Search NASA⌕ Search

Engineering topics

Gul, Rubi

Publications and source records attributed to Gul, Rubi.

Structural and Electronic Properties of Indium-Doped n-type Cd-Se-Te Crystals

Here, we present a comprehensive investigation into the potential of n-type indium-doped cadmium selenide telluride (CST:In) as a high-performance candidate for solar cell applications, without the need for resource-intensive post-growth treatments that are required for CdTe:In. We compared undoped CST and CST:In crystals under different growth conditions, analyzing their structural and electronic properties using x-ray diffraction (XRD), electron probe microanalysis (EPMA), current-voltage (IV) and Hall effect measurements, time-resolved photoluminescence (TRPL), optical transmission, and photoluminescence (PL) mapping. The results reveal that as-grown CST:In crystals achieve nearly 100% carrier activation, yielding an electron concentration of 9.5x1018 cm -3 , mobility of 653 cm 2 /V.s and a 5 ns lifetime which approaches the radiative limit. Furthermore, comparison of PL maps from crystal growths having different cooling profiles suggests a strong effect of cooling rate on selenium segregation and cubic/hexagonal/polytype phase distribution. Slower cooling leads to a more homogeneous cubic structure with lower Se segregation, while a faster cooling rate results in increased Se segregation, and twin boundaries and stacking faults with polytypic and hexagonal character.

14 SOLAR ENERGY↗

Developing CdTe homojunctions applying high throughput deposition

In this project, we attempted to make CdTe homojunctions using single crystal p-type doped substrates and closed-space sublimation epitaxy (CSSE) n-type doped films. The project included modeling which determined the ideal thickness for the n-type layer as being <200 nm. Boules of high concentration indium-doped CdTe and CdSe 0.4 Te 0.6 (CST) were grown using modified vertical Bridgman (MVB) methods. Similarly, iodine-doped CdTe crystals were grown for the first time. Washington State University (WSU) stock phosphorus-doped CdTe was used as the p-type substrate layer. The crystals were characterized by Hall effect and time-resolved photoluminescence (TRPL, for electrical properties), photoluminescence microscopy (for uniformity), X-ray diffraction (for crystal structure), and glow discharge mass spectrometry (GDMS, for dopant and impurity concentration). CdTe:I crystals were also characterized by visible and infrared transmission measurements, and various Cd or Te heat treatments were performed to assess changes in optical and electrical properties. The grown n-type materials – CdTe:In, CdSe0.4Te0.6:In, and CdTe:I – were provided to the National Renewable Energy Laboratory (NREL) for growth of CSSE thick films for characterization by two photon TRPL (for carrier lifetime), electron back-scatter diffraction (EBSD, to assess epitaxy), and Hall effect. Several measurements of secondary ion mass spectroscopy (SIMS) were performed. Nearly 100% of the indium from the crystal was incorporated into the measured thick films, while only ~2-22% of the iodine from the crystal was incorporated. The net result of the diffusion issue is that homojunction devices created using CSSE have a buried homojunction, as indicated by the near infrared peak in the external quantum efficiency (EQE). Various parameterization of front and back contacts suggested that the poor device performance was primarily a result of this buried junction and not due to other effects. There may also be an issue with the CSSE film lifetime in addition to the dopant profile.

14 SOLAR ENERGY↗

Study of Chemical Etching and Chemo-Mechanical Polishing on CdZnTe Nuclear Detectors

Cadmium zinc telluride (CdZnTe) semiconductor has applications in the detection of Xrays and gamma-rays at room temperature without having to use a cooling system. Chemical etching and chemo-mechanical polishing are processes used to smoothen CdZnTe wafer during detector device fabrication. These processes reduce surface damages left after polishing the wafers. In this paper, we compare the effects of etching and chemo-mechanical polishing on CdZnTe nuclear detectors, using a solution of hydrogen bromide in hydrogen peroxide and ethylene glycol mixture. X-ray photoelectron spectroscopy (XPS) was used to monitor TeO 2 on the wafer surfaces. Current-voltage and detector-response measurements were made to study the electrical properties and energy resolution. XPS results showed that the chemical etching process resulted in the formation of more TeO 2 on the detector surfaces compared to chemo-mechanical polishing. The electrical resistivity of the detector is of the order of 10 10 Ω-cm. The chemo-mechanical polishing process increased the leakage current more that chemical etching. For freshly treated surfaces, the etching process is more detrimental to the energy resolution more than chemo-mechanically polishing. The energy resolutions of the CdZnTe wafers are expected to improve as the surfaces stabilize and result in reduced surface currents.

