of a MAX Phase/Superalloy Hybrid Interface

Corrosion resistant, strain tolerant MAX phase coatings are of interest for turbine applications. Thin Cr2AlC MAX phase wafers were vacuum diffusion bonded to an advanced turbine disk alloy, LSHR, at 1100 C. The interface, examined by optical and scanning electron microscopy, revealed a primary diffusion zone consisting of ~ 10 micrometers of beta-Ni(Co)Al, decorated with various NiCoCrAl, MC and M3B2 precipitates. On the Cr2AlC side, an additional ~40 micrometers Al-depletion zone of Cr7C3 formed in an interconnected network with the beta-Ni(Co)Al. Oxidation of an exposed edge at 800 C for 100 h produced a fine-grained lenticular alumina scale over Cr2AlC and beta-Ni(Co)Al, with coarser chromia granules over the Cr7C3 regions. Subsequent growth of the diffusion layers was only ~ 5 micrometers in total. A residual stress of ~ 500 MPa was estimated for the MAX phase layer, but no interfacial damage was observed. Subsequent tests for 1000 h reveal similar results.

heat resistant alloys↗

Macroscopic and Microstructural Aspects of the Transformation Behavior in a Polycrystalline NiTi Shape Memory Alloy

The mechanical and microstructural behavior of a polycrystalline Ni(49.9)Ti(50.1) (at.%) shape memory alloy was investigated as a function of temperature around the transformation regime. The bulk macroscopic responses, measured using ex situ tensile deformation and impulse excitation tests, were compared to the microstructural evolution captured using in situ neutron diffraction. The onset stress for inelastic deformation and dynamic Young's modulus were found to decrease with temperature, in the martensite regime, reaching a significant minimum at approximately 80 C followed by an increase in both properties, attributed to the martensite to austenite transformation. The initial decrease in material compliance during heating affected the ease with which martensite reorientation and detwinning could occur, ultimately impacting the stress for inelastic deformation prior to the start of the reverse transformation.

Benafan, Othmane↗

Characterization and Computational Modeling of Minor Phases in Alloy LSHR

The minor phases of powder metallurgy disk superalloy LSHR were studied. Samples were consistently heat treated at three different temperatures for long times to approach equilibrium. Additional heat treatments were also performed for shorter times, to assess minor phase kinetics in non-equilibrium conditions. Minor phases including MC carbides, M23C6 carbides, M3B2 borides, and sigma were identified. Their average sizes and total area fractions were determined. CALPHAD thermodynamics databases and PrecipiCalc(TradeMark), a computational precipitation modeling tool, were employed with Ni-base thermodynamics and diffusion databases to model and simulate the phase microstructural evolution observed in the experiments with an objective to identify the model limitations and the directions of model enhancement.

Jou, Herng-Jeng↗

Effect of Upper-Cycle Temperature on the Load-Biased, Strain-Temperature Response of NiTi

Over the past decade, interest in shape memory alloy based actuators has increased as the primary benefits of these solid-state devices have become more apparent. However, much is still unknown about the characteristic behavior of these materials when used in actuator applications. Recently we have shown that the maximum temperature reached during thermal cycling under isobaric conditions could significantly affect the observed mechanical response of NiTi (55 wt% Ni), especially the amount of transformation strain available for actuation and thus work output. The investigation we report here extends that original work to ascertain whether further increases in the upper-cycle temperature would produce additional changes in the work output of the material, which has a stress-free austenite finish temperature of 113 C, and to determine the optimum cyclic conditions. Thus, isobaric, thermal-cycle experiments were conducted on the aforementioned alloy at various stresses from 50-300 MPa using upper-cycle temperatures of 165, 200, 230, 260, 290, 320 and 350 C. The data indicated that the amount of applied stress influenced the transformation strain, as would be expected. However, the maximum temperature reached during the thermal excursion also plays an equally significant role in determining the transformation strain, with the maximum transformation strain observed during thermal cycling to 290 C. In situ neutron diffraction at stress and temperature showed that the differences in transformation strain were mostly related to changes in martensite texture when cycling to different upper-cycle temperatures. Hence, understanding this effect is important to optimizing the operation of SMA-based actuators and could lead to new methods for processing and training shape memory alloys for optimal performance.

Padula, Santo, II↗

Oxide Scales Formed on NiTi and NiPtTi Shape Memory Alloys

Ni-49Ti and Ni-30Pt-50Ti (at.%) shape memory alloys were oxidized isothermally in air over the temperature range of 500 to 900 C. The microstructure, composition, and phase content of the scales were studied by SEM, EDS, XRD, and metallography. Extensive plan view SEM/EDS identified various features of intact or spalled scale surfaces. The outer surface of the scale was a relatively pure TiO2 rutile structure, typified by a distinct highly striated and faceted crystal morphology. Crystal size increased significantly with temperature. Spalled regions exhibited some porosity and less distinct features. More detailed information was obtained by correlation of SEM/EDS studies of 700 C/100 hr cross-sections with XRD analyses of serial or taper-polishing of plan surfaces. Overall, multiple layers exhibited graded mixtures of NiO, TiO2, NiTiO3, Ni(Ti) or Pt(Ni,Ti) metal dispersoids, Ni3Ti or Pt3Ti depletion zones, and substrate, in that order. The NiTi alloy contained a 3 at.% Fe impurity that appeared in embedded localized Fe-Ti-rich oxides, while the NiPtTi alloy contained a 2 v/o dispersion of TiC that appeared in lower layers. The oxidation kinetics of both alloys (in a previous report) indicated parabolic growth and an activation energy (250 kJ/mole) near those reported in other Ti and NiTi studies. This is generally consistent with TiO2 existing as the primary scale constituent, as described here.

