Engineering topics
Hsiao, B
Publications and source records attributed to Hsiao, B.
Development of Internal Fine Structure in Stretched Rubber Vulcanizates
Small-angle X-ray scattering (SAXS) pattern and tensile stress during relaxation of stretched rubber vulcanizates (synthetic polyisoprene) were measured simultaneously at room temperature and at 0 C. The samples were quickly stretched to the prefixed strain and then allowed to relax for 1 h. In every SAXS pattern, the intensity distribution was elongated along the equator, indicating the formation of structures elongated in the stretching direction. The so-called two-spots pattern corresponding to the long period of stacked lamellar crystals did not appear even when the critical strain to induce crystallization was exceeded. On the other hand, even below the critical strain, additional development of equatorial streaks was detected in the differential SAXS patterns. This result suggests the growth of the density fluctuation elongated in the stretching direction, which is not directly related to strain-induced crystallization.
Synchrotron X-ray Scattering Analysis of the Interaction Between Corn Starch and an Exogenous Lipid During Hydrothermal Treatment
Lipids have an important effect on starch physicochemical properties. There exist few reports about the effect of exogenous lipids on native corn starch structural properties. In this work, a study of the morphological, structural and thermal properties of native corn starch with L-alpha-lysophosphatidylcholine (LPC, the main phospholipid in corn) was performed under an excess of water. Synchrotron radiation, in the form of real-time small and wide-angle X-ray scattering (SAXS/WAXS), was used in order to track structural changes in corn starch, in the presence of LPC during a heating process from 30 to 85 C. When adding LCP, water absorption decreased within starch granule amorphous regions during gelatinization. This is explained by crystallization of the amylose-LPC inclusion complex during gelatinization, which promotes starch granule thermal stability at up to 95 C. Finally, a conceptual model is proposed for explaining the formation mechanism of the starch-LPC complex.
Rupture Orientation and Strain-induced Crystallization of Polymer Chain and Network in Vulcanized Polyisoprene During Uniaxial Deformation by in-situ Electron Spin Resonance(ESR) and Synchrotron X-ray Analysis
Different network structures of vulcanized polyisoprene rubbers were studied by in-situ ESR and synchrotron X-ray during deformation to analyze the rupture, orientation, and strain-induced crystallization of polymer chains and network points. Rupture of network points occur, depending on network structure, and create an un-reversible change in vulcanized rubber. The flexibility of network points affects the possibility of rupture, polymer orientation and strain-induced crystallization. Peroxide vulcanized network is rigid and un-rupturable. Poly-sulfide rich vulcanized network is more flexible and less rupturable than mono-sulfide rich vulcanized network. Chain flexibility and rupturability of network points affect the strain-induced crystallization and stress-strain relation.
Thin-film Nanofibrous Composite Membranes Containing Cellulose or Chitin Barrier Layers Fabricated by Ionic Liquids
The barrier layer of high-flux ultrafiltration (UF) thin-film nanofibrous composite (TFNC) membranes for purification of wastewater (e.g., bilge water) have been prepared by using cellulose, chitin, and a cellulose-chitin blend, regenerated from an ionic liquid. The structures and properties of regenerated cellulose, chitin, and a cellulose-chitin blend were analyzed with thermogravimetric analysis (TGA) and wide-angle X-ray diffraction (WAXD). The surface morphology, pore size and pore size distribution of TFNC membranes were determined by SEM images and molecular weight cut-off (MWCO) methods. An oil/water emulsion, a model of bilge water, was used as the feed solution, and the permeation flux and rejection ratio of the membranes were investigated. TFNC membranes based on the cellulose-chitin blend exhibited 10 times higher permeation flux when compared with a commercial UF membrane (PAN10, Sepro) with a similar rejection ratio after filtration over a time period of up to 100 h, implying the practical feasibility of such membranes for UF applications.
An In-situ X-ray Scattering Study During Uniaxial Stretching of Ionic Liquid/Ultra-high Molecular Weight Polyethylene Blends
An ionic liquid (IL) 1-docosanyl-3-methylimidazolium bromide was incorporated into ultra-high molecular weight polyethylene (UHMWPE) and formed IL/UHMWPE blends by solution mixing. The structure evolution of these blends during uniaxial stretching was followed by in-situ synchrotron wide-angle X-ray diffraction (WAXD) and small-angle X-ray scattering (SAXS) techniques. During deformation at room temperature, deformation-induced phase transformation from orthorhombic to monoclinic phase was observed in both IL/UHMWPE blends and neat UHMWPE. The elongation-to-break ratios of IL/UHMWPE blends were found to increase by 2-3 times compared with that of pure UHMWPE, while the tensile strength remained about the same. In contrast, during deformation at high temperature (120 C), no phase transformation was observed. However, the blend samples showed much better toughness, higher crystal orientation and higher tilting extent of lamellar structure at high strains.
