Search NASA⌕ Search

Engineering topics

Hnatowicz, V

Publications and source records attributed to Hnatowicz, V.

The Energy Loss of Li and C Ions with MeV Energies in the Polycarbonate and Polypropylene

Stopping power and straggling of Li ions and C ions at mean energy 3.8-5.4 MeV and 5.6-6.9 MeV, respectively, in polycarbonate (PC) and at mean energy 3.7-5.2 MeV and 6.8-8.0 MeV in polypropylene (PP) foils have been measured using ion beams from a Tandetron 4130 MC accelerator. The ions scattered from a thin, primary gold target were registered by a surface barrier detector partially covered with a thin foil of the investigated polymer. The stopping power was determined from the energy difference between the signals from the ions directly backscattered from the Au layer and the ions backscattered and slowed down in the foil. The foil thickness was determined by the weighing procedure. The experimentally determined stopping powers were compared with those calculated with the SRIM 2010 code. The measured stopping powers are in good agreement for Li and C in PC, the differences being within 0.1-1.6% for Li and 0.2-2.1% for C. For Li and C in PP, the stopping powers are lower than the calculated ones, the differences being within 0.5-2.8% for Li and 3.6-6.1% for C. The energy straggling was determined from the width of the RBS signals. The experimentally determined energy straggling was found to fluctuate around the values calculated according to Bohr theory.

36 MATERIALS SCIENCE↗

Hybridization and Modification of the Ni/C{sub 60} Composites

Hybridization and thermal evolution of the Ni+C{sub 60} composites, deposited on Si(001) at room temperature, were studied using Scanning Electron Microscopy, {mu}-Raman spectroscopy and Rutherford Backscattering. As-deposited, the hybrid films exhibited a granular nano-structure with Ni nano-particles encapsulated in C{sub 60} polymerized rinds. The Ni and C (C{sub 60}) distributions in a top layer were found homogeneous with a stable Ni/C (C{sub 60}) ratio; in the larger depth the distributions were inhomogeneous and their ratio dramatically varied. At elevated temperatures, all structural parameters were changed. In the subsurface layer Ni- and C (C{sub 60})-rich zones were formed (due to the induced phase separation), C{sub 60}-molecules decayed and their fragments were transformed into amorphous carbon (a-C). The free volume distribution of the stressed hybrid matter was analyzed by the Hg marker that (in a form of vapors) in-diffused in to the samples. The RBS analysis showed that the Hg distribution of the as-deposited films followed the character of distribution of the C (C{sub 60}) component. At elevated temperatures, however, the Hg profiles decreased dramatically (especially in the subsurface layer) suggesting a significant drop-off of the free volume concentration due to the formation of the spatially compact a-C clusters.

36 MATERIALS SCIENCE↗

On Boron Diffusion in MgF{sub 2}

The MgF{sub 2} monocrystals were irradiated at room temperature with 390 keV B{sup +} ions up to the fluence of 10{sup 16} cm{sup -2}. The irradiated samples were (isochronally and isothermally) annealed in high vacuum at the temperatures 200 deg. C, 300 deg. C, 400 deg. C, 500 deg. C, 600 deg. C and 700 deg. C for the times ranging from 2-100 hours. After each annealing step, the boron depth distribution was determined using the neutron depth profiling technique. As implanted, the depth distributions of boron exhibited standard Gaussian-like forms, but the evaluated profile parameters, R{sub P} = 960 nm and {delta}R{sub P} = 140 nm, were higher than those calculated using the SRIM code (R{sub P} = 870 nm and {delta}R{sub P} = 115 nm). Annealing at temperatures up to 400 deg. C did not change the depth profiles. Annealing at 600 deg. C, however, led to a one-way gradual transfer of the boron atoms from the site of implantation towards the sample surface, and in this way a bimodal profile was created. The amount of boron atoms, transferred to the sample surface, was an increasing function of the annealing time. After annealing at 700 deg. C for 64 hours the bimodal profile collapsed into a single broad distribution, extending from the sample surface up to the implantation depth. The observed phenomena clearly points out the stability of the as-implanted boron depth profiles at lower annealing temperatures. Thermal annealing above 600 deg. C, however, liberates boron atoms, which then predominantly migrate from the implantation site towards the sample surface, where they are captured on some unspecified surface defects.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