Diffusion-limited hydrolysis in polymeric materials

Polymer degradation under aggressive environmental stressors often develops heterogeneities due to diffusion-limited reaction phenomena. This is well established for diffusion-limited oxidation (DLO), which is known to occur for most polymeric materials at elevated temperatures but has been less summarized for the conditions of diffusion-limited hydrolysis (DLH). Here, an overview of hydrolysis for several materials and a computational model, analogous to the underlying equations for DLO, able to define this diffusion-reaction system is presented. A systematic study of the influence of various parameters, such as water diffusivity, reaction rate and order, and a more in-depth focus on residual isocyanate hydrolysis in a polymeric methylene diphenyl diisocyanate (pMDI) based polyurethane (PU) foam is given. For this system, we present experimental data for model ‘input’ parameters and discuss predictions for different conditions. We conceptually compare the behavior of diffusion-limited oxidation to that of diffusion-limited hydrolysis (DLH). With the mathematical framework and key material properties presented herein, any DLH phenomena following Fickian diffusion behavior can be understood, modeled, and predicted.

36 MATERIALS SCIENCE↗

Anomalous aging of EPDM and FEPM under combined thermo-oxidative and hydrolytic conditions

Previous observation of EPDM and FEPM materials aged in thermo-oxidative and thermo-oxidative plus hydrolytic environments revealed an unusual trend: the degradation and disintegration of these polymers in the former case but the ability to maintain mechanical performance and shape in the latter [1]. No abnormalities were observed in the chemical (oxidation rates, FTIR spectra, solvent uptake, gel content, and weight loss vs. temperature) or physical (modulus profile) measurements that could explain these empirically observed aging differences. A second controlled aging test was conducted to verify this trend using only EPDM. Once again it was shown that thermo-oxidative conditions appear to cause more degradative damage (enhanced embrittlement) than observed for the combined thermo-oxidative plus hydrolytic environments. From these data we conclude that water may favorably interfere with normal thermo-oxidative degradation processes. This interference may occur via some combination of chemical and physical property changes in the presence of steam such as: oxidation rate and O2 permeability changes, additional sensitivity to hydrolytic damage, and/or mechanistic changes in relation to pH and hydroperoxide formation.

15 GEOTHERMAL ENERGY↗

Stress Relaxation in Epoxy Thermosets via a Ferrocene-Based Amine Curing Agent

Physical stress relaxation in rubbery, thermoset polymers is limited by cross-links, which impede segmental motion and restrict relaxation to network defects, such as chain ends. In parallel, the cure shrinkage associated with thermoset polymerizations leads to the development of internal residual stress that cannot be effectively relaxed. Recent strategies have reduced or eliminated such cure stress in thermoset polymers largely by exploiting chemical relaxation processes, wherein temporary cross-links or otherwise transient bonds are incorporated into the polymer network. In this paper, we explore an alternative approach, wherein physical relaxation is enhanced by the incorporation of organometallic sandwich moieties into the backbone of the polymer network. A standard epoxy resin is cured with a diamine derivative of ferrocene and compared to conventional diamine curing agents. The ferrocene-based thermoset is clearly distinguished from the conventional materials by reduced cure stress with increasing cure temperature as well as unique stress relaxation behavior above its glass transition in the fully cured state. The relaxation experiments exhibit features characteristic of a physical relaxation process. Furthermore, the cure stress is observed to vanish precipitously upon deliberate introduction of network defects through an increasing imbalance of epoxy and amine functional groups. Finally, we postulate that these beneficial properties arise from fluxional motion of the cyclopentadienyl ligands on the polymer backbone.

36 MATERIALS SCIENCE↗

High temperature polymer degradation: Rapid IR flow-through method for volatile quantification

Accelerated aging of polymers at elevated temperatures often involves the generation of volatiles. These can be formed as the products of oxidative degradation reactions or intrinsic pyrolytic decomposition as part of polymer scission reactions. A simple analytical method for the quantification of water, CO 2 , and CO as fundamental signatures of degradation kinetics is required. Here, we describe an analytical framework and develops a rapid mid-IR based gas analysis methodology to quantify volatiles that are contained in small ampoules after aging exposures. The approach requires identification of unique spectral signatures, systematic calibration with known concentrations of volatiles, and a rapid acquisition FTIR spectrometer for time resolved successive spectra. Furthermore, the volatiles are flushed out from the ampoule with dry N2 carrier gas and are then quantified through spectral and time integration. This method is sufficiently sensitive to determine absolute yields of ~50 μg water or CO 2 , which relates to probing mass losses of less than 0.01% for a 1 g sample, i.e. the early stages in the degradation process. Such quantitative gas analysis is not easily achieved with other approaches. Our approach opens up the possibility of quantitative monitoring of volatile evolution as an avenue to explore polymer degradation kinetics and its dependence on time and temperature.

36 MATERIALS SCIENCE↗