High Thermoelectric Performance through Crystal Symmetry Enhancement in Triply Doped Diamondoid Compound Cu 2 SnSe 3

The presence of high crystallographic symmetry and nanoscale defects are favorable for thermoelectrics. With proper electronic structures, a highly symmetric crystal tends to possess multiple carrier channels and promote electrical conductivity without sacrificing Seebeck coefficient. In addition, nanoscale defects can effectively scatter acoustic phonons to suppress thermal conductivity. Here, we report that the triple doping of Cu 2 SnSe 3 leads to a high ZT value of 1.6 at 823 K for Cu 1.85 Ag 0.15 (Sn 0.88 Ga 0.1 Na 0.02 )Se 3 , and a decent average ZT (ZT ave ) value of 0.7 is also achieved for Cu 1.85 Ag 0.15 (Sn 0.93 Mg 0.06 Na 0.01 )Se 3 from 475 to 823 K. Our study reveals: (1) Ag doping on Cu sites generates numerous point defects and greatly decreases lattice thermal conductivity. (2) Doping Mg or Ga converts the monoclinic Cu 2 SnSe 3 into a cubic structure. This symmetry enhancing leads to increase in the effective mass from 0.8 m e to 2.6 m e (m e , free electron mass) and the power factor from 4.3 μW/cm –1 K –2 for Cu 2 SnSe 3 to 11.6 μW/cm –1 K –2 . (3) Na doping creates dense dislocation arrays and nanoprecipitates, which strengthens the phonon scattering. (4) Pair distribution function analysis shows localized symmetry breakdwon in the cubic Cu 1.85 Ag 0.15 (Sn 0.88 Ga 0.1 Na 0.02 )Se 3 . Furthermore, the present work provides a standpoint to design promising thermoelectric materials by synergistically manipulating crystal symmetry and nanoscale defects.

36 MATERIALS SCIENCE↗

Dimer rattling mode induced low thermal conductivity in an excellent acoustic conductor

A solid with larger sound speeds usually exhibits higher lattice thermal conductivity. Here, we report an exception that CuP2 has a quite large mean sound speed of 4155 m s –1 , comparable to GaAs, but single crystals show very low lattice thermal conductivity of about 4 W m –1 K –1 at room temperature, one order of magnitude smaller than GaAs. To understand such a puzzling thermal transport behavior, we have thoroughly investigated the atomic structures and lattice dynamics by combining neutron scattering techniques with first-principles simulations. This compound crystallizes in a layered structure where Cu atoms forming dimers are sandwiched in between P atomic networks. In this work, we reveal that Cu atomic dimers vibrate as a rattling mode with frequency around 11 meV, which is manifested to be remarkably anharmonic and strongly scatters acoustic phonons to achieve the low lattice thermal conductivity.

36 MATERIALS SCIENCE↗

Direct observation of vast off-stoichiometric defects in single crystalline SnSe

Single crystalline tin selenide (SnSe) recently emerged as a very promising thermoelectric material for waste heat harvesting and thermoelectric cooling, due to its record high figure of merit ZT in mediate temperature range. The most striking feature of SnSe lies in its extremely low lattice thermal conductivity as ascribed to the anisotropic and highly distorted Sn-Se bonds as well as the giant bond anharmonicity by previous studies, yet no theoretical models so far can give a quantitative explanation to such low a lattice thermal conductivity. Here, we presented direct observation of an astonishingly vast number of off-stoichiometric Sn vacancies and Se interstitials, using sophisticated aberration corrected scanning transmission electron microscope; and credited the previously reported ultralow thermal conductivity of the SnSe single crystalline samples partly to their off-stoichiometric feature. In order to further validate the conclusion, we also synthesized stoichiometric SnSe single crystalline samples, and illustrated that the lattice thermal conductivity is deed much higher as compared with the off-stoichiometric single crystals. Finally, the scattering efficiency of individual point defect on heat-carrying phonons was then discussed in the state-of-art Debye-Callaway model.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Grain Boundary Engineering for Achieving High Thermoelectric Performance in n-Type Skutterudites

