Ionomer Optimization for Water Uptake and Swelling in Anion Exchange Membrane Electrolyzer: Hydrogen Evolution Electrode

Green hydrogen produced through anion exchange membrane water electrolysis is a promising, low-cost chemical storage solution for intermittent renewable energy sources. Low-temperature electrolysis using anion exchange membranes (AEM) combines the benefits of established water electrolysis technologies based on alkaline electrolysis and proton exchange membrane electrolysis. The anion conductive ionomers (ACI) used in the AEM electrolyzer (AEMEL) electrodes has been investigated. The ACI serves two primary purposes: (i) facilitate hydroxide conduction between the catalyst and bulk electrolyte and (ii) bind the catalyst to the porous transport layer and membrane. High ion exchange capacity (IEC) ACIs are desired, however, high IEC can cause excessive water uptake (WU) and detrimental ACI swelling. Proper water management is a key factor in obtaining maximum performance in AEM-based devices. In this study, a series of poly(norbornene)-based ACIs were synthesized and deployed in hydrogen evolving AEMEL cathode electrodes. A balance between ionic conductivity, WU and ionomer swelling was achieved in the ACI by varying the IEC and degree of polymer cross-linking. It was found that higher IEC ACIs with light crosslinking are preferred in the HER electrode. Furthermore, such a configuration fine-tuned the WU and ionomer swelling to achieve optimum cell performance and reduce cell operating voltages.

08 HYDROGEN↗

Ionomer Optimization for Water Uptake and Swelling in Anion Exchange Membrane Electrolyzer: Oxygen Evolution Electrode

Water electrolysis using an anion conductive, solid polymer electrolyte is an attractive method for point-of-use hydrogen production. Recent advances in catalysts and anion exchange membranes (AEM) have made alkaline devices increasingly competitive with their acidic counterparts. However, less attention has been paid to the anion conductive ionomers (ACI) used in the fabrication of electrodes for AEM electrolyzers. The ACI contributes to ion conduction between the catalyst and bulk electrolyte and serves as a binder for adhering the catalyst to the gas diffusion layer and AEM. Ionic conductivity, water uptake and ionomer swelling are critical properties for electrode performance. High ion exchange capacity (IEC) in the ionomer is desired for reduced electrode resistance, however, it can lead to excess water uptake (WU) and disruptive ACI swelling. In this study, a series of poly(norbornene)-based ionomers were synthesized, characterized and used to fabricate oxygen evolving anodes for low-temperature AEM water electrolysis. The IEC of the ionomers (0 to 4.73 meq g −1 ) was adjusted by controlling the ratio of ion conducting to non-ion conducting norbornene monomers in the ACI tetrablock copolymers. Low conductivity ionomers are shown to yield the best-performing oxygen evolution electrodes, in the absence of ACI polymer cross-linking because they do not experience excessive water swelling. Light cross-linking within the anode ACI was used as a means to independently lower WU of the ionomer without compromising ionic conductivity. This control over water swelling allows higher ionic conductivity within the ACI to be used in water-fed electrolyzer applications. Other methods of water management were compared including the use of hydrophobic additives and adjustment of the ionomer concentration in the electrode. As a result, it was shown that the cell performance greatly benefits from a highly conductive ionomer in the oxygen evolution reaction electrode if the WU is managed.

08 HYDROGEN↗

Achieving High‐Performance and 2000 h Stability in Anion Exchange Membrane Fuel Cells by Manipulating Ionomer Properties and Electrode Optimization

The primary function of the ionomers that are incorporated into fuel cell electrode catalyst layers is to provide pathways for ion transport between the catalyst active sites and the electrolyte. This is influenced by many variables, including the ion-exchange capacity, water uptake, and molecular weight. In anion exchange membrane fuel cells (AEMFCs), controlling ionomer water uptake is particularly important and tailoring this property in each electrode is an important consideration when looking to maximize cell performance. In this study, three poly(norbornene) tetrablock copolymer ionomers with a range of physical properties are synthesized and incorporated into AEMFC anode and cathode electrodes. Systematic electrode engineering with these ionomers allows the peak power density to be increased by 100% (1.6 W cm -2 → 3.2 W cm -2 ) and the current density at 0.2 V to be increased by 59% (5.9 A cm -2 → 9.4 A cm -2 ). Moreover, the top-performing electrode configuration is tested in an operating AEMFC at the US Department of Energy defined current density of 600 mA cm -2 for 2000 h, showing a record-low voltage decay rate of 15.36 µV h -1 – only 3.65% –a over 2000 h. Here, this work sets a new bar for AEMFCs, reporting the best combination of performance and durability of any AEMFC to date.