36 MATERIALS SCIENCE↗

Evaluation of CdZnTeSe as a high-quality gamma-ray spectroscopic material with better compositional homogeneity and reduced defects

X- and gamma-ray detectors have broad applications ranging from medical imaging to security, non-proliferation, high-energy physics and astrophysics. Detectors with high energy resolution, e.g. less than 1.5% resolution at 662 keV at room temperature, are critically important in most uses. The efficacy of adding selenium to the cadmium zinc telluride (CdZnTe) matrix for radiation detector applications has been studied. In this paper, the growth of a new quaternary compound Cd 0.9 Zn 0.1 Te 0.98 Se 0.02 by the Traveling Heater Method (THM) is reported. The crystals possess a very high compositional homogeneity with less extended defects, such as secondary phases and sub-grain boundary networks. Virtual Frisch-grid detectors fabricated from as-grown ingots revealed ~0.87-1.5% energy resolution for 662-keV gamma rays. The superior material quality with a very low density of defects and very high compositional homogeneity heightens the likelihood that Cd 0.9 Zn 0.1 Te 0.98 Se 0.02 will be the next generation room-temperature detector material.

36 MATERIALS SCIENCE↗

Mini Compton Camera Based on an Array of Virtual Frisch-Grid CdZnTe Detectors

In this study, we constructed a mini Compton camera based on an array of CdZnTe detectors and assessed its spectral and imaging properties. The entire array consisted of 6×6 Frisch-grid CdZnTe detectors, each with a size of 6×6 ×15 mm 3 . Since it is easier and more practical to grow small CdZnTe crystals rather than large monolithic ones, constructing a mosaic array of parallelepiped crystals can be an effective way to build a more efficient, large-volume detector. With the fully operational CdZnTe array, we measured the energy spectra for 133 Ba -, 137 Cs -, 60 Co-radiation sources; we also located these sources using a Compton imaging approach. Although the Compton camera was small enough to hand-carry, its intrinsic efficiency was several orders higher than those generated in previous researches using spatially separated arrays, because our camera measured the interactions inside the CZT detector array, wherein the detector elements were positioned very close to each other. Lastly, the performance of our camera was compared with that based on a pixelated detector.

36 MATERIALS SCIENCE↗

Effects of chemo-mechanical polishing on CdZnTe X-ray and gamma-ray detectors

Here, mechanically polishing cadmium zinc telluride (CdZnTe) wafers for x-ray and gamma-ray detectors often is inadequate in removing surface defects caused by cutting them from the ingots. Fabrication-induced defects, such as surface roughness, dangling bonds, and nonstoichiometric surfaces, often are reduced through polishing and etching the surface. In our earlier studies of mechanical polishing with alumina powder, etching with hydrogen bromide in hydrogen peroxide solution, and chemomechanical polishing with bromine–methanol–ethylene glycol solution, we found that the chemomechanical polishing process produced the least surface leakage current. In this research, we focused on using two chemicals to chemomechanically polish CdZnTe wafers after mechanical polishing, viz. bromine–methanol–ethylene glycol (BME) solution, and hydrogen bromide (HBr) in a hydrogen peroxide and ethylene–glycol solution. We used x-ray photoelectron spectroscopy (XPS), current–voltage (I–V) measurements, and Am-241 spectral response measurements to characterize and compare the effects of each solution. The results show that the HBr-based solution produced lower leakage current than the BME solution. Results from using the same chemomechanical polishing solution on two samples confirmed that the surface treatment affects the measured bulk current (a combination of bulk and surface currents). XPS results indicate that the tellurium oxide to tellurium peak ratios for the mechanical polishing process were reduced significantly by chemomechanical polishing using the BME solution (78.9% for Te 3d 5/2 O 2 and 76.7% for Te 3d 3/2 O 2 ) compared with the HBr-based solution (27.6% for Te 3d 5/2 O 2 and 35.8% for Te 3d 3/2 O 2 ). Spectral response measurements showed that the 59.5-keV peak of Am-241 remained under the same channel number for all three CdZnTe samples. While the BME-based solution gave a better performance of 7.15% full-width at half-maximum (FWHM) compared with 7.59% FWHM for the HBr-based solution, the latter showed a smaller variation in performance of 0.39% FWHM over 7 days compared with 0.69% for the BME-based solution.

36 MATERIALS SCIENCE↗