Grain or phase boundaries play a critical role in the carrier and phonon transport in bulk thermoelectric materials. Previous investigations about controlling boundaries primarily focused on the reducing grain size or forming nanoinclusions. Herein, liquid phase compaction method is first used to fabricate the Yb–filled CoSb 3 with excess Sb content, which shows the typical feature of low–angle grain boundaries with dense dislocation arrays. Seebeck coefficients show a dramatic increase via energy filtering effect through dislocation arrays with little deterioration on the carrier mobility, which significantly enhances the power factor over a broad temperature range with a high room–temperature value around 47 μW cm –2 K –1 . Simultaneously, the lattice thermal conductivity could be further suppressed via scattering phonons via dense dislocation scattering. As a result, the highest average figure of merit ZT of ≈1.08 from 300 to 850 K could be realized, comparable to the best reported result of single or triple–filled Skutterudites. Furthermore, this work clearly points out that low–angle grain boundaries fabricated by liquid phase compaction method could concurrently optimize the electrical and thermal transport properties leading to an obvious enhancement of both power factor and ZT .

36 MATERIALS SCIENCE↗

Integrating Band Structure Engineering with All-Scale Hierarchical Structuring for High Thermoelectric Performance in PbTe System

We investigated PbTe 1-x Se x -2%Na-y%SrTe system and report a high ZT of 2.3 at 923 K for PbTe 0.85 Se 0.15 -2%Na-4%SrTe. This is achieved by performing electronic band structures modifications as well as all-scale hierarchical structuring and combining the two effects. We find that high ZTs in PbTe 0.85 Se 0.15 -2%Na-4%SrTe are possible at all temperature from 300K to 873K with an average ZT ave of 1.23. The high performance in PbTe 1-x Se x -2%Na-y%SrTe could be achieved by either choosing PbTe-2Na-4SrTe or PbTe 0.85 Se 0.15 -2Na as a matrix. At room temperature the carrier mobility shows negligible variations as SrTe fraction is increased, however the lattice thermal conductivity is significantly reduced from ~ 1.1 Wm-1K-1 to ~ 0.82 Wm -1 K -1 when 5.0 % SrTe is added. The lattice thermal conductivity at 923 K decreases from ~ 0.59 Wm-1K-1 to ~ 0.43 Wm -1 K -1 . The power factor maxima of PbTe 1-x Se x -2Na-4SrTe shift systematically to higher temperature with rising Se fractions due to bands divergence. The maximum power factors reach ~ 27 μWcm -1 K -2 , ~ 30 μWcm -1 K -2 , ~ 31 μWcm -1 K -2 for the x = 0, 0.05, and 0.15 samples peak at 473K, 573K and 623K,

36 MATERIALS SCIENCE↗

Electrical and thermal transport properties of layered Bi{sub 2}YO{sub 4}Cu{sub 2}Se{sub 2}

