Search NASA⌕ Search

Engineering topics

Hu, J. S.

Publications and source records attributed to Hu, J. S..

At least 19 records

Recent progress in the development of liquid metal plasma facing components for magnetic fusion devices

One of the most critical challenges for future fusion reactors is to develop longevity plasma-facing components (PFCs) exposed to extremely high heat and neutron loads. As opposed to those employing solid metals, PFCs with flowing liquid metals (LM) have shown self-healing, heat removal and good impurity control capabilities, all essential to fusion devices. Recently, significant progress in LM-PFC development has been reported globally, with data from several magnetic fusion devices. These studies reveal that LM-PFCs can endure extreme heat fluxes while maintaining plasma compatibility. New design concepts have been proposed and numerically analyzed, advancing models for liquid PFCs in future reactors. Despite existing technical challenges, these developments suggest that LM-PFCs hold promise for future fusion applications.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Deuterium recycling and wall retention characteristics during boron powder injection in EAST

Boron (B), as a low-Z material, is widely employed for wall conditioning to enhance plasma performance in fusion devices. In the Experimental Advanced Superconducting Tokamak, a series of experiments involving real-time B powder injection has been conducted to investigate fuel particle behavior. It was observed that fuel particle recycling decreased with an increase in the amount of B powder injected, resulting in an increase in short-term fuel retention. The fuel recycling decreased by up to 80%, as indicated by divertor neutral pressure and D α line emission. Furthermore, each B atom exhibited a trapping capacity of 0.3 D particles during B powder injection at a typical flow rate. The real-time B injection had no wall hysteresis effect on D retention, implying that cumulative B injection and deposited film did not affect long-term D retention. The possible mechanism for D retention is the formation of B-C-O-D compounds and co-deposition between B and D particles during discharges. This investigation would be valuable for evaluating T retention when B is used as wall conditioning material in future fusion reactor devices.

36 MATERIALS SCIENCE↗

First results of Ne shattered pellet injection for mitigating plasma disruption with full metal wall in EAST tokamak

Disruption mitigation poses a significant and unresolved challenge for ITER and future fusion reactor devices. To mitigate the effect of plasma disruption, a Shattered Pellet Injection (SPI) system has been developed and the first rapid shutdown experiments have been successfully performed in the Experimental Advanced Superconducting Tokamak with full metal wall. The experiments confirmed the system’s capability to inject 5 mm diameter neon (Ne) pellets at velocities ranging from 100 to 400 m s −1 , with a maximum injected quantity of 13.2 Pa m 3 . Compared to unmitigated disruptions, the total radiation power was significantly higher with the respective use of SPI and Massive Gas Injection (MGI). Additionally, the radiation distribution and divertor heat flux were compared between SPI and MGI methods. The results demonstrated that SPI exhibited shorter cooling time, stronger core radiation and more uniform poloidal radiation distribution compared to MGI, indicating deeper deposition using SPI. Furthermore, during plasma shutdown, the electron temperature and peak heat flux near outer divertor strike points were reduced by 40% and 50% respectively, with SPI, in comparison to MGI. These findings serve as a valuable reference for implementing SPI technology as the baseline approach for disruption mitigation in ITER.

