Effective passivation of In{sub 0.2}Ga{sub 0.8}As by HfO{sub 2} surpassing Al{sub 2}O{sub 3} via in-situ atomic layer deposition
High {kappa} gate dielectrics of HfO{sub 2} and Al{sub 2}O{sub 3} were deposited on molecular beam epitaxy-grown In{sub 0.2}Ga{sub 0.8}As pristine surface using in-situ atomic-layer-deposition (ALD) without any surface treatment or passivation layer. The ALD-HfO{sub 2}/p-In{sub 0.2}Ga{sub 0.8}As interface showed notable reduction in the interfacial density of states (D{sub it}), deduced from quasi-static capacitance-voltage and conductance-voltage (G-V) at room temperature and 100 Degree-Sign C. More significantly, the midgap peak commonly observed in the D{sub it}(E) of ALD-oxides/In{sub 0.2}Ga{sub 0.8}As is now greatly diminished. The midgap D{sub it} value decreases from {>=}15 Multiplication-Sign 10{sup 12} eV{sup -1} cm{sup -2} for ALD-Al{sub 2}O{sub 3} to {approx}2-4 Multiplication-Sign 10{sup 12} eV{sup -1} cm{sup -2} for ALD-HfO{sub 2}. Further, thermal stability at 850 Degree-Sign C was achieved in the HfO{sub 2}/In{sub 0.2}Ga{sub 0.8}As, whereas C-V characteristics of Al{sub 2}O{sub 3}/p-In{sub 0.2}Ga{sub 0.8}As degraded after the high temperature annealing. From in-situ x-ray photoelectron spectra, the AsO{sub x}, which is not the oxidized state from the native oxide, but is an induced state from adsorption of trimethylaluminum and H{sub 2}O, was found at the ALD-Al{sub 2}O{sub 3}/In{sub 0.2}Ga{sub 0.8}As interface, while that was not detected at the ALD-HfO{sub 2}/In{sub 0.2}Ga{sub 0.8}As interface.