Magnetic and high frequency properties of nanogranular CoFe-TiO{sub 2} films

A series of soft magnetic nanogranular CoFe-TiO{sub 2} films with different thicknesses were fabricated on Si substrates by co-sputtering CoFe and TiO{sub 2}, and the magnetic and high frequency properties were studied in details. X-ray diffraction analysis confirmed that the films were nanocrystalline/amorphous composites. A saturation magnetization as high as 21 kGs and a ferromagnetic resonance (FMR) frequency above 3 GHz were obtained. It was found that the coercivity decreased steeply with the increase of film thickness and its minimum value was about 6 Oe. In addition, the variations of FMR peak broadness of the imaginary part and damping factor were also presented and discussed as functions of film thickness.

36 MATERIALS SCIENCE↗

Effects of ruthenium seed layer on the microstructure and spin dynamics of thin permalloy films

The spin dynamics and microstructure properties of a sputtered 12 nm Ni{sub 81}Fe{sub 19} thin film have been enhanced by the use of a ruthenium seed layer. Both the ferromagnetic resonance field and linewidth are enhanced dramatically as the thickness of ruthenium seed layer is increased. The surface anisotropy energy constant can also be largely tailored from 0.06 to 0.96 erg/cm{sup -2} by changing the seed layer thickness. The changes to the dynamics magnetization properties are caused by both ruthenium seed layer induced changes in the Ni{sub 81}Fe{sub 19} structure properties and surface topography properties. Roughness induced inhomogeneous linewidth broadening is also seen. The damping constant is highly tunable via the ruthenium thickness. This approach can be used to tailor both the structure and spin dynamic properties of thin Ni{sub 81}Fe{sub 19} films over a wide range. And it may benefit the applications of spin dynamics and spin current based devices.

36 MATERIALS SCIENCE↗

Tuning the direction of exchange bias in ferromagnetic/antiferromagnetic bilayer by angular-dependent spin-polarized current

The angular dependence of an external magnetic field applied with an in-plane alternating pulse that induces a new direction of exchange bias (EB) is observed in an NiFe/IrMn bilayer. Depending strongly on the direction of the external field, EB field gradually orients along the external field with the increase in current pulse, and the new direction of EB is finally established. Furthermore, the new direction of EB can also be induced along the external field at once when the applied pulse is larger than the critical current. Because the strength and direction of the EB is highly correlated with the micromagnetic state distribution of the antiferromagnet, the observations are explained by the spin torque exerted on the antiferromagnetic moments and provide evidence for the prediction of spin transfer and current-induced switching in antiferromagnets.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Improvement of high-frequency characteristics of Z-type hexaferrite by dysprosium doping

Z-type hexaferrite has great potential applications as anti-EMI material for magnetic devices in the GHz region. In this work, Dy-doped Z-type hexaferrites with nominal stoichiometry of Ba{sub 3}Co{sub 2}Dy{sub x}Fe{sub 24-x}O{sub 41} (x 0.0, 0.05, 0.5, 1.0) were prepared by an improved solid-state reaction method. The effects of rare earth oxide (Dy{sub 2}O{sub 3}) addition on the phase composition, microstructure and electromagnetic properties of the ceramics were investigated. Structure and micromorphology characterizations indicate that certain content of Dy doping will cause the emergence of the second phase Dy{sub 3}Fe{sub 5}O{sub 12} at the grain boundaries of the majority phase Z-type hexaferrite, due to which the straightforward result is the grain refinement during the successive sintering process. Permeability spectra measurements show that the initial permeability reaches its maximum of 17 at 300 MHz with x = 0.5, while the cutoff frequency keeps above 800 MHz. The apparent specific anisotropy field H{sub K} of Dy-doped Z-type hexaferrites decreases with x increasing. The relationships among phase composition, grain size, permeability spectra, and anisotropy are theoretically investigated, and according to the analysis, Dy doping effects on its magnetic properties can be well explained and understood.