Smialek, James L.↗

Grain Boundary Engineering the Mechanical Properties of Allvac 718Plus(Trademark) Superalloy

Grain Boundary Engineering can enhance the population of structurally-ordered "low S" Coincidence Site Lattice (CSL) grain boundaries in the microstructure. In some alloys, these "special" grain boundaries have been reported to improve overall resistance to corrosion, oxidation, and creep resistance. Such improvements could be quite beneficial for superalloys, especially in conditions which encourage damage and cracking at grain boundaries. Therefore, the effects of GBE processing on high-temperature mechanical properties of the cast and wrought superalloy Allvac 718Plus (Allvac ATI) were screened. Bar sections were subjected to varied GBE processing, and then consistently heat treated, machined, and tested at 650 C. Creep, tensile stress relaxation, and dwell fatigue crack growth tests were performed. The influences of GBE processing on microstructure, mechanical properties, and associated failure modes are discussed.

Gabb, Timothy P.↗

Characterization of Ternary NiTiPd High-Temperature Shape-Memory Alloys under Load-Biased Thermal Cycling

While NiTiPd alloys have been extensively studied for proposed use in high-temperature shape-memory applications, little is known about the shape-memory response of these materials under stress. Consequently, the isobaric thermal cyclic responses of five (Ni,Pd)49.5Ti50.5 alloys with constant stoichiometry and Pd contents ranging from 15 to 46 at. pct were investigated. From these tests, transformation temperatures, transformation strain (which is proportional to work output), and unrecovered strain per cycle (a measure of dimensional instability) were determined as a function of stress for each alloy. It was found that increasing the Pd content over this range resulted in a linear increase in transformation temperature, as expected. At a given stress level, work output decreased while the amount of unrecovered strain produced during each load-biased thermal cycle increased with increasing Pd content, during the initial thermal cycles. However, continued thermal cycling at constant stress resulted in a saturation of the work output and nearly eliminated further unrecovered strain under certain conditions, resulting in stable behavior amenable to many actuator applications.

Bigelow, Glen S.↗

Bonding and Microstructural Stability in Ni55Ti45 Studied by Experimental and Theoretical Methods

Spiral orbit tribometry friction tests performed on Ni-rich Ni55Ti45 titanium ball bearings indicate that this alloy is a promising candidate for future aerospace bearing applications. Microstructural characterization of the bearing specimens was performed using transmission electron microscopy and energy dispersive spectroscopy, with NiTi, Ni4Ti3, Ni3Ti, and Ni2Ti4Ox phases identified within the microstructure of the alloy. Density functional theory was applied to predict the electronic structure of the NixTiy phases, including the band structure and site projected density of states. Ultraviolet photoemission spectroscopy was used to verify the density of states results from the density functional theory calculations, with good agreement observed between experiment and theory.

Stott, Amanda C.↗

A Compendium of Scale Surface Microstructures: Ni(pt)al Coatings Oxidized at 1150 C for 2000 1-h Cycles

The surface structure of scales formed on Ni(Pt)Al coatings was characterized by SEM/EDS/BSE in plan view. Two nominally identical {100} samples of aluminide coated CMSX4 single crystal were oxidized at 1150 C for 2000 1-h cycles and were found to produce somewhat disparate behavior. One sample, with less propensity for coating grain boundary ridge deformation, presented primarily alpha-Al2O3 scale structures, with minimal weight loss and spallation. The original scale structure, still retained over most of the sample, consisted of the classic theta-alpha transformation-induced ridge network structure, with approx. 25 nm crystallographic steps and terraces indicative of surface rearrangement to low energy alumina planes. The scale grain boundary ridges were often decorated with a fine, uniform distribution of (Hf,Ti)O2 particles. Another sample, producing steady state weight losses, exhibited much interfacial spallation and a complex assortment of different structures. Broad areas of interfacial spalling, crystallographically-faceted (Ni,Co)(Al,Cr)2O4 spinel, with an alpha-Al2O3 base scale, were the dominant features. Other regions exhibited nodular spinel grains, with fine or (Ta,Ti)-rich (rutile) particles decorating or interspersed with the spinel. While these features were consistent with a coating that presented more deformation at extruded grain boundaries, the root cause of the different behavior between the duplicate samples could not be conclusively identified.

Smialek, James L.↗

Effect of Upper-Cycle Temperature on the Load-Biased, Strain-Temperature Response of NiTi

Over the past decade, interest in shape memory alloy based actuators has increased as the primary benefits of these solid-state devices have become more apparent. However, much is still unknown about the characteristic behavior of these materials when used in actuator applications. Recently we have shown that the maximum temperature reached during thermal cycling under isobaric conditions could significantly affect the observed mechanical response of NiTi (55 wt% Ni), especially the amount of transformation strain available for actuation and thus work output. This investigation extends that original work to ascertain whether further increases in the upper-cycle temperature would produce additional improvement in the work output of the material, which has a stress-free Af of 113 oC, and to determine the optimum cyclic conditions. Thus, isobaric, thermal-cycle experiments were conducted in the aforementioned alloy at various stress levels from 50-300 MPa using upper-cycle temperatures of 165, 200, 230, 260, 290, 320 and 350 oC. The data indicated that the amount of applied stress influenced the transformation strain available in the system, as would be expected. However, the maximum temperature reached during the thermal excursion also plays a role in determining the transformation strain, with the maximum transformation strain being developed by thermal cycling to 290 oC. In situ, neutron diffraction showed that the differences in transformation strain were related to differences in martensite texture within the microstructure when cycling to different upper-cycle temperatures. Hence, understanding this effect is important to optimizing the operation of SMA-based actuators and could lead to new methods for processing and training shape memory alloys for optimal performance.

Padula, Santo, II↗