Suppressing the Skin-Core Structure of Injection-Molded Isotactic Polypropylene via Combination of an in situ Microfibrillar Network and an Interfacial Compatibilizer
Injection-molded semicrystalline polymer parts generally exhibited a so-called skin-core structure basically as a result of the large gradients of temperature, shear rate, stress, and pressure fields created by the boundary conditions of injection molding. Suppression of the skin-core structure is a long-term practical challenge. In the current work, the skin-core structure of the conventional injection-molded isotactic polypropylene (iPP) was largely relieved by the cooperative effects of an in situ microfibrillar network and interfacial compatibilizer. The in situ poly(ethylene terephthalate) microfibrils of 1-8 {micro}m in diameter and large aspect ratios of above 40 tended to entangle with each other to generate a microfibrillar network in the iPP melt. During injection molding, the iPP molecules experienced confined flow in the microchannels or pores formed by the microfibrillar network, which could redistribute and homogenize the flow field of polymer melt. Addition of the compatibilizer, glycidyl methacrylate-grafted iPP, restrained the molecular orientation but facilitated preservation of oriented molecules due to the chemical bonds at the interface between PET microfibrils and iPP. The cooperative effects of in situ microfibrillar network and interfacial compatibilizer led to almost the same molecular orientation across the whole thickness of the injection-molded parts. Additionally, the content of {beta} crystals in different layers of injection-molded iPP parts depended on the combined effects of the molecular orientation, the amount of oriented crystals, and the crystallization time between 105 and 140 C. The presence of the interfacial compatibilizer facilitated formation of the {beta} crystals because of preservation of the oriented molecules.
Wide-Angle X-ray Scattering Study on Shear-Induced Crystallization of Propylene-1-Butylene Random Copolymer: Experiment and Diffraction Pattern Simulation
Shear-induced crystallization of a propylene-1-butylene random copolymer with low butylene content (5.7 mol %) was studied using time-resolved wide-angle X-ray scattering (WAXS) techniques. Polymorphism, preferred crystal orientation, crystallization kinetics, and disorder effect were investigated based on WAXS 2D whole pattern analysis. It was found that at 100 C, the crystallite of P-B copolymer was a mixture of 80% {gamma}-form and 20% {alpha}-form of isotactic polypropylene (iPP) crystals. The application of a step shear (shear rate = 100 s{sup -1}, shear duration =3s) induced {gamma}-form crystals with c-axis oriented perpendicular to the shear direction. In contrast, the c-axis of {alpha}-form crystals was normally in parallel to the shear direction. Both crystallization kinetics and crystallinity were greatly enhanced by shear. The disorder effect was found to play an important role in the crystallization behavior of P-B copolymer. In the early stage crystallization, the chosen copolymer contained a large amount of structure defects, where crystals became more ordered upon annealing. The degree of crystal orientation was also found to decrease during crystallization due to the relaxation after shear.
Graphene Nanosheets and Shear Flow Induced Crystallization in Isotactic Polypropylene Nanocomposites
Combined effects of graphene nanosheets (GNSs) and shear flow on the crystallization behavior of isotactic polypropylene (iPP) were investigated by in-situ synchrotron wide-angle X-ray diffraction (WAXD) and small-angle X-ray scattering (SAXS) techniques. For crystallization under quiescent condition (at 145 C), the half-crystallization time (t{sub 1/2}) of nanocomposites containing 0.05 and 0.1 wt % GNSs was reduced to at least 50% compared to that of neat iPP, indicating the high nucleation ability of GNSs. The crystallization rate of iPP was directly proportional to the GNS content. Under a relatively weak shear flow (at a rate of 20 s{sup -1} for 5 s duration) and a low degree of supercooling, the neat iPP exhibited an isotropic structure due to the relaxation of row nuclei. However, visible antisotropic crystals appeared in sheared iPP/GNSs nanocomposites, indicating that GNSs induced a network structure hindering the mobility of iPP chains and allowing the survival of oriented row nuclei for a long period of time. The presence of GNSs clearly enhanced the effects of shear-induced nucleation as well as orientation of iPP crystals. Two kinds of nucleating origins coexisted in the sheared nanocomposite melt: heterogeneous nucleating sites initiated by GNSs and homogeneous nucleating sites (row nuclei) induced by shear. The difference of t{sub 1/2} of nanocomposites with and without shear was significantly larger than that of neat iPP. The presence of GNSs and shear flow exhibited a synergistic interaction on promoting crystallization kinetics of iPP, although the effect of GNS concentration was not apparent. From WAXD results of isothermal and nonisothermal crystallization of sheared iPP, it was found that the appearance of {beta}-crystals depended on the preservation of row nuclei, where the {alpha}-crystals were predominant in the iPP/GNSs nanocomposites, indicating that GNSs could directly induce {alpha}-crystals of iPP.