36 MATERIALS SCIENCE↗

Sintering dense NiZn ferrite by two-step sintering process

A two-step sintering process has been adopted to produce NiZn ferrite with composition of (NiO){sub 0.35}(ZnO){sub 0.57}(CuO){sub 0.08}(Fe{sub 2}O{sub 3}). The densification, microstructure, and magnetic properties of the ferrite have been investigated and compared with those of ferrites produced by the traditional final-stage sintering process. It was found that the sample produced by a two-step sintering process with a high temperature of 1200 deg. C and a lower temperature of 1100 deg. C attained more than 96% of the theoretical density and had a uniform microstructure with a small average grain size. It also exhibited good performances in terms of permeability and Q-factor. Hence, this would seem to be an effective method for producing dense ferrites with a microstructure composed of small and even grains, which is a very effective strategy for improving the magnetic properties of ferrites.

36 MATERIALS SCIENCE↗

Soft magnetic properties of (Ni{sub 80}Fe{sub 20}){sub 1-x}(Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4}){sub x} films for high frequency applications

A series of (Ni{sub 80}Fe{sub 20}){sub 1-x}(Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4}){sub x} films were fabricated on Si substrates by means of radio frequency magnetron sputtering and the electrical and magnetic properties were studied. Optimal films with the desired properties of low coercivity H{sub c} {approx} 4 Oe, high saturation magnetization 4{pi}Ms {approx} 14.5 kG, and high electrical resistivity {rho} {approx} 1500 {mu}{Omega} cm were obtained. The permeability spectra measured shows that its natural ferromagnetic resonant frequency was about 3.4 GHz. The tested results shown that the sputtering power had an important effect on the films properties and that it can be convenient to adjust the natural ferromagnetic resonant frequency of the films.

36 MATERIALS SCIENCE↗

Synthesis and magnetic properties of Co-Ti-Bi codoped M-type barium ferrite

The effects of Co{sup 2+}, Ti{sup 4+}, and Bi{sup 3+} substitution on the microstructures and properties of low-temperature fired M-type barium hexaferrites have been studied in order to adapt the development of low-temperature cofired ferrites technology and produce gyromagnetic devices with a multilayer process. It is found that Bi{sup 3+} ions can enter into the 2a sublattice and consequently enhance the grain growth and densification due to the activation of the lattice, which in turn first lead to an increase and then a decrease of M{sub s}. The substitution of Bi{sup 3+} ions is beneficial to forming the M phase and lowers the sintering temperature to about 900 deg. C, which is ideal for cofiring with silver paste. Scanning electron microscope and x-ray diffraction analysis have shown that the samples have excellent crystalline grains with a uniform size about 1-2 {mu}m. Moreover, nonmagnetic Ti{sup 4+} ions prefer to enter the 4f{sub VI} octahedral sites, giving rise to the weakening of the strong 12k-4f{sub VI} superexchange path and thus the isotropic exchange energy approaches the other second-order terms on the magnetic Hamiltonian, such as the antisymmetric interaction or even the magnetocrystalline anisotropy. With increasing the substitution content, some Co{sup 2+} ions, which locate in octahedral 12k sites, give a strong planar contribution to the anisotropy. Therefore, M{sub s} and H{sub c} decrease with the Co-Ti-substitution.

36 MATERIALS SCIENCE↗

Structural and magnetic properties of NiZn-ferrite thin films prepared by radio frequency magnetron sputtering

Polycrystalline NiZn-ferrite thin films were deposited on Si(100) substrate by rf magnetron sputtering, using targets with a nominal composition of Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4}. The effects of substrate condition, sputtering pressure, and postannealing on the structure and magnetic properties of thin films have been investigated. Our results show that the preferred orientation of the NiZn spinel film changed from (311) to (400) with increasing the Ar pressure from 0.8 to 1.6 Pa, meanwhile, the grain size also increased. Atomic force microscopy analysis indicates that perfect surface morphology of the film can be obtained at a relatively lower sputtering pressure of 1.0 Pa. The relative percentage of residual oxygen increases significantly on a condition of lower sputtering pressure, and plays an important role in film structure due to the strong molecular adsorption tendency of oxygen on the film surface during the deposition process. A thin film with a typical thickness of 1 {mu}m, a saturation magnetization of 150 emu/cm{sup 3}, and a coercivity of 8.8 kA/m has been obtained after annealing at 800 deg. C, which has the potential application in magnetic integrated circuits.

