Elimination of carbon vacancies in 4H-SiC employing thermodynamic equilibrium conditions at moderate temperatures

The carbon vacancy (V{sub C}) is a major point defect in high-purity 4H-SiC epitaxial layers limiting the minority charge carrier lifetime. In layers grown by chemical vapor deposition techniques, the V{sub C} concentration is typically in the range of 10{sup 12 }cm{sup −3}, and after device processing at temperatures approaching 2000 °C, it can be enhanced by several orders of magnitude. In the present study, both as-grown layers and a high-temperature processed one have been annealed at 1500 °C and the V{sub C} concentration is demonstrated to be strongly reduced, exhibiting a value of only a few times 10{sup 11 }cm{sup −3} as determined by deep-level transient spectroscopy measurements. The value is reached already after annealing times on the order of 1 h and is evidenced to reflect thermodynamic equilibrium under C-rich ambient conditions. The physical processes controlling the kinetics for establishment of the V{sub C} equilibrium are estimated to have an activation energy below ∼3 eV and both in-diffusion of carbon interstitials and out-diffusion of V{sub C}'s are discussed as candidates. This concept of V{sub C} elimination is flexible and readily integrated in a materials and device processing sequence.

36 MATERIALS SCIENCE↗

Elimination of carbon vacancies in 4H-SiC epi-layers by near-surface ion implantation: Influence of the ion species

The carbon vacancy (V{sub C}) is a prevailing point defect in high-purity 4H-SiC epitaxial layers, and it plays a decisive role in controlling the charge carrier lifetime. One concept of reducing the V{sub C}-concentration is based on carbon self-ion implantation in a near surface layer followed by thermal annealing. This leads to injection of carbon interstitials (C{sub i}'s) and annihilation of V{sub C}'s in the epi-layer “bulk”. Here, we show that the excess of C atoms introduced by the self-ion implantation plays a negligible role in the V{sub C} annihilation. Actually, employing normalized implantation conditions with respect to displaced C atoms, other heavier ions like Al and Si are found to be more efficient in annihilating V{sub C}'s. Concentrations of V{sub C} below ∼2 × 10{sup 11} cm{sup −3} can be reached already after annealing at 1400 °C, as monitored by deep-level transient spectroscopy. This corresponds to a reduction in the V{sub C}-concentration by about a factor of 40 relative to the as-grown state of the epi-layers studied. The negligible role of the implanted species itself can be understood from simulation results showing that the concentration of displaced C atoms exceeds the concentration of implanted species by two to three orders of magnitude. The higher efficiency for Al and Si ions is attributed to the generation of collision cascades with a sufficiently high energy density to promote C{sub i}-clustering and reduce dynamic defect annealing. These C{sub i}-related clusters will subsequently dissolve during the post-implant annealing giving rise to enhanced C{sub i} injection. However, at annealing temperatures above 1500 °C, thermodynamic equilibrium conditions start to apply for the V{sub C}-concentration, which limit the net effect of the C{sub i} injection, and a competition between the two processes occurs.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Sodium diffusion in 4H-SiC

Sodium diffusion has been studied in p-type 4H-SiC. Heat treatments have been performed from 1200 °C to 1800 °C for 1 min to 4 h. Secondary ion mass spectrometry has been used to measure the sodium distribution. We show that sodium has a considerable mobility at 1200 °C in p-type 4H-SiC. On the other hand for sodium atoms trapped at suitable sites the mobility is limited up to 1800 °C. Trap limited diffusion kinetics is suggested and an effective diffusivity has been extracted with an activation energy of 4 eV for sodium diffusion in p-type 4H-SiC.

36 MATERIALS SCIENCE↗

Origin of the anomalous temperature dependence of coercivity in soft ferromagnets

We report on the origin of the anomalous temperature dependence of coercivity observed in some soft ferromagnets by studying the magnetic and electronic properties of FeZr films doped using ion implantation by H, He, B, C, and N. The anomalous increase of the coercivity with temperature was observed only in the C- and B-doped samples. Using x-ray photoelectron spectroscopy, we show that the anomalous behavior of the coercivity coincides with the occurrence of an electron charge transfer for those implanted samples. The origin of the anomaly is discussed in terms of (i) magnetic softness, (ii) nature of the Fe-C and -B covalent bonds, and (iii) large charge transfer.

36 MATERIALS SCIENCE↗

Effect of implanted species on thermal evolution of ion-induced defects in ZnO

Implanted atoms can affect the evolution of ion-induced defects in radiation hard materials exhibiting a high dynamic annealing and these processes are poorly understood. Here, we study the thermal evolution of structural defects in wurtzite ZnO samples implanted at room temperature with a wide range of ion species (from {sup 11}B to {sup 209}Bi) to ion doses up to 2 × 10{sup 16} cm{sup −2}. The structural disorder was characterized by a combination of Rutherford backscattering spectrometry, nuclear reaction analysis, and transmission electron microscopy, while secondary ion mass spectrometry was used to monitor the behavior of both the implanted elements and residual impurities, such as Li. The results show that the damage formation and its thermal evolution strongly depend on the ion species. In particular, for F implanted samples, a strong out-diffusion of the implanted ions results in an efficient crystal recovery already at 600 °C, while co-implantation with B (via BF{sub 2}) ions suppresses both the F out-diffusion and the lattice recovery at such low temperatures. The damage produced by heavy ions (such as Cd, Au, and Bi) exhibits a two-stage annealing behavior where efficient removal of point defects and small defect clusters occurs at temperatures ∼500 °C, while the second stage is characterized by a gradual and partial annealing of extended defects. These defects can persist even after treatment at 900 °C. In contrast, the defects produced by light and medium mass ions (O, B, and Zn) exhibit a more gradual annealing with increasing temperature without distinct stages. In addition, effects of the implanted species may lead to a nontrivial defect evolution during the annealing, with N, Ag, and Er as prime examples. In general, the obtained results are interpreted in terms of formation of different dopant-defect complexes and their thermal stability.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