Investigating the Effects of Lithium Deposition on the Abuse Response of Lithium-Ion Batteries

Li deposition at the graphitic anode is widely reported in literature as one of the leading causes of capacity fade in lithium-ion batteries (LIBs). Previous literature has linked Li deposition resulting from low-temperature ageing to diminished safety characteristics, however no current research has probed the effects of Li deposition on the abuse response of well-characterized cells. Using overtemperature testing, a relationship between increased concentrations of Li deposition and exacerbated abuse response in 1 Ah pouch cells has been established. A novel Li deposition technique is also investigated, where cells with n:p < 1 (anode-limiting) have been cycled at a high rate to exploit Li + diffusion limitations at the anode. Scanning Electron Microscopy of harvested anodes indicates substantial Li deposition in low n:p cells after 20 cycles, with intricate networks of Li(s) deposits which hinder Li + intercalation/deintercalation. Peak broadening and decreased amplitude of differential capacity plots further validates a loss of lithium inventory to Li + dissolution, and Powder X-ray Diffraction indicates Li + intercalation with staging in anode interstitial sites as the extent of Li deposition increases. A cradle-to-grave approach is leveraged on cell fabrication and testing to eliminate uncertainty involving the effects of cell additives on Li deposition and other degradation mechanisms.

25 ENERGY STORAGE↗

Evaluation of Multi-cell Failure Propagation

Failure propagation testing is of increasing interest to the designers and end users of battery systems. One of the chief difficulties, however, is choosing an appropriate initiation method to perform the test. Single cell abuse testing is typically used to initiate thermal runaway but this can involve a large amount of additional energy injected into the system. It is assumed that this will have some impact on the behavior of a propagating thermal runaway event, but there is little data available as to how significant this would be. Further, it is ultimately difficult to develop viable propagation tests for compliance and public safety activities without better knowledge of how test methods will impact the results. This work looks at propagating battery failure with a variety of chemistries, formats, configurations and initiation methods to determine the level of significance of the chosen initiation method on the test results. We have ultimately found while there is some impact on the detailed results of propagation testing, in most cases other factors, particularly the energy density of the system play a much greater role in the likelihood of a propagation event consuming an entire battery. We have also provided some guidelines for test design to support best practices in testing.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /Graphite cells–effect of binder

Cells based on NMC/graphite, containing styrene-butadiene rubber/carboxymethylcellulose binder in the anodes and pVdF latex/carboxymethykellulose in the cathodes, were systematically overcharged to 100, 120, 140, 160, 180, 250% and 270% state-of-charge. The impact of the binder was characterized by elemental analysis, SEM, and HPLC. These results were compared to similar cells just using the poly (vinylidene difluoride) binder. Not only did the binder impact the rate of transition metal transport from the cathode to the anode, it also had a marked effect on the microstructure and composition of the materials on the anode surface.

25 ENERGY STORAGE↗

Effect of binder on the overcharge response in LiFePO 4 -containing cells

Two types of small pouch cells based on LiFePO 4 /graphite, one containing a N-methyl pyrrolidinone (NMP)-soluble binder, poly(vinylidene difluoride), and the other an aqueous-soluble binder, styrene-butadiene rubber/carboxymethylcellulose were systematically charged to 100, 120, 140, 160, 180, and 250% state of charge (SOC). The cells were then discharged to 3.0 V at room temperature before being disassembled for postmortem analysis. Microstructural changes in the anode associated with increasing SOC were more pronounced in the aqueous processed cells in comparison to the NMP-processed cells. Dendrite formation was observed on the aqueous-processed anode at 120% SOC, while the NMP-processed anode surface does not show dendrites until 250% SOC. Overall, the aqueous-processed anode surfaces displayed more evidence of microstructural degradation as a function of increasing SOC. In the NMP-processed cells, four organic compounds on the anode surface were found to show a dependence on SOC, while only two displayed a similar dependency in the aqueous-processed cells. The nature of the binder changed the number and composition of the species found at the anode.

25 ENERGY STORAGE↗

Effect of overcharge on lithium-ion cells: Silicon/graphite anodes

Small pouch cells containing Si/graphite electrodes were systematically charged to 100, 120, 140, 160, 180 and 250% state of charge. Description of the Si/graphite electrode after the overcharge showed some features similar to those found in a pure graphite electrode. Since the amount of silicon in the electrode was ~15 wt%, this was not unexpected. The effect of silicon was observed in the composition of the SEI layer and the trends in two components of the SEI layer.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /Graphite lithium ion cells with poly(vinylidene fluoride) binder. I - Microstructural changes in the anode

Cells based on NMC/graphite, containing poly(vinylidene difluoride) (PVDF) binders in the positive and negative electrodes, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state-of-charge (SOC). At 250% SOC the cell vented. Scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) of the anodes showed several state-of-overcharge-dependent trends. Starting at 120% SOC, dendrites appeared and increased in concentration as the SOC increased. Dendrite morphology appeared to be dependent on whether the active material was on the “dull” or “shiny” side of the copper collector. Significantly more delamination of the active material from the collector was seen on the “shiny” side of the collector particularly at 180 and 250% SOC. Transition metals were detected at 120% SOC and increased in concentration as the SOC increased. Finally, there was considerable spatial heterogeneity in the microstructures across each laminate with several regions displaying complex layered structures.

25 ENERGY STORAGE↗