08 HYDROGEN↗

Effect of reacting gas flowrates and hydration on the carbonation of anion exchange membrane fuel cells in the presence of CO 2

Anion exchange membrane fuel cells (AEMFCs) have been widely touted as a low-cost alternative to existing proton exchange membrane fuel cells. However, one of the limitations of this technology has been the severe performance penalty related to the introduction of CO 2 to the cell – typically in the air cathode feed. Introduction of CO 2 into AEMFCs results in cell carbonation, which imparts thermodynamic, kinetic and Ohmic overpotentials that can add up to hundreds of millivolts. Therefore, it is important to find strategies and operational protocols for AEMFCs that minimize these overpotentials. In this paper, we reserach the impacts of the anode and cathode flowrate, as well as the cell hydration level, on the extent of cell carbonation and cell polarization. Key findings include: (1) decreasing the cathode flowrate generally decreases the total CO 2 -related voltage loss while changing the anode flowrate has a minimal effect; (2) increasing cell hydration helps to mitigate the performance loss in the presence of CO 2 ; and (3) operational combinations are found that significantly reduce the CO 2 penalty compared to the present literature.

25 ENERGY STORAGE↗

Poly(norbornene) anion conductive membranes: homopolymer, block copolymer and random copolymer properties and performance

It has previously been shown that phase-separated block copolymers with non-ion conducting (hydrophobic) blocks and ion conducting (hydrophilic) blocks can form efficient ion conducting channels with high ionic mobility and conductivity. Block copolymers can provide a means for phase segregation and ion channel formation while homopolymers and random copolymers have been shown to have lower ion mobility. In this study, the properties of poly(norbornene) based anion exchange membranes (AEMs) comprising homopolymers, block copolymers, and random copolymers with high ion-exchange capacity (IEC) (3.48–4.55 meq. g -1 ) have been investigated and compared. The polymers were cross-linked with N,N,N',N'-tetramethyl-1,6-hexanediamine before casting the membranes to avoid excessive water swelling due to high water uptake. It was shown that high ionic conductivity can be achieved in both random copolymers and homopolymers even in the absence of microphase-separated structures. For example, the conductivity of a random copolymer was 194 mS cm -1 at 80 °C, which was comparable to the block copolymer, 201 mS cm -1 at 80 °C. The H 2 /O 2 fuel cell performance of random copolymer composite membranes showed a peak power density of 3.05 W cm -2 and peak current density of 7.85 A cm -2 at 80 °C compared to block copolymer membranes (peak power density of 3.21 W cm -2 and peak current density of 8.27 A cm -2 at 80 °C). It is more critical that high water transport be achieved in AEMs than achieving a phase-segregated morphology. Finally, the homopolymer, block copolymer, and random copolymer membranes showed <1.35% degradation after aging in 1 M NaOH at 80 °C for 1000 h.

08 HYDROGEN↗

Influence of Water Transport Across Microscale Bipolar Interfaces on the Performance of Direct Borohydride Fuel Cells

Direct borohydride fuel cells (DBFCs) can operate at double the voltage of proton exchange membrane fuel cells (PEMFCs) by employing an alkaline NaBH 4 fuel feed and an acidic H 2 O 2 oxidant feed. The pH-gradient-enabled microscale bipolar interface (PMBI) facilitates the creation and maintenance of an alkaline environment at the anode and an acidic environment at the cathode for the borohydride oxidation and peroxide reduction reactions. However, given the need to dissociate water at the interface to ensure ionic conduction, PMBI can be efficient only when anion exchange ionomer (AEI) moieties enable fast water transport for autoprotolysis. Herein, a series of polynorbornene-based AEIs with a range of water uptake values are examined to unravel the optimum water uptake required to enable high performance DBFCs. The DBFC with PMBI configuration containing the optimal AEI composition delivers a current density of 302 mA cm –2 at 1.5 V and a peak power density of 580 mW cm –2 at 1 V. This AEI composition exhibits high hydroxide ionic conductivity of 90.7 mS cm –1 at 80 °C with an IEC of 2.01 mequiv g –1 and demonstrates impressive chemical stability by retaining 98.75% of its initial ionic conductivity after immersion into anolyte (3 M KOH and 1.5 M NaBH 4 ) at 70 °C for 536 h.