EAST↗

Long-pulse high-performance H-mode plasmas achieved on EAST

A record duration of a 310 s H-mode plasma (H 98y2 ~ 1.3, n e /n GW ~ 0.7, f BS > 50%) has been recently achieved on experimental advanced superconducting tokamak (EAST) with metal walls, exploiting the device's improved long-pulse capabilities. The experiment demonstrates good control of tungsten concentration, core/edge MHD stability, and particle and heat exhaust with an ITER-like tungsten divertor and zero injected torque, establishing a milestone on the path to steady-state long-pulse high-performance scenarios in support of ITER and CFETR. Important synergistic effects are leveraged toward this result, which relies purely on radio frequency (RF) powers for heating and current drive (H&CD). On-axis electron cyclotron heating enhances the H&CD efficiency from lower hybrid wave injection, increasing confinement quality and enabling fully non-inductive operation at high density (n e /n GW ~ 70%) and high poloidal beta (β P ~ 2.5). A small-amplitude grassy edge localized mode regime facilitates the RF power coupling to the H-mode edge and reduces divertor sputtering/erosion. The high energy confinement quality (H 98y2 ~ 1.3) is achieved with the experimental and simulated results pointing to the strong effect of Shafranov shift on turbulence. Transport analysis suggests that trapped electron modes dominate in the core region during the record discharge. The detailed physics processes (RF synergy, core-edge integration, confinement properties, etc.) of the steady-state operation will be illustrated in the content. In the future, EAST will aim at accessing more relevant dimensionless parameters to develop long-pulse high-performance plasma toward ITER and CFETR steady-state advanced operation.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

A review of lithium application for the plasma-facing material in EAST Tokamak

As a low-Z material, lithium is widely tested and used in tokamak devices for particle recycling and impurity control to improve plasma performance. Lithium application as plasma-facing materials via different methods, such as coating, injection and flowing liquid limiter, has been investigated more than 10 years on EAST. This study presents the development of the lithium techniques applied on EAST, and reviews the progresses on the investigation of its interaction with plasma and its effects on the improvement on the plasma performances. In addition, this paper further discusses the potential applications of lithium technique in future fusion devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Active wall conditioning through boron powder injection compatible $\mathrm{ELM}$ control in $\mathrm{EAST}$

Real-time wall conditioning and edge-localized mode (ELM) suppression through real-time boron powder injection into high-confinement mode discharges of the Experimental Advanced Superconducting Tokamak (EAST) have been investigated. The boron powder injection effectively conditioned the plasma-facing components, as shown by the reductions in low-Z and high-Z impurities and the global recycling level in the whole inner vessel, and suppressed the strong magnetohydrodynamic (MHD) activity in the plasma core. The improved wall conditions also resulted in an earlier transition from L- to H-mode. Boron powder injection also effectively suppressed ELM in the lower single null configuration with BT in the favorable direction while leaving the plasma density and stored energy largely unaffected.

36 MATERIALS SCIENCE↗

Corrosion characteristics of Mo and TZM alloy for plasma facing components in molten lithium at 623 K

Here, in this study, the corrosion behaviours of molybdenum (Mo) and a Mo-based alloy (TZM) were investigated using a static immersion corrosion technique. Weight loss, surface microstructure, and corrosion depth of Mo and the TZM alloy were correlated with elements. The compatibility of Mo and the TZM alloy in static liquid Li was suitable. Mo demonstrated uniform corrosion with a homogenous dissolution of free C and Mo, and TZM alloy exhibited a nonuniform corrosion behaviour with a preferential grain boundary attack caused by the selective dissolution of free C, Ti, and Zr. When the surface oxidation layer of the samples was consumed, free C from Mo and TZM diffused into molten Li to form Li 2 C 2 and then was captured by Zr, Ti, and Mo to form thermodynamically stable carbides, which resulted in the enrichment of the C layer near the sample surfaces. In addition, Ti and Zr acted as N-trappers in liquid Li; the formation of Zr and Ti nitrides resulted in the enrichment of N, Ti, and Zr elements on the surface and led to TZM corrosion increase. Thus, Zr and Ti depletion, pitting, and grain boundary corrosion were problematic for TZM under long-term exposure to liquid Li. Reducing the content of free C and nonmetallic N and increasing the amount of Ti and Zr carbides on the surface of and inside the raw TZM alloy helped improve the corrosion resistance of TZM in liquid Li.

