Microscopic origin of highly enhanced current carrying capabilities of thin NdFeAs(O,F) films
The physical properties of FBS depend strongly on crystal structure, chemical composition and microstructure.
Engineering topics
Publications and source records attributed to Gerthsen, Dagmar.
The physical properties of FBS depend strongly on crystal structure, chemical composition and microstructure.
This work clarifies the mechanism of the formation of hollow nanostructures (nanotubes and nanospheres) during the InOOH to rh-In 2 O 3 transformation.
The growth of core–shell nanocrystals (NCs) can lead to extended interface disorder due to the intermixing of core and shell materials. Such an issue is particularly important for large single- and multi-shell upconverting NCs, which have been considered as being relatively insusceptible to intermixing. In this work, a robust methodology – based on structure-independent local chemical analyses with nanometer-scale resolution and high-energy synchrotron X-ray powder diffraction – has been used to shed new light on the chemical and structural organization of large single-, double-, and triple-shell upconverting NCs. Furthermore, the experimental results reveal, for the first time, that significant disorder: (i) exists at the interfaces of large (20–50 nm) multi-shell upconverting NCs; (ii) reaches core–shell and shell–shell interfaces, independently of their position within the structure; (iii) can be partially controlled by the shell deposition method; and (iv) leads to the formation of multiple length-scale interfaces depending on the size of the starting seeds, the number and relative thickness of the pre-existing shells in the seeds. It is likely that the results will be beneficial in furthering the fundamental understanding of the structure–property relationships of multi-shell upconverting NCs.
Core@shell design represents an important class of architectures because of its capability to dramatically increase the absolute upconversion quantum yield (UCQY) of upconverting nanocrystals (UCNCs) but also to tune energy migration pathways. A relatively new trend towards the use of very thick optically inert shells affording significantly higher absolute UCQYs raises the question of the crystallographic and chemical characteristics of such nanocrystals (NCs). In this article, local chemical analyses performed by scanning transmission electron microscopy (STEM) combined with energy dispersive x-ray spectroscopy (EDXS) and x-ray total scattering experiments together with pair distribution function (PDF) analyses were used to probe the local chemical and structural characteristics of hexagonal β-NaGd0.78Yb0.2Er0.02F4@NaYF4 core@shell UCNCs. The investigations lead to a new crystallochemical model to describe core@shell UCNCs that considerably digresses from the commonly accepted epitaxial growth concept with sharp interfaces. The results obtained on ultra-small (4.8 ± 0.5 nm) optically active cores (β-NaGd0.78Yb0.2Er0.02F4) surrounded by an optically inert shell (NaYF4) of tunable thickness (roughly 0, 1, 2, and 3.5 nm) clearly indicate the massive dissolution of the starting seeds and the inter-diffusion of the shell element (such as Y) into the Gd/Yb/Er-containing core giving rise to the formation of a non-homogeneous solid solution characterized by concentration gradients and the lack of sharp interfaces. Independently of the inert shell thickness, core/interface/shell architectures were observed for all synthesized UCNCs. The presented results constitute a significant step towards the comprehensive understanding of the “structure - property” relationship of upconverting core@shell architectures, which is of prime interest not only in the development of more efficient structures but also to provide new physical insights at the nanoscale to better explain upconversion (UC) properties alterations.
Abstract not provided
We report on a simple approach for the fabrication of polycrystalline Cu{sub 2}ZnSnSe{sub 4} films on GaAs with strongly preferential grain orientation. Such layers are important for both fundamental spectroscopic investigations as well as studies of the impact of grain boundaries on the performance of solar cells. Cu{sub 2}ZnSnSe{sub 4} (CZTSe) layers were fabricated by growing a Sn/Cu/ZnSe(001) stack on a GaAs(001) substrate in a molecular-beam epitaxy system followed by selenization in a tube furnace. Raman spectroscopy as well as X-ray diffraction measurements combined with a microstructural investigation indicate the presence of the kesterite phase. Further, X-ray analysis such as rocking curves and ϕ-scans proves a preferential grain orientation of the obtained CZTSe films in all three dimensions.
Tribological testing of a coarse-grained diamond layer, deposited by plasma-enhanced chemical vapor deposition, was performed on a ring-on-ring tribometer with a diamond counterpart. The origin of the wear of diamond and of the low friction coefficient of 0.15 was studied by analyzing the microstructure of worn and unworn regions by transmission and scanning electron microscopy. In the worn regions, the formation of an amorphous carbon layer with a thickness below 100 nm is observed. Electron energy loss spectroscopy of the C-K ionization edge reveals the transition from sp{sup 3}-hybridized C-atoms in crystalline diamond to a high fraction of sp{sup 2}-hybridized C-atoms in the tribo-induced amorphous C-layer within a transition region of less than 5 nm thickness. The mechanically induced phase transformation from diamond to the amorphous phase is found to be highly anisotropic which is clearly seen at a grain boundary, where the thickness of the amorphous layer above the two differently oriented grains abruptly changes.