36 MATERIALS SCIENCE↗

Influence of sputtering power on the high frequency properties of nanogranular FeCoHfO thin films

Soft magnetic nanogranular FeCoHfO thin films were fabricated using rf magnetron sputtering in an oxygen/argon ambient. During the deposition process, the partial pressure of oxygen was fixed at 2.5% and sputtering power was used as the control parameter, varying from 50 to 300 W. It was found that the film electrical resistivity ({rho}) decreases steeply with the increase of sputtering power, and the saturation magnetization (4{pi}M{sub s}) and the natural ferromagnetic resonant frequency f{sub r} increase with increasing sputtering power from 50 to 200 W, and then decrease when sputtering power exceeded 200 W. The maximum value of 4{pi}M{sub s} and f{sub r} were 20.5 kG and 3.2GHz, respectively. The coercivity of films had a contrary trend compared with 4{pi}M{sub s} and f{sub r}, and its minimum value was about 1 Oe. The physical origin of the influence was suggested to be related to the structure and composition changes in films.

36 MATERIALS SCIENCE↗

Electromagnetic properties of microwave sintered ferromagnetic-ferroelectric composites for application in low temperature co-fired ceramic devices

In this paper, microwave sintering (MS) technology has been applied in the preparation of ferromagnetic-ferroelectric composites. Several kinds of (Ni{sub 0.3}Zn{sub 0.6}Cu{sub 0.1})Fe{sub 2}O{sub 4} (NiCuZn) ferrite with different contents of BaTiO{sub 3}(BT) have been fabricated by MS technology. We found that the sintering time and temperature were significantly reduced from 22 h and 1100 deg. C for the conventional sintering (CS) process to 2 h and 840 deg. C for MS process, respectively. Experiments show that MS treated NiCuZn-BT composites possess both excellent ferromagnetic and ferroelectric properties. For the composites of NiCuZn added with 15% BaTiO{sub 3}, the real part of permittivity is larger than 50 below 20 MHz and the real part of dielectric constant is larger than 18 below 1 GHz. Our results indicate that the microwave sintering method is a potential important technique in LTCC technology.

36 MATERIALS SCIENCE↗

Effects of off-stoichiometry and density on the magnetic and magneto-optical properties of yttrium iron garnet films by magnetron sputtering method

Yttrium iron garnet films were deposited on Si and Si/CeO{sub 2} substrates by magnetron sputtering method followed by postannealing. By varying the fabrication parameters such as sputtering atmosphere, sputtering power, and annealing atmosphere, single phase garnet films were obtained with different off-stoichiometry and film density. The dependence of cation ratio, magnetic and magneto-optical characteristics, and absorption coefficient were systemically investigated. The results reveal that a proper oxygen pressure in both sputtering and annealing process give rise to a small cation ratio of (Fe{sup 2+} or Fe{sup 4+})/Fe{sup 3+}, thus is beneficial to obtain large saturation magnetization, large Faraday rotation, and small optical absorption. The sputtering power can also affect the properties of the film through changing the film density. Our results indicate that the properties of sputtering deposited yttrium iron garnet (YIG) film can be easily tuned and optimized by modifying the off-stoichiometry and density of the film, thus provides flexibility to fabricate YIG film for extensive applications.

36 MATERIALS SCIENCE↗

Colossal dielectric constant and relaxation behaviors in Pr:SrTiO{sub 3} ceramics

Sr{sub 1-x}Pr{sub x}TiO{sub 3} ceramics (0.00{<=}x{<=}0.03) were prepared by a traditional solid-state reaction method. Two relaxation processes (marked as A and B) of the Sr{sub 0.09}Pr{sub 0.01}TiO{sub 3} ceramics were investigated by analyzing the E{sub a} values obtained from the Arrhenius law. Colossal dielectric constant (CDC) was first obtained in Sr{sub 0.09}Pr{sub 0.01}TiO{sub 3} ceramics, whose permittivity was up to 3000 (1 kHz, room temperature), greater than that of pure SrTiO{sub 3} ceramics and samples with more Pr addition (x=0.02 and 0.03). This CDC behavior was related to the internal barrier layer capacitance mechanism.