36 MATERIALS SCIENCE↗

Comparison of active impurity control between lithium and boron powder real-time injection in EAST

The lithium and boron powder have been successfully real-time injected into Experimental Advanced Superconducting Tokamak (EAST) high-confinement (H-) mode discharges, showing good wall conditioning effects, especially on the impurities control. Both of lithium and boron powder particles are gravitationally accelerated into the upper edge of a upper single null discharge. The lithium powder real-time injection effectively reduced the tungsten impurity content both in the plasma edge and core. Contrary to the lithium injection, the boron injection mainly reduced the impurities content in the plasma core, while the impurities increased in the edge. Furthermore, this mainly due to that there was an edge harmonic mode stimulated by boron injection, providing sufficient particles transport. Moreover, the impurities control through boron injection has much wider operation windows than lithium powder injection. Furthermore, there was accumulative wall conditioning effects after sequential boron powder injection discharges.

36 MATERIALS SCIENCE↗

Enhancement of edge turbulence concomitant with ELM suppression during boron powder injection in EAST

A reproducible, quasi-stationary edge localized mode (ELM)-suppressed scenario was obtained over a wide range of plasma parameters by continuous injection of boron (B) powder into an upper-single null discharge in the experimental advanced superconducting tokamak [Sun et al., Nucl. Fusion 61, 014002 (2021)]. This powder-induced ELM-absent regime is associated with an edge harmonic mode (EHM) that provides continuous particle exhaust to maintain constant density without confinement degradation and impurity accumulation, the latter of which is often observed in ELM-free regimes. A flow rate threshold of B powder injection, leading to a threshold intensity of the EHM, is necessary for full ELM suppression. The fundamental harmonic of the EHM exhibits a toroidal mode number n = 1. The mode is observable in the entire poloidal cross section with a peak near the upper X-point in an upper-single null configuration. Here, the EHM spans radially across the pedestal and scrape-off layer, peaking inside the separatrix. The EHM appears to be insensitive to q 95 , heating power, plasma toroidal rotation, and pedestal collisionality.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Progress of Divertor Heat and Particle Flux Control in EAST for Advanced Steady-State Operation in the Last 10 Years

Active control of the excessively high heat and particle fluxes on the divertor target plates is of fundamental importance to the steady state operation of tokamaks, especially for fusion reactors. A series of experiments have been carried out on this critical issue to relieve the plasma-wall interactions in the experimental advanced superconducting tokamak (EAST) in the last ten years, not only contributing to the long pulse operation of EAST itself, but also providing physical understandings and potential techniques to the next-generation devices like ITER. Here we have characterized the power deposition pattern and broadened the divertor footprint width effectively. The plasma-wetted area is actively handled using either 3-dimentional edge magnetic topology or advanced plasma equilibrium, thereby peak heat flux around the strike point is reduced. Active control of detachment or radiation compatible with core plasma performance has progressed significantly in very recent years, with a series of active feedback control modules developed and utilized successfully, based on the divertor physics advances with both experiments and simulation. The upper divertor of EAST was upgraded from graphite to active water-cooling ITER-like tungsten in 2014, exhibiting much enhanced heat removal capability. As for the particle exhaust including both fueling and impurity particles, in addition to wall conditioning and impurity source control, the efficiency of particle flux exhaust is optimized by making full use of the divertor closure and the plasma drifts in both scrape-off layer and divertor volume. These heat and particle exhaust advances contribute greatly to a series of EAST achievements like H-mode operation over 100 s. A brief near-term plan on the integrated control of divertor plasma-wall interactions in long-time scale will also be introduced, aiming to provide favorable divertor operation solution for ITER and CFETR.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Suppression of edge localized modes with real-time boron injection using the tungsten divertor in EAST

We report an observation of robust suppression of edge-localized modes (ELMs) in the Experimental Advanced Superconducting Tokamak (EAST), enabled by continuous boron (B) powder injection. Edge harmonic oscillations appear during B powder injection, providing sufficient particle transport to maintain constant density and avoid impurity accumulation in ELM-stable plasmas. Here, quasi-steady ELM suppression discharges are demonstrated with modest energy confinement improvement and over a wide range of conditions: heating power and technique variation, electron density range over a factor ~3.5, deuterium or helium ion species, and with either direction of the toroidal magnetic field. ELM suppression is observed above a threshold edge B intensity and ceases within 0.5 s of termination of the B injection. In contrast to ELM suppression accompanied by recycling reduction during Li powder injection in NSTX and EAST (Maingi et al 2018 Nucl. Fusion 58 024003), reduced recycling due to hydrogenic species retention is unnecessary for the ELM suppression with B powder injection, paving the way for its consideration as an ELM control tool for future fusion devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Deuterium retention characteristics in Li film by coating and during flowing liquid Li limiter operation in experimental advanced superconducting tokamak