Bi{sub 2}YO{sub 4}Cu{sub 2}Se{sub 2} possesses a low thermal conductivity and high electrical conductivity at room temperature, which was considered as a potential thermoelectric material. In this work, we have investigated the electrical and thermal transport properties of Bi{sub 2}YO{sub 4}Cu{sub 2}Se{sub 2} system in the temperature range from 300 K to 873 K. We found that the total thermal conductivity decreases from ~1.8 W m{sup −1} K{sup −1} to ~0.9 W m{sup −1} K{sup −1}, and the electrical conductivity decreases from ~850 S/cm to ~163 S/cm in the measured temperature range. To investigate how potential of Bi{sub 2}YO{sub 4}Cu{sub 2}Se{sub 2} system, we prepared the heavily Iodine doped samples to counter-dope intrinsically high carrier concentration and improve the electrical transport properties. Interestingly, the Seebeck coefficient could be enhanced to ~+80 μV/K at 873 K, meanwhile, we found that a low thermal conductivity of ~0.7 W m{sup −1} K{sup −1} could be achieved. The intrinsically low thermal conductivity in this system is related to the low elastic properties, such as Young's modulus of 70–72 GPa, and Grüneisen parameters of 1.55–1.71. The low thermal conductivity makes Bi{sub 2}YO{sub 4}Cu{sub 2}Se{sub 2} system to be a potential thermoelectric material, the ZT value ~0.06 at 873 K was obtained, a higher performance is expected by optimizing electrical transport properties through selecting suitable dopants, modifying band structures or by further reducing thermal conductivity through nanostructuring etc. - Highlights: • The total thermal conductivity decreases from 1.8 to 0.9 Wm{sup –1}K{sup –1} at 300–873K. • The electrical conductivity decreased from 850 to 163 S/cm at 300–873K. • The Seebeck coefficients were enhanced through heavily Iodine doping. • The ZT ~0.06 at 873K suggests that Bi{sub 2}YO{sub 4}Cu{sub 2}Se{sub 2} systems are potential thermoelectrical materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synergistically optimized electrical and thermal transport properties of SnTe via alloying high-solubility MnTe

Lead chalcogenides are the most efficient thermoelectric materials. In comparison, SnTe, a lead-free analogue of PbTe, exhibits inferior thermoelectric performance due to low Seebeck coefficient and high thermal conductivity. In this report, we show that we can synergistically optimize the electrical and thermal transport properties of SnTe via alloying Mn. Further, we report that the introduction of Mn (0–50%) induces multiple effects on the band structure and microstructure of SnTe: for the former, it can tune the Fermi level and promote the convergence of the two valence bands, concurrently enhancing the Seebeck coefficient; for the latter, it can profoundly modify the microstructure into an all-scale hierarchical architecture (including nanoscale precipitates/MnTe laminates, stacking faults, layered structure, atomic-scale point defects, etc.) to scatter phonons with a broad range of mean free paths, strongly reducing the lattice thermal conductivity. Meanwhile, most significantly, the Mn alloying enlarges the energy gap of the conduction band (C band) and the light valence band (L band), thereby suppressing the bipolar thermal conductivity by increasing the band gap. The integration of these effects yields a high ZT of 1.3 at 900 K for 17% Mn alloyed SnTe.

36 MATERIALS SCIENCE↗

Superior thermoelectric performance in PbTe-PbS pseudo-binary. Extremely low thermal conductivity and modulated carrier concentration

Lead chalcogenides have exhibited their irreplaceable role as thermoelectric materials at the medium temperature range, owing to highly degenerate electronic bands and intrinsically low thermal conductivities. PbTe-PbS pseudo-binary has been paid extensive attentions due to the even lower thermal conductivity which originates largely from the coexistence of both alloying and phase-separated precipitations. To investigate the competition between alloying and phase separation and its pronounced effect on the thermoelectric performance in PbTe-PbS, we systematically studied Spark Plasma Sintered (SPSed), 3 at% Na- doped (PbTe) 1-x (PbS)x samples with x=10%, 15%, 20%, 25%, 30% and 35% by means of transmission electron microscopy (TEM) observations and theoretical calculations. Corresponding to the lowest lattice thermal conductivity as a result of the balance between point defect- and precipitates- scattering, the highest figure of merit ZT~2.3 was obtained at 923 K when PbS phase fraction x is at 20%. The consistently lower lattice thermal conductivities in SPSed samples compared with corresponding ingots, resulting from the powdering and follow-up consolidation processes, also contribute to the observed superior ZT. Notably, the onset of carrier concentration modulation ~600 K due to excessive Na’s diffusion and re-dissolution leads to the observed saturations of electrical transport properties, which is believed equally crucial to the outstanding thermoelectric performance of SPSed PbTe-PbS samples.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