25 ENERGY STORAGE↗

The Importance of Water Transport in High Conductivity and High-Power Alkaline Fuel Cells

High ionic conductivity membranes can be used to minimize ohmic losses in electrochemical devices such as fuel cells, flow batteries, and electrolyzers. Very high hydroxide conductivity was achieved through the synthesis of a norbornene-based tetrablock copolymer with an ion-exchange capacity of 3.88 meq/g. The membranes were cast with a thin polymer reinforcement layer and lightly cross-linked with N,N,N',N'-tetramethyl-1,6-hexanediamine. The norbornene polymer had a hydroxide conductivity of 212 mS/cm at 80°C. Light cross-linking helped to control the water uptake and provide mechanical stability while balancing the bound (i.e. waters of hydration) vs. free water in the films. The films showed excellent chemical stability with <1.5% conductivity loss after soaking in 1 M NaOH for 1000 h at 80°C. The aged films were analyzed by FT-IR before and after aging to confirm their chemical stability. A H 2 /O 2 alkaline polymer electrolyte fuel cell was fabricated and was able to achieve a peak power density of 3.5 W/cm 2 with a maximum current density of 9.7 A/cm 2 at 0.15 V at 80°C. The exceptionally high current and power densities were achieved by balancing and optimizing water removal and transport from the hydrogen negative electrode to the oxygen positive electrode. High water transport and thinness are critical aspects of the membrane in extending the power and current density of the cells to new record values.

08 HYDROGEN↗

Highly Conductive Anion-Exchange Membranes Based on Cross-Linked Poly(norbornene): Vinyl Addition Polymerization

Cross-linked (XL) anion-exchange membranes (AEMs) synthesized by vinyl addition polymerization of norbornene were prepared for use in anion-exchange membrane electrochemical devices, including fuel cells and electrolyzers. Tetrablock copolymers composed of an all-hydrocarbon backbone with a very high ion-exchange capacity (IEC), 3.46 mequiv/g, were synthesized. Light cross-linking was found to be adequate for providing critical control over unwanted water uptake. This enabled use of very high IEC membranes. Without light cross-linking, the unwanted water uptake would cause swelling and softening of the membrane. The best performing membrane had no significant drop in ionic conductivity over 1000 h of aging in 1 M NaOH at 80 °C and a record high ionic conductivity of 198 mS/cm at 80 °C (for a chemically stable AEM). The number of bound and free water molecules per ion pair is described along with ion mobility comparisons to previous materials. Here, the membranes are suitable for electrochemical devices and were used in AEM fuel cells

08 HYDROGEN↗

Anionic multiblock copolymer membrane based on vinyl addition polymerization of norbornenes: Applications in anion-exchange membrane fuel cells

Stable, non-hydrolysable, hydroxide-conducting polymers are of interest for electrochemical devices such as fuel cells, electrolyzers and flow-batteries. In this study, a series of tetrablock copolymers containing an all-hydrocarbon backbone were synthesized. The synthesis is based on vinyl addition polymerization of norbornene using (η 3 -allyl)Pd( i Pr 3 P)Cl as the catalyst and lithium tetrakis(pentafluorophenyl)-borate·(2.5Et 2 O) (Li[FABA]) as the activator. The tetrablock polymers were cast into membranes with an ion-exchange capacity (IEC) between 1.55 and 2.60 milliequivalents per gram (meq/g). The number of bound and unbound water molecules per ion pair was measured and correlated with conductivity. The membrane with the highest IEC (2.60 meq/g) had 10.6 unbound (i.e. free) and 17.9 bound water molecules per ion pair within the polymer. The presence of excess unbound water has led to flooding of the ion conductive channels and low hydroxide ion conductivity. The optimal anion conductivity was found with about 6.7 unbound and 11.9 bound water molecules per ion pair. Excellent hydroxide conductivity (> 120 mS/cm at 80 °C) was obtained at an ion-exchange capacity of 1.88 meq/g. The results show that hydroxide mobility is aided by phase segregation within the copolymer. The ion conducting polymer was stable in 1M NaOH solution at 80 °C, showing essentially no loss in ion conductivity in 1200 h. Thermogravimetric analysis showed that the membrane backbone was stable up to 400 °C, consistent with previous polynorbornene-based materials. The peak power density of a H 2 /O 2 , hydroxide conducting fuel cell containing one of these membranes was 542.57 mW/cm 2 at 0.43 V and current density of 1.26 A/cm2 at 60 °C.

08 HYDROGEN↗