Lithium (Li) is a promising low-Z material for particle recycling and impurity control to improve plasma performance in fusion devices. In the experimental advanced superconducting tokamak (EAST), Li coating has become a routine method for wall conditioning, and a flowing liquid Li (FLiLi) limiter has been successfully tested several times. Deuterium retention characteristics in the Li film coated on the international thermonuclear experimental reactor-like tungsten divertor and FLiLi during plasma discharges, which is important for the utilization of Li in future fusion devices, were investigated in EAST. It is found that the absorption of the fuel particles by Li coatings decreases gradually, and recycling gradually increases over a series of discharges. The maximum net amount of deuterium retained reached ~0.8 g, corresponding to 12% deuterium in the Li. Furthermore, this corresponds to a whole day's worth of shots with a total of 87 plasma discharges and a total of ~640s plasma time after 11.75 g Li was deposited. Compared to the Li coating, it is shown that FLiLi continuously traps fuel particles and achieves a higher deuterium retention ratio over both the short- and long-term, leading to lower recycling. Meanwhile, it is also observed that the fuel particle retention ratio increases when FLiLi is closer to the plasma. This result is likely due to higher plasma heating power and limiter temperature, which cause an increased Li efflux from FLiLi due to a higher limiter temperature, which then redeposits on the other plasma-facing surfaces and increases fuel particle absorption. It is estimated that ≥ 80% of the retained D particles are captured by the continual renewal of the Li redeposition film during the FLiLi operation. This investigation would also be useful for D/T retention in future fusion devices if Li is used as a plasma-facing component.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Lithium splashing from flowing liquid lithium limiter and its effect on high confinement plasma performance in EAST tokamak

To study the potential applications of liquid lithium (Li) as plasma facing material, the third generation of flowing liquid Li (FLiLi) limiter has been designed and successfully tested in EAST tokamak H-mode discharges in the 2018 run campaign. Here, the stability of liquid Li on FLiLi surface, and Li splashing and its effect on the plasma performance are investigated in detail. Li splashing was observed in L-mode and H-mode discharges due to Rayleigh-Taylor (R-T) instability, resulting from electromagnetic forces J → x B → . Li splashing in low-parameter plasma decreased both core and edge electron temperatures, resulting in the degradation of plasma energy confinement and even H-L back transition, however, it almost did not influence plasma confinement performance in high-parameter plasma. These findings indicate that high-parameter plasma has higher tolerance to Li impurities than low-parameter plasma. By contrast, tungsten splashing from the melted layer on the upper divertor was also induced by the R-T instability but generally resulted in plasma disruption, which suggests lower tolerance to tungsten impurities in EAST tokamak.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Corrosion of 304 stainless steel in static liquid lithium under high vacuum

To study the compatibility especially the corrosion characteristic of structural material stainless steel (SS) with liquid lithium (Li) is an important factor for the simultaneous application of liquid Li and SS as a blanket material or potential plasma facing material (PFM) in future fusion devices. Here, the corrosion behaviors of 304SS exposed to liquid Li at 700 K for 1320 hr under high vacuum were investigated. After exposure to liquid Li, 304SS produces non-uniform corrosion which includes corrosion products and grain boundary corrosion. Compared with the corrosion behaviors at 600 K and 640 K, temperature plays an important role in the corrosion behaviors of 304SS in static liquid Li. The weight loss, corrosion depth and corrosion products of 304SS specimens increase with the corrosion temperature. In general, the compatibility between 304SS and static liquid Li is relatively good under the experimental conditions. And besides, it is unexpectedly found that the compatibility of copper with Li is not good.

304SS↗