Search NASA⌕ Search

Engineering topics

Hu, Ling

Publications and source records attributed to Hu, Ling.

Low-loss interconnects for modular superconducting quantum processors

Low-loss superconducting aluminium cables and on-chip impedance transformers can be used to link qubit modules and create superconducting quantum computing networks with high-fidelity intermodule state transfer. Scaling is now a key challenge in superconducting quantum computing. One solution is to build modular systems in which smaller-scale quantum modules are individually constructed and calibrated and then assembled into a larger architecture. This, however, requires the development of suitable interconnects. Here we report low-loss interconnects based on pure aluminium coaxial cables and on-chip impedance transformers featuring quality factors of up to 8.1 x 10 5 , which is comparable with the performance of our transmon qubits fabricated on a single-crystal sapphire substrate. We use these interconnects to link five quantum modules with intermodule quantum state transfer and Bell state fidelities of up to 99%. To benchmark the overall performance of the processor, we create maximally entangled, multiqubit Greenberger-Horne-Zeilinger states. The generated intermodule four-qubit Greenberger-Horne-Zeilinger state exhibits 92.0% fidelity. We also entangle up to 12 qubits in a Greenberger-Horne-Zeilinger state with 55.8 ± 1.8% fidelity, which is above the genuine multipartite entanglement threshold of 1/2.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructures and deformation mechanisms of the medium-entropy alloy (NiCoCr) 76 (Ni 6 AlTi) 3

Here the microstructures and deformation mechanisms of the f.c.c. medium-entropy alloy (MEA) (NiCoCr) 76 (Ni 6 AlTi) 3 has been analyzed after various thermo-mechanical treatments. The solutionized, single-phase MEA, which had a grain size of 93.4 ± 31.9 μm, was cold-rolled (CR) to a 80% thickness reduction after which it showed both a high yield strength (YS) of 1539 MPa and a high ultimate tensile strength (UTS) of 1602 MPa, but an elongation to failure, ε, of only 16%. The CR MEA was then subjected to one of two heat treatments: (1) the CR MEA was recrystallized at 1100°C for 24 h, which produced a single-phase material with 85 ± 61.7 μm grain size that exhibited a much lower YS and UTS of 364 MPa and 747 MPa, respectively, but a much greater ε of 73%; and (2) the MEA was aged at 700°C for 24 h, which produced a fine-grained (1.1 ± 0.9 μm) material and a high volume fraction (0.35) of 12 nm dia. L1 2 nanoparticles that exhibited an excellent combination of strength and ductility, viz., YS~1501 MPa, UTS~1651 MPa, elongation ~26%. The grain boundary strengthening and precipitation strengthening were together estimated to account for ~58% of the YS in the latter material. After deformation, the recrystallized MEA contained numerous stacking faults and a Taylor lattice structure containing domain boundaries and microbands, while the aged MEA exhibited numerous stacking faults and sheared particles. The density of low-angle grain boundaries (LAGBs) in the recrystallized MEA increased by 100 times to 2.2 × 10 –1 μm/μm 2 while the density of CSL Σ3 n boundaries decreased by 71% to 7.8 × 10 –3 μm/μm 2 after deformation. In contrast, the density of LAGBs in the aged MEA increased by 5 times to 2.6 μm/μm 2 while the density of CSL Σ3 n boundaries decreased by 57% to 0.6 μm/μm 2 after deformation.

36 MATERIALS SCIENCE↗

Optimization of the microstructure and mechanical properties of electron beam welded high-strength medium-entropy alloy (NiCoCr) 94 Al 3 Ti 3

For this work, the weldability and effects of subsequent heat treatment on the microstructure and mechanical properties of the medium-entropy alloy (MEA) (NiCoCr) 94 Al 3 Ti 3 have been explored using electron beam welding (EBW). It was found that EBW joints consist of a supersaturated f.c.c. matrix with coarse, asymmetric columnar grains (17.7–24 μm). The fraction of twins and Σ3 n CSL boundaries in weld joints was only 10% of that in the base metal, a value which increased to 30% after aging at 800 °C. The aging also led to improvements in the hardness, tensile strength, and work hardening rate, a result of the precipitation of a high volume fraction (0.29–0.33) of ultrafine (15–17.4 nm dia.) coherent spherical L1 2 -structured particles. The contributions of the L1 2 nanoparticles and Hall-Petch strengthening to the yield strength were estimated to be 537–573 MPa and 105–123 MPa, respectively. The MEA shows excellent weldability and, after aging, good strength (YS~1098 MPa, UTS~1368 MPa) and elongation to failure (~11%) by ductile fracture.

36 MATERIALS SCIENCE↗

Preparation of Imide Oligomers via Concurrent Reactive Extrusion

Reactive extrusion can be used in a continuous, solvent-less preparation of imide oligomers involving two competing reactions among three ingredients, the first reaction between a dianhydride and a diamine and the second reaction between an endcap and the same diamine. The imide oligomer can form a composite via conventional production methods or via formation of a film from imide oligomer re-melted in an extruder before being impregnated into tape or fabric.

Avakian, Roger W.↗