Real-Time Structure Changes during Uniaxial Stretching of Poly (omega-pentadecalactone) by in Situ Synchrotron WAXD/SAXS Techniques
Poly({omega}-pentadecalactone) (PPDL), a model polymer in the poly({omega}-hydroxyl fatty acids) family, is a new biopolymer with monomer synthesized by yeast-catalyzed {omega}-hydroxylation of fatty acids. In this study, deformation-induced structural changes in two PPDL samples with different molecular weights were studied by in situ wide-angle X-ray diffraction (WAXD) and small-angle X-ray scattering (SAXS) techniques. The high molecular weight PPDL (PPDL-high) sample exhibited notable strain hardening, while the low molecular weight PPDL (PPDL-low) sample did not. The behavior can be explained by the entanglement density concept. The evolution of crystallinity (from WAXD) as a function of strain could be divided into four distinct regions, but their respective mechanisms differ slightly in each sample. During stretching, a mesomorphic phase formed in both samples, bridging between the amorphous and strain-induced crystal phases. The SAXS data verified the effect of molecular weight (or the entanglement density) on the deformation-induced structure of PPDL. The parameters of chain orientation factor (f) calculated from the orthorhombic crystal cell as well as the nonorthorhombic crystal cell proposed by Wilchinsky were used to follow the orientation process during stretching of PPDLs. It was found that the different molecular entanglement network (i.e., PPDL-low versus PPDL-high) led to different crystal orientation behavior, especially in the low strain range.
Characterization of Nanoclay Orientation in Polymer Nanocomposite Film by Small-angle X-ray Scattering
The orientation distribution of layer-shaped nanoclays (e.g. organoclays and pristine clays) dispersed in a polymer matrix is an important parameter to control the properties of polymer nanocomposites. In this study, we demonstrate that the use of multi-directional 2-D small-angleX-rayscattering (SAXS) can quantitatively describe the orientation distribution of organoclays (e.g. Cloisite C20A) in melt-pressed nanocompositefilms, containing ethylene-vinyl acetate (EVA) copolymers as polymer matrices. Different weight fractions of organoclays were used to alter the orientation profile of nanocompositefilms, in which the dispersion and morphology of organoclays were also characterized by complementary 2-D and 3-D transmission electron microscopy (TEM). All nanocomposites exhibited mixed intercalation/exfoliation clay morphology, where the intercalated structure possessed partial orientation parallel to the in-plane direction of the film. The higher content of the clay loading showed a higher clay orientation. A simple analytical scheme for SAXS data analysis to determine the orientation parameter (P{sub 2}) was demonstrated, the results of which are in agreement with the gas permeation properties of the nanocompositefilms.
Phase Behavior of Neat Triblock Copolymers and Copolymer/Homopolymer Blends Near Network Phase Windows
The phase behavior of poly(isoprene-b-styrene-b-methyl methacrylate) (ISM) copolymers near the styrene-rich network phase window was examined through the use of neat triblock copolymers and copolymer/homopolymer blends. Both end-block and middle-block blending protocols were employed using poly(isoprene) (PI), poly(methyl methacrylate) (PMMA), and poly(styrene) (PS) homopolymers. Blended specimens exhibited phase transformations to well-ordered nanostructures (at homopolymer loadings up to 26 vol % of the total blend volume). Morphological consistency between neat and blended specimens was established at various locations in the ISM phase space. Copolymer/homopolymer blending permitted the refinement of lamellar, hexagonally packed cylinder, and disordered melt phase boundaries as well as the identification of double gyroid (Q{sup 230}), alternating gyroid (Q{sup 214}), and orthorhombic (O{sup 70}) network regimes. Additionally, the experimental phase diagram exhibited similar trends to those found in a theoretical ABC triblock copolymer phase diagram with symmetric interactions and statistical segments lengths generated by Tyler et al.