Search NASA⌕ Search

Engineering topics

Guo, Zezhou

Publications and source records attributed to Guo, Zezhou.

Formation and Detriments of Residual Alkaline Compounds on High-Nickel Layered Oxide Cathodes

High-nickel layered oxides LiNi x M 1-x O 2 (x ≥ 0.9) have emerged as promising cathode materials for automotive batteries due to their high energy density and lower cost. However, the formation and accumulation of surface alkaline compounds during storage hinder their mass production and commercialization. Here, in this study, a validated chemical method is employed to deconvolute and quantify the evolution of each residual lithium compound in four representative cathodes during ambient-air storage, viz., LiNiO 2 (LNO), LiNi 0.95 Co 0.05 O 2 (NC), LiNi 0.95 Mn 0.05 O 2 (NM), and LiNi 0.95 Al 0.05 O 2 (NA). Furthermore, the activation energy of the reaction between water and the cathode is determined by measuring the leached LiOH concentration at various temperatures. While residual lithium and time-of-flight secondary-ion mass spectrometry measurements collectively reveal that the air stability overall follows the trend of NM > NA ≈ NC > LNO, the aged NM exhibits the highest charge-transfer resistance and the worst electrochemical performance among the cathodes. In situ, X-ray diffraction and scanning transmission electron microscopy unveil that the aged NM is plagued by a large area of resistive spinel-like M 3–x Li x O 4 phases, leading to aggravated particle reaction heterogeneity. Finally, a one-step recalcination method is demonstrated effective in fully restoring the degraded cathodes. This work provides insights into overcoming air sensitivity issues of high-Ni cathodes.

(S)TEM↗

Irreparable Interphase Chemistry Degradation Induced by Temperature Pulse in Lithium‐Ion Batteries

Abstract While it is widely recognized that the operating temperature significantly affects the energy density and cycle life of lithium‐ion batteries, the consequence of electrode‐electrolyte interphase chemistry to sudden environmental temperature changes remains inadequately understood. Here, we systematically investigate the effects of a temperature pulse (T pulse) on the electrochemical performance of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) pouch full cells. By utilizing advanced characterization tools, such as time‐of‐flight secondary‐ion mass spectrometry, we reveal that the T pulse can lead to an irreversible degradation of cathode‐electrolyte interphase chemistry and architecture. Despite negligible immediate impacts on the solid‐electrolyte interphase (SEI) on graphite anode, aggregated cathode‐to‐anode chemical crossover gradually degrades the SEI by catalyzing electrolyte reduction decomposition and inducing metallic dead Li formation because of insufficient cathode passivation after the T pulse. Consequently, pouch cells subjected to the T pulse show an inferior cycle stability to those free of the T pulse. This work unveils the effects of sudden temperature changes on the interphase chemistry and cell performance, emphasizing the importance of a proper temperature management in assessing performance.

Cui, Zehao↗

Irreparable Interphase Chemistry Degradation Induced by Temperature Pulse in Lithium–Ion Batteries

While it is widely recognized that the operating temperature significantly affects the energy density and cycle life of lithium-ion batteries, the consequence of electrode-electrolyte interphase chemistry to sudden environmental temperature changes remains inadequately understood. Here, we systematically investigate the effects of a temperature pulse (T pulse) on the electrochemical performance of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) pouch full cells. By utilizing advanced characterization tools, such as time-of-flight secondary-ion mass spectrometry, we reveal that the T pulse can lead to an irreversible degradation of cathode-electrolyte interphase chemistry and architecture. Despite negligible immediate impacts on the solid-electrolyte interphase (SEI) on graphite anode, aggregated cathode-to-anode chemical crossover gradually degrades the SEI by catalyzing electrolyte reduction decomposition and inducing metallic dead Li formation because of insufficient cathode passivation after the T pulse. Consequently, pouch cells subjected to the T pulse show an inferior cycle stability to those free of the T pulse. Furthermore, this work unveils the effects of sudden temperature changes on the interphase chemistry and cell performance, emphasizing the importance of a proper temperature management in assessing performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Localized High–Concentration Electrolytes with Low–Cost Diluents Compatible with Both Cobalt–Free LiNiO 2 Cathode and Lithium–Metal Anode

High-nickel layered oxide cathodes and lithium-metal anode are promising candidates for next-generation battery systems due to their high energy density. Nevertheless, the instability of the electrode–electrolyte interphase is hindering their practical application. Localized high-concentration electrolytes (LHCEs) present a promising solution for achieving uniform lithium deposition and a stable cathode–electrolyte interphase. However, the limited choice of diluents and their high cost are restricting their implementation. Four novel cost-effective diluents and their performance with highly reactive LiNiO 2 cathode and Li-metal anode are reported here. The results show that all the LHCE cells exhibit a Coulombic efficiency of >99.38% in Li | Cu cells and a capacity retention of >85% in Li | LiNiO 2 cells after 250 cycles. Advanced characterizations unveil that the stable cell operation is due to well-tuned electrode–electrolyte interphases and Li deposition morphology. In addition, online electrochemical mass spectroscopy and differential scanning calorimetry reveal that the gas generation and heat-release are greatly reduced with the LHCEs presented. Altogether, the study provides new insights into the role of diluents in LHCEs and offers valuable guidance for further optimization of LHCEs for high energy density lithium-metal batteries.

25 ENERGY STORAGE↗

Assessing the Intrinsic Roles of Key Dopant Elements in High–Nickel Layered Oxide Cathodes in Lithium–Based Batteries

A rational compositional design is critical for utilizing LiNiO 2 -based cathodes with Ni contents > 90% as promising next-generation cathode materials. Unfortunately, the lack of a fundamental understanding of the intrinsic roles of key elements, such as cobalt, manganese, and aluminum, makes the rational compositional design of high-Ni cathodes with a limited range of dopants (<10%) particularly challenging. Here, with 5% single-element doped cathodes, viz., LiNi 0.95 Co 0.05 O 2 , LiNi 0.95 Mn 0.05 O 2 , and LiNi 0.95 Al 0.05 O 2 , along with undoped LiNiO 2 (LNO), the influences of the dopants are systematically examined through a control of cutoff charge energy density and a common practice of cutoff charge voltage. Comprehensive investigations into the electrochemical properties, combined with in-depth analyses of the structural and interfasial stabilities and electrolyte decomposition pathways through advanced characterizations, unveil the following: i) the intrinsic role of dopants regulates the cathode energy density or state-of-charge and, more critically, the occurrence of H2–H3 phase transition, which essentially dictates cyclability; ii) undoped LNO can be stabilized well with the avoidance of H2–H3 phase transition; and iii) Co provides more merits overall with an optimized electrochemical operating condition. Finally, this work provides guidance for the compositional design of high-energy-density high-Ni cathodes and sheds light on the challenges of removing Co.

25 ENERGY STORAGE↗