Search NASA⌕ Search

Engineering topics

Hawley, William

Publications and source records attributed to Hawley, William.

Deconvoluting sources of failure in lithium metal batteries containing NMC and PEO-based electrolytes

Solid-state lithium metal batteries (SSLMBs) containing polyethylene oxide (PEO)-derived polymer electrolytes and high-voltage (> 4 V vs. Li/Li + ) cathode materials suffer from three sources of failure: (1) instability between the polymer electrolyte and cathode at high voltage, (2) instability of the polymer electrolyte with Li metal, and (3) poorly-designed cathodes. In this study, these three sources of failure are deconvoluted by studying Ni-rich LiNi x Mn y Co 1-x-y O 2 (NMC, x ≥ 0.6) cathodes and a gel polymer electrolyte (GPE) derived from PEO. Initial cycling data reveals that rapid capacity fade occurs regardless of whether soft short circuits form due to Li dendrites. Cyclic voltammetry scans on cells featuring a Li metal electrode, GPE, and a NMC811 electrode free of additives suggest that there are no runaway reactions between the GPE and NMC811 up to 4.5 V vs. Li/Li + . Cathode/cathode symmetric cell cycling demonstrates that Li metal reactivity is a prime source of failure, though a poorly-designed cathode leads to subpar performance. A cathode with single-crystal NMC particles was demonstrated to achieve better initial capacity and longer cycle life, indicating room for improvement in SSLMB cathode design. Therefore, the sources of failure as enumerated may be ranked as follows from most to least concerning: 2 > 3 > 1.

25 ENERGY STORAGE↗

Role of silicon-graphite homogeneity as promoted by low molecular weight dispersants

This study explores low molecular weight polymers with the same chemical repeat structure as high molecular weight poly acrylic acid (PAA) and lithium poly acrylic acid (LiPAA) binders which act as a dispersant to improve the silicon-graphite electrode performance. The electrodes which utilize LiPAA as a dispersant perform, on average, the best with respect to the maximum capacity (compared to theoretical), rate performance, and capacity retention with time. These electrodes also have the poorest dispersion of binder, indicating that the poor binder dispersion is essential to electrode performance. In contrast, this study shows that electrodes formulated using PAA had good dispersion and performs the worst in cycling. Finally, this work demonstrates that the binder is not uniformly distributed in the electrode, but rather resides in local regions. Overall, the results indicate these regions accommodate volume expansion during cycling.

25 ENERGY STORAGE↗

Practical Considerations for Testing Polymer Electrolytes for High-Energy Solid-State Batteries

Polymer electrolytes are an important class of materials in enabling solid-state batteries, which have the potential to exceed 400 Wh/kg energy density. Despite significant advancements in their lithium-ion transport and mechanical properties over the last two decades, the integration and testing of these novel electrolyte materials into functioning cells with the electrode loadings and dimensions required to meet the cell-level energy density goals have been limited. Here, through multiple representative examples, we demonstrate the need of testing in close to practical cell conditions for a faster and more reliable evaluation of polymeric electrolytes. In particular, the need for testing with thin lithium anodes and practical cycling capacities is demonstrated for evaluation of their lithium-metal interfacial stability and dendritic resistance, respectively, and a testing protocol is suggested. The guidelines presented here will also apply to testing of other solid electrolytes for solid-state batteries.

25 ENERGY STORAGE↗

Corrosion Mitigation and Increased Discharge Capacity in Aqueous Processed Thick Cathodes using Phosphoric Acid Additives

Aqueous processed cathodes for lithium-ion batteries are favorable for both cost and environmental reasons; however, these electrodes still face significant problems with increasing areal capacities (i.e. thickness). Highly basic slurry conditions (pH in excess of 12) corrode the current collector surface and evolve hydrogen gas. Consequently, bubbling at the electrode interface causes substantial damage to the dried electrode. As the loading of these electrodes is increased, damage becomes severe and results in lack of adhesion and cohesion. Here introduction of phosphoric acid to combat the rise in pH and suppress the corrosion at the current collector surface is investigated. Phosphoric acid was added in increments of 0.5, 1.0, and 1.5 wt% and the subsequent effects on slurry rheology, particle size, adhesion, and electrochemical cycling were investigated. A technique is reported for obtaining thick (6-8 mAh/cm2) cathodes that exhibit reduced surface cracking and improved rate performance as compared to control samples.

Kukay, Alexander↗

Beneficial rheological properties of lithium-ion battery cathode slurries from elevated mixing and coating temperatures

It is crucial that lithium-ion battery manufacturers implement strategies to expedite production without sacrificing quality due to rising consumer demand. Cathode coating is commonly performed at the industrial scale with a slot-die coater. In slot-die coating, substrate velocity is maximized and imperfections (such as air entrainment and thickness variations) are minimized by reducing the viscosity of the material being coated. A simple, scalable technique of reducing the viscosity of the cathode slurry is to increase its temperature, though it is dire that this heat does not cause irreversible gelation or otherwise deteriorate the slurry constituents. Cathode slurries were prepared at different mixing temperatures between 25 °C and 75 °C and their flow behavior was studied at their mixing temperature. At practical shear rates, the slurry coated at 60 °C was 23% less viscous than that coated at 25 °C, meaning the critical coating speed could be increased by roughly 14% at 60 °C. Between 25 °C and 60 °C, the slurries’ yield stress and equilibrium storage modulus increased monotonically, providing the additional benefit of higher sedimentation resistance of the active materials. To examine the influence of temperature on coating morphology and electrochemical performance, slurries were prepared and coated at 25 °C and 60 °C. Micrographs revealed no superficial differences between coatings. The electrode coated at 60 °C demonstrated comparable capacity retention during long-term cycling and high-rate discharge testing when compared to the electrode coated at 25 °C. The findings of this study indicate that warmer mixing and coating operations serve to maximize cathode productivity, particularly if advancements can be made in industrial-scale electrode drying.

25 ENERGY STORAGE↗

Electrode manufacturing for lithium-ion batteries—Analysis of current and next generation processing

As modern energy storage needs become more demanding, the manufacturing of lithium-ion batteries (LIBs) represents a sizable area of growth of the technology. Specifically, wet processing of electrodes has matured such that it is a commonly employed industrial technique. Despite its widespread acceptance, wet processing of electrodes faces a number of problems, including expensive and dangerous solvent recovery, cut-off waste, coating inconsistencies, and microstructural defects due to the solvent drying process. This review considers each of these issues and discusses which electrode slurry properties should be considered when optimizing wet slurry fabrication. Simultaneously, methods to replace traditional wet processing of electrodes are being extensively researched. Some of these novel electrode manufacturing techniques prioritize solvent minimization, while others emphasize boosting energy and power density by thickening the electrode and, subsequently, creating an organized pore structure to permit faster ion diffusion. This review contemplates the advantages and disadvantages of each of these approaches and provides a comprehensive outlook on the future of electrode manufacturing.

25 ENERGY STORAGE↗