36 MATERIALS SCIENCE↗

Effect of B{sub 2}O{sub 3}-Bi{sub 2}O{sub 3}-SiO{sub 2}-ZnO glass on the dielectric and magnetic properties of ferroelectric/ferromagnetic composite for low temperature cofired ceramic technology

Ni-Cu-Zn ferrite/BaTiO{sub 3} composites with different additive amounts of B{sub 2}O{sub 3}-Bi{sub 2}O{sub 3}-SiO{sub 2}-ZnO (BBSZ) glass have been prepared by a conventional solid-reaction method and sintered at 900 deg. C to adapt to low temperature cofired ceramic (LTCC) technology. The dielectric and magnetic properties of the composites can be effectively improved with increasing BBSZ content. Here, the BBSZ glass mainly plays two roles, one is as a sintering aid promoting grain growth and the other is as a low permittivity phase or nonmagnetic phase leading to dilution effect on the dielectric or magnetic properties of the composites. The effect degree of above two roles is related to the variation in BBSZ content and has been discussed combining with the effective medium theory. The lower and upper bounds for the effective permittivity and permeability have been given by the Maxwell-Garnett rules.

36 MATERIALS SCIENCE↗

Tuning magnetic properties of yttrium iron garnet film with oxygen partial pressure in sputtering and annealing process

In this paper, the magnetic properties of these films which deposited and annealed at different atmospheres were investigated. The experimental results show that the magnetic properties of yttrium iron garnet films prepared by rf magnetron sputtering method can be tuned with oxygen partial pressure in sputtering and annealing processes. The optimal condition is depositing in atmosphere of R=0 and annealing at 0.5 Pa O{sub 2}, or depositing in atmosphere of R=2% and annealed in vacuum.

36 MATERIALS SCIENCE↗

Effect of CeO{sub 2} buffer layer on the microstructure and magnetic properties of yttrium iron garnet film on Si substrate

Yttrium iron garnet films were grown by radio frequency magnetron sputtering on Si(111) substrate with and without CeO{sub 2} buffer layer, and influence of CeO{sub 2} buffer on the microstructure and magnetic behaviors of the films were investigated. As compared with the film without buffer, a larger saturation magnetizaton (M{sub s}), lower coercive force (H{sub c}), and higher remnant magnetization (M{sub r}) were obtained due to the introduction of CeO{sub 2} layer. The higher M{sub s} results from the denser structure and the smaller content of Fe{sup 2+} ions. The lower H{sub c} and higher M{sub r} can be explained by the small surface roughness and crystal grains size. The film on CeO{sub 2} buffer layer possess fine microstructure and its surface roughness is smaller than the unbuffered films, which provides an increased exchange between the crystal grains and an enhanced spontaneous magnetization effect, leading to the higher remnant magnetization.

36 MATERIALS SCIENCE↗

Correlation between sputtering parameters and composition of SmCo-based films for microelectromechanical system applications

About 3.0 {mu}m thick SmCo-based films with additives of Fe, Cu, and Zr were deposited on Si substrates. Based on a developed semiempirical theoretical model, the dependence of the film composition on the sputtering parameters was discussed. The experimental results show that the Sm concentration increases with decreasing sputtering power or increasing Ar gas pressure, which are in good agreement with the calculated results when the preferential sputtering effect is disregarded. The effect of the sputtering parameters on the film composition provides an opportunity for the same composite target to fabricate films with Sm concentration varying from 13.8 to 17.3 at. %, which is reasonable for the permanent magnetic phase transformation (Sm{sub 2}Co{sub 17}{yields}SmCo{sub 7}{yields}SmCo{sub 5}). Furthermore, the observed TbCu{sub 7}-type film shows a better crystal texture with a low remanence ratio for the hysteresis loops measured out plane to in plane of